62.
    发明专利
    未知

    公开(公告)号:DE59704509D1

    公开(公告)日:2001-10-11

    申请号:DE59704509

    申请日:1997-06-05

    Applicant: BASF AG

    Abstract: The production of polymer powder (I) suitable for the modification of mineral binder building materials, involves drying an aqueous polymer dispersion which forms films with a Tg of not above 30 degrees C, where before drying, the dispersion is treated with drying agents (IIa) which have a liquefying action on the mineral binder when it is mixed with water and ready for use; after drying, the powder (I) is treated with finely divided solid additive(s) (IIIa) which have a solidifying action on the binder/water mix. Alternatively, the dispersion is treated with solidifying driers (IIb) before drying, and the dried powder is treated with finely divided solid additives (IIIb) which have a liquefying action on the mix. Also claimed are: (i) polymer powder (I) obtained by this process; (ii) mineral binders containing (I); and (iii) dry mortar preparations containing 20-60 wt% mineral binder, 0.1-20 wt% (I) and up to 25 wt% conventional additives, the remainder consisting of sand, fillers, pigments and natural and/or synthetic fibres.

    64.
    发明专利
    未知

    公开(公告)号:DE59703682D1

    公开(公告)日:2001-07-05

    申请号:DE59703682

    申请日:1997-07-21

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP97/03929 Sec. 371 Date Jan. 20, 1999 Sec. 102(e) Date Jan. 20, 1999 PCT Filed Jul. 21, 1997 PCT Pub. No. WO98/03576 PCT Pub. Date Jan. 29, 1998Phenolsulfonic acid-formaldehyde condensates are used as assistants in the drying of aqueous polymer dispersions. Also described are a process for preparing polymer powders by drying, using these condensates; the polymer powders obtainable by the process; and their use as binders.

    66.
    发明专利
    未知

    公开(公告)号:ES2153518T3

    公开(公告)日:2001-03-01

    申请号:ES96111237

    申请日:1996-07-12

    Applicant: BASF AG

    Abstract: Prodn. of modified mineral building materials is effected using an aq. dispersion contg. polymer particles of wt. average dia. 100-300 (pref. 100-200)nm, the polymer being free radically polymerised and being of each of the following 3 types of monomers; (a) up to 5 wt.% (meth)acrylate acid or salts; (b) up to 5 wt.% (meth)acrylamide; and (c) 90-97.5 wt.% other non-ionic, ethylenically unsaturated monomers, pref. styrene and/or butadiene. The dispersions are claimed, as are powders obtd. by spray drying of the dispersions.