公开(公告)号:PT1036100E
公开(公告)日:2002-09-30
申请号:PT98965218
申请日:1998-12-01
Applicant: BASF AG
Inventor: WENDEROTH BERND , DECKERS ANDREAS , WEDEL PETER , WEBER WILHELM
IPC: C10L1/18 , C08F2/00 , C08F210/02 , C08F218/08 , C10L1/197
Abstract: In a process for preparing ethylene-vinyl acetate copolymers in which a mixture of ethylene and vinyl acetate is polymerized continuously in the presence of free-radical polymerization initiators and, if desired, molecular weight regulators in a cooled tube reactor at a pressure in the range from 1000 to 3500 bar, and the poly-merization initiator is added at the beginning and at two or more points along the tube reactor, and temperature changes in the reaction mixture along the tube reactor, between the first temperature maximum and the last addition of the polymerization initiator, are within a range of not more than 20° C.
-
公开(公告)号:DE10102937A1
公开(公告)日:2002-07-25
申请号:DE10102937
申请日:2001-01-23
Applicant: BASF AG
Inventor: WITTKOWSKI LARS , DECKERS ANDREAS , WEBER WILHELM , DROEGE THOMAS , GONIOUKH ANDREI , MAEHLING FRANK-OLAF
Abstract: Preparation of ethylene polymers (A) by a high pressure process involves dissolving radical initiator(s) in ketone(s) (I); compressing; dosing the mixture to the polymerization reactor in one or more portions; and carrying out polymerization. Preparation of ethylene polymers (A) by a high pressure process involves: (1) dissolving radical initiator(s) in ketone(s) of formula R1-CO-R2 (I); (2) compressing; (3) dosing the mixture to the polymerization reactor in one or more portions; and (4) carrying out polymerization at 140-350 deg C and 400-4500 bars. R1, R2 = 1-6C alkyl or 3-12C cycloalkyl; or are linked to complete a 4-13 membered ring.
-
公开(公告)号:ES2168629T3
公开(公告)日:2002-06-16
申请号:ES97920747
申请日:1997-04-24
Applicant: BASF AG
Inventor: MOLL ULRICH , DECKERS ANDREAS , KINGMA AREND JOUKE , WEBER WILHELM
IPC: C08F2/00 , C08F4/44 , C08F4/46 , C08F4/50 , C08F4/622 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/68 , C08F10/02 , C08F110/02
Abstract: A process is disclosed for preparing ethylene polymers with a molecular weight Mw (weight average) lower than 20,000 g/mole at temperatures in a range from 200 to 280 DEG C and pressures in a range from 1000 to 3500 bars in the presence of a catalyst system. The catalyst system used contains: (A) a non-bridged substituted or unsubstituted biscyclopentadienyl complex; (B) a metal compound of general formula (I) M (R )r (R )s (R )t, in which M is an alkaline, an alkaline earth metal or a metal of the third main group of the periodic table; R is hydrogen, C1-C10-alkyl, C6-C15-aryl, alkylaryl or arylalkyl with 1 to 10 C atoms in the alkyl radical and 6 to 20 C atoms in the aryl radical; R and R independently represent hydrogen, halogen, C1-C10-alkyl, C6-C15-aryl, alkylaryl, arylalkyl or alkoxy with 1 to 10 C atoms in the alkyl radical and 6 to 20 C atoms in the aryl radical; r is an integer from 1 to 3; and s and t are integers from 0 to 2, the sum r+s+t corresponding to the valency of M ; and (C) a metallocene ion-forming compound selected in a group which consists of strong, neutral Lewis acids, ionic compounds with lewis acid cations and ionic compounds with Brönsted acids as cations. Components (A), (B) and (C) are mixed together and after at the latest 5 minutes are dosed in the reactor.
-
公开(公告)号:DE59803667D1
公开(公告)日:2002-05-08
申请号:DE59803667
申请日:1998-12-01
Applicant: BASF AG
Inventor: DECKERS ANDREAS , WENDEROTH BERND , WEDEL PETER , WEBER WILHELM
IPC: C10L1/18 , C08F2/00 , C08F210/02 , C08F218/08 , C10L1/197
Abstract: In a process for preparing ethylene-vinyl acetate copolymers in which a mixture of ethylene and vinyl acetate is polymerized continuously in the presence of free-radical polymerization initiators and, if desired, molecular weight regulators in a cooled tube reactor at a pressure in the range from 1000 to 3500 bar, and the poly-merization initiator is added at the beginning and at two or more points along the tube reactor, and temperature changes in the reaction mixture along the tube reactor, between the first temperature maximum and the last addition of the polymerization initiator, are within a range of not more than 20° C.
-
公开(公告)号:AT209221T
公开(公告)日:2001-12-15
申请号:AT97920747
申请日:1997-04-24
Applicant: BASF AG
Inventor: MOLL ULRICH , DECKERS ANDREAS , KINGMA AREND JOUKE , WEBER WILHELM
IPC: C08F2/00 , C08F4/44 , C08F4/46 , C08F4/50 , C08F4/622 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/68 , C08F10/02 , C08F110/02
Abstract: A process is disclosed for preparing ethylene polymers with a molecular weight Mw (weight average) lower than 20,000 g/mole at temperatures in a range from 200 to 280 DEG C and pressures in a range from 1000 to 3500 bars in the presence of a catalyst system. The catalyst system used contains: (A) a non-bridged substituted or unsubstituted biscyclopentadienyl complex; (B) a metal compound of general formula (I) M (R )r (R )s (R )t, in which M is an alkaline, an alkaline earth metal or a metal of the third main group of the periodic table; R is hydrogen, C1-C10-alkyl, C6-C15-aryl, alkylaryl or arylalkyl with 1 to 10 C atoms in the alkyl radical and 6 to 20 C atoms in the aryl radical; R and R independently represent hydrogen, halogen, C1-C10-alkyl, C6-C15-aryl, alkylaryl, arylalkyl or alkoxy with 1 to 10 C atoms in the alkyl radical and 6 to 20 C atoms in the aryl radical; r is an integer from 1 to 3; and s and t are integers from 0 to 2, the sum r+s+t corresponding to the valency of M ; and (C) a metallocene ion-forming compound selected in a group which consists of strong, neutral Lewis acids, ionic compounds with lewis acid cations and ionic compounds with Brönsted acids as cations. Components (A), (B) and (C) are mixed together and after at the latest 5 minutes are dosed in the reactor.
-
公开(公告)号:DE10008931A1
公开(公告)日:2001-08-30
申请号:DE10008931
申请日:2000-02-25
Applicant: BASF AG
Inventor: WITTKOWSKI LARS , DECKERS ANDREAS , WEBER WILHELM , WEISS STEFAN , EHLE MICHAEL , GAST SIEGFRIED
IPC: C11D3/37 , C08F8/12 , C08F210/02 , C09D5/02 , C09D123/08 , C11D7/22 , C11D17/00 , C11D17/08 , C08F220/04
Abstract: Emulsifiable ethylene polymers comprising copolymers offrom 90 to 95% by weight of ethylene,from 4 to 10% by weight of one or more C3-C12 alkenecarboxylic acids, andfrom 0 to 1.2% by weight of one or more tertiary esters of the corresponding C3-C12 alkenecarboxylic acids,where the wax has a cinematic melt viscosity of from 800 to 3000 mm2/s, measured at 120° C.;and a process for preparing the novel emulsifiable ethylene polymers, emulsions comprising the novel ethylene polymers, a process for preparing the emulsions from the novel ethylene polymers, and also floor cleaners, car cleaners, leather cleaners and stone cleaners, and coatings for surfaces made from wood, metal, paper, glass or from plastics, comprising aqueous emulsions of the novel emulsifable waxes.
-
公开(公告)号:DK0742812T3
公开(公告)日:1999-06-23
申请号:DK95907582
申请日:1995-01-23
Applicant: BASF AG
Inventor: M LLER MICHAEL WOLFGANG , WEISS STEFAN , BOEHLKE KLAUS , WEBER WILHELM
Abstract: PCT No. PCT/EP95/00225 Sec. 371 Date Jul. 31, 1996 Sec. 102(e) Date Jul. 31, 1996 PCT Filed Jan. 23, 1995 PCT Pub. No. WO95/21221 PCT Pub. Date Aug. 10, 1995Prints are produced by the offset heatset process using a printing ink based on mineral oil and additionally using an agent for increasing the abrasion resistance of the prints, where the agent for increasing the abrasion resistance is an oxidized olefin polymer which has a melt viscosity of from 100 to 15,000 mm2/s, measured in accordance with DGF M-III 8 (75), and an acid number of from 5 to 50 mg of KOH/g of polymer, measured in accordance with DGF M-IV 2 (57).
-
公开(公告)号:ES2122544T3
公开(公告)日:1998-12-16
申请号:ES95907582
申请日:1995-01-23
Applicant: BASF AG
Inventor: WEISS STEFAN , MULLER MICHAEL WOLFGANG , BOEHLKE KLAUS , WEBER WILHELM
Abstract: PCT No. PCT/EP95/00225 Sec. 371 Date Jul. 31, 1996 Sec. 102(e) Date Jul. 31, 1996 PCT Filed Jan. 23, 1995 PCT Pub. No. WO95/21221 PCT Pub. Date Aug. 10, 1995Prints are produced by the offset heatset process using a printing ink based on mineral oil and additionally using an agent for increasing the abrasion resistance of the prints, where the agent for increasing the abrasion resistance is an oxidized olefin polymer which has a melt viscosity of from 100 to 15,000 mm2/s, measured in accordance with DGF M-III 8 (75), and an acid number of from 5 to 50 mg of KOH/g of polymer, measured in accordance with DGF M-IV 2 (57).
-
公开(公告)号:DE59503927D1
公开(公告)日:1998-11-19
申请号:DE59503927
申请日:1995-01-23
Applicant: BASF AG
Inventor: WEISS STEFAN , MUELLER MICHAEL , BOEHLKE KLAUS , WEBER WILHELM
Abstract: PCT No. PCT/EP95/00225 Sec. 371 Date Jul. 31, 1996 Sec. 102(e) Date Jul. 31, 1996 PCT Filed Jan. 23, 1995 PCT Pub. No. WO95/21221 PCT Pub. Date Aug. 10, 1995Prints are produced by the offset heatset process using a printing ink based on mineral oil and additionally using an agent for increasing the abrasion resistance of the prints, where the agent for increasing the abrasion resistance is an oxidized olefin polymer which has a melt viscosity of from 100 to 15,000 mm2/s, measured in accordance with DGF M-III 8 (75), and an acid number of from 5 to 50 mg of KOH/g of polymer, measured in accordance with DGF M-IV 2 (57).
-
公开(公告)号:FI89750C
公开(公告)日:1993-11-10
申请号:FI873500
申请日:1987-08-12
Applicant: BASF AG
Inventor: LAUKE HARALD , WEBER WILHELM , LEYRER REINHOLD J , NICK BERNHARD , LOERZER THOMAS
-
-
-
-
-
-
-
-
-