유기 실란과 인계 에스테르 공 중합 수지의 제조 방법과 이를 이용한 투명 난연 도료의 제조방법
    1.
    发明公开
    유기 실란과 인계 에스테르 공 중합 수지의 제조 방법과 이를 이용한 투명 난연 도료의 제조방법 无效
    有机硅烷和亚磷酸酯的共聚物,以及制备阻燃透明漆的工艺

    公开(公告)号:KR1020120060980A

    公开(公告)日:2012-06-12

    申请号:KR1020100095759

    申请日:2010-10-01

    Abstract: PURPOSE: A manufacturing method of organic silane and phosphate ester copolymer resin is provided to manufacture a thermosetting flame retardant pigment with high clearness and effectively improved toxicity of combustion gas in halogen based flame retardant paint. CONSTITUTION: A solution-polymerizable acrylic polyol resin composition comprises 40-70 weight% of copolymer of phosphor-silane monomers, and 30-60 weight% of organic solvent. The copolymer of the acrylic monomer is 30.0-60.0 weight% of an organosilane monomer, and 40.0-70.0 weight% of a phosphate ester monomer. The phosphate-silane acrylic resin composition has non-volatile fraction of 40-70%, a Gardner bubble viscosity of U - Z6, the acid value of 0-20 mg/KOH, and the color value of 3 or less. The phosphate ester is 1 phosphate (meth)acrylate compound comprising ethylenically unsaturated double bond in chemical formula 1.

    Abstract translation: 目的:提供有机硅烷和磷酸酯共聚物树脂的制造方法,以制造具有高清晰度并有效提高燃烧气体在卤素阻燃涂料中的毒性的热固性阻燃颜料。 构成:可溶液聚合的丙烯酸多元醇树脂组合物包含40-70重量%的荧光体 - 硅烷单体和30-60重量%的有机溶剂的共聚物。 丙烯酸类单体的共聚物为有机硅烷单体的30.0〜60.0重量%,磷酸酯单体为40.0〜70.0重量%。 磷酸酯 - 硅烷丙烯酸树脂组合物的非挥发分为40-70%,加德纳气泡粘度为U-Z6,酸值为0-20mg / KOH,颜色值为3以下。 磷酸酯是化学式1中含有烯键式不饱和双键的磷酸酯(甲基)丙烯酸酯化合物。

    실란 변성 블록이소시아네이트를 적용한 내스크래치성 향상 자동차용 일액형 클리어코트 조성물
    2.
    发明公开
    실란 변성 블록이소시아네이트를 적용한 내스크래치성 향상 자동차용 일액형 클리어코트 조성물 有权
    使用硅烷改性阻塞异构体汽车的高耐刮擦1K清漆组合物

    公开(公告)号:KR1020120003690A

    公开(公告)日:2012-01-11

    申请号:KR1020100064434

    申请日:2010-07-05

    Abstract: PURPOSE: A One component type clear coat composition is provided to maintain initial color as long as possible by minimizing scratch generated on the surface of vehicles. CONSTITUTION: A One component type clear coat composition having high scratch resistance comprises 35-45 weight% acryl resin, 20-25 weight% melamine resin, 5-10 weight silane-modified block isocyanate resin, 15-20 weight% flow-controllable resin, 0.2-0.3 weight% leveling agent, 1.0-1.5 weight% ultraviolet-absorbing agent, 0.3-0.6 weight% UV stabilizer, 2-3 weight% reaction accelerator and 12-15 weight% solvent. The glass transition temperature of the acrylic resin is -5-15 °C and the viscosity is 500-600 cps. The melamine resin is butylated melamine resin.

    Abstract translation: 目的:提供一种单组分型透明涂料组合物,通过最小化车辆表面产生的划痕,尽可能长地保持初始颜色。 构成:具有高耐擦伤性的单组分型透明涂料组合物包含35-45重量%丙烯酸树脂,20-25重量%三聚氰胺树脂,5-10重量份硅烷改性嵌段异氰酸酯树脂,15-20重量%流动可控树脂 ,0.2-0.3重量%的流平剂,1.0-1.5重量%的紫外线吸收剂,0.3-0.6重量%的UV稳定剂,2-3重量%的反应促进剂和12-15重量%的溶剂。 丙烯酸树脂的玻璃化转变温度为-5-15℃,粘度为500-600cps。 三聚氰胺树脂是丁基化三聚氰胺树脂。

    자동차 오이엠용 용접성 프리-프라임용 도료 조성물 및 이를 이용한 코팅방법
    3.
    发明公开
    자동차 오이엠용 용접성 프리-프라임용 도료 조성물 및 이를 이용한 코팅방법 有权
    用于汽车OEM和其涂层方法的可焊预涂布的组成

    公开(公告)号:KR1020110138490A

    公开(公告)日:2011-12-28

    申请号:KR1020100058403

    申请日:2010-06-21

    Abstract: PURPOSE: A weldable pre-priming paint composition for a vehicle original equipment manufacturing and a coating method using the same are provided to maximize the abrasion characteristic and the paint adhesion of an existing electrode-position coating system and to include an elastomeric resin. CONSTITUTION: A weldable pre-priming paint composition 20-30 parts by weight of polyester polyol and 2-5 parts by weight of an epoxy resin as binder resins, 4-10 parts by weight of a melamine resin as a cross-linking agent, 5-10 parts by weight of strontium chlromate as an anti-corrosive pigment, 10-20 parts by weight of zinc dust as conductive metal powder, 10-20 parts by weight of aluminum powder, 10-20 parts by weight of carbon nano-tubes, 5-15 parts by weight of a solvent, and 1.0-3.0 parts by weight of an additive.

    Abstract translation: 目的:提供用于车辆原始设备制造的可焊接预喷漆组合物和使用其的涂覆方法,以使现有电极位置涂覆系统的磨损特性和涂料附着力最大化并包括弹性体树脂。 构成:20-30重量份聚酯多元醇和2-5重量份作为粘合剂树脂的环氧树脂的可焊接的预喷漆组合物,4-10重量份作为交联剂的三聚氰胺树脂, 5-10重量份作为防腐颜料的氯酸锶,10-20重量份的作为导电金属粉末的锌粉,10-20重量份的铝粉,10-20重量份的碳纳米 - 管,5-15重量份的溶剂和1.0-3.0重量份的添加剂。

    자동차 오이엠용 용접성 프리-프라임용 도료 조성물 및 이를 이용한 코팅방법
    4.
    发明公开
    자동차 오이엠용 용접성 프리-프라임용 도료 조성물 및 이를 이용한 코팅방법 有权
    用于汽车OEM和其涂层方法的可焊预涂涂料的组合物

    公开(公告)号:KR1020110060575A

    公开(公告)日:2011-06-08

    申请号:KR1020090117196

    申请日:2009-11-30

    Abstract: PURPOSE: A weldable paint composition for pre-prime for automobile OEM is provided to maximize corrosion resistance and coating adhesion included in existing electron coating system and to enhance moldability and solderability after processing by applying an elastomeric resin. CONSTITUTION: A weldable paint composition for pre-prime for automobile OEM includes: 30~40 parts by weight of polyester polyol and 2~5 parts by weight of epoxy resin as a binder resin; 3~10 parts by weight of cross-linking agent; 15~20 parts by weight of strontium chromate as anticorrosive pigment; 20~30 parts by weight of Zn dust as metal powder; 10~15 parts by weight of titanium oxide(TiO2); 10~20 parts by weight of solvent; and 1.0~3.0 weight of additives.

    Abstract translation: 目的:提供用于汽车OEM的预焊的可焊接涂料组合物,以使现有电子涂层系统中包含的耐腐蚀性和涂层附着力最大化,并通过应用弹性体树脂提高加工后的成型性和可焊性。 构成:用于汽车OEM原料的可焊接涂料组合物包括:30〜40重量份的聚酯多元醇和2〜5重量份的作为粘合剂树脂的环氧树脂; 3〜10重量份的交联剂; 15〜20重量份铬酸锶作为防腐颜料; 20〜30重量份的锌粉作为金属粉末; 10〜15重量份的氧化钛(TiO2); 10〜20重量份溶剂; 和1.0〜3.0重量的添加剂。

    도막전이가 개선된 후도막 프리 코티드 자동차 강판의 배면 코팅용 아크릴 수지 조성물과 이를 포함하는 도료
    5.
    发明公开
    도막전이가 개선된 후도막 프리 코티드 자동차 강판의 배면 코팅용 아크릴 수지 조성물과 이를 포함하는 도료 失效
    涂层转印改进的丙烯酸树脂组合物用于厚膜预涂汽车钢板和涂料组合物的背面涂料

    公开(公告)号:KR1020130042714A

    公开(公告)日:2013-04-29

    申请号:KR1020110106748

    申请日:2011-10-19

    CPC classification number: C09D133/04 C08L63/00 C23C26/00

    Abstract: PURPOSE: An acrylic resin composition with excellent releasing force is provided to absolutely improve a releasing agent-transition phenomenon which is a weakness of existing silicon releasing agent. CONSTITUTION: An acrylic resin composition consists of 40-70 weight% of an acrylic monomer copolymer. The acrylic monomer copolymer is obtained by mixing 60-90 weight5 of an alkoxy silane group-containing acrylic monomer and 10-40 weight% of an amide group-containing acrylic monomer. The paint composition consists of 15-35 weight% of the acrylic resin composition, 20-40 weight5 of an epoxy resin composition, 30-54 weight% of an organic solvent, and 1-5 weight% of an additive.

    Abstract translation: 目的:提供具有优异释放力的丙烯酸树脂组合物,以绝对改善作为现有硅脱模剂的弱点的脱模剂转变现象。 构成:丙烯酸树脂组合物由40-70重量%的丙烯酸单体共聚物组成。 通过混合60-90重量%的含烷氧基硅烷基的丙烯酸单体和10-40重量%的含酰胺基的丙烯酸类单体得到丙烯酸单体共聚物。 涂料组合物由15-35重量%的丙烯酸树脂组合物,20-40重量%的环氧树脂组合物,30-54重量%的有机溶剂和1-5重量%的添加剂组成。

    자동차 프리코티드 도료용 후막형 프라이머 제조를 위한 수지 혼합 조성물 및 제조방법
    6.
    发明公开
    자동차 프리코티드 도료용 후막형 프라이머 제조를 위한 수지 혼합 조성물 및 제조방법 有权
    适用于汽车预涂涂料的高级建筑材料树脂的树脂混合及合成方法

    公开(公告)号:KR1020120064832A

    公开(公告)日:2012-06-20

    申请号:KR1020100126058

    申请日:2010-12-10

    CPC classification number: C09D167/04 B05D7/14 C08G18/28 C09D175/06

    Abstract: PURPOSE: A resin mixture composition and a manufacturing method thereof are provided to be used for vehicle free coated paint manufacturing and to improve water resistance, corrosion resistance, weatherability, workability, and shock resistance. CONSTITUTION: A resin mixture composition comprises highly flexible polyester polyol resin, caprolactone-modified resin, and urethane-modified polyester blocked resin. A manufacturing method of highly flexible polyester polyol resin comprises the following steps: a step of mixing 20-25 parts by weight of trimethyl propanediol, 18-20 parts by weight of neopentyl glycol, and 8-9 parts by weight of adipic acid, 20-25 parts by weight of isophthalic acid, and 0.1-0.2 parts by weight of dibutyltin oxide which is an esterification catalyst; a step of obtaining a synthesized material by performing esterification at 200~220 deg. Celsius; and a step of diluting synthesized material into 20-30 parts by weight of propylene carbonate.

    Abstract translation: 目的:提供一种树脂混合物组合物及其制造方法,用于无车辆涂料涂料制造,并提高耐水性,耐腐蚀性,耐候性,可加工性和抗冲击性。 构成:树脂混合物组合物包含高度柔性的聚酯多元醇树脂,己内酯改性树脂和氨基甲酸酯改性聚酯封端树脂。 高柔性聚酯多元醇树脂的制造方法包括以下步骤:将20-25重量份的三甲基丙二醇,18-20重量份的新戊二醇和8-9重量份的己二酸,20 -25重量份间苯二甲酸和0.1-0.2重量份作为酯化催化剂的二丁基氧化锡; 通过在200〜220℃进行酯化获得合成材料的步骤。 摄氏度; 和将合成的材料稀释成20-30重量份的碳酸亚丙酯的步骤。

    자동차용 듀얼 경화 이액형 클리어 코트 조성물

    公开(公告)号:KR101052223B1

    公开(公告)日:2011-07-27

    申请号:KR1020090117205

    申请日:2009-11-30

    Abstract: 본 발명은 수산화기와 올리고머기를 갖는 아크릴 수지, 반응 희석제 광개시제, 열개시제, 자외선 흡수제, 자외선 안정제, 레벨링제, 반응 촉진제 및 용제로 이루어지는 주제와, 경화제로 이루어지는 것을 특징으로 하는 자동차용 듀얼 경화 이액형 클리어 코트 조성물에 관한 것이다.
    그리고 본 발명은 수산화기와 올리고머기를 갖는 아크릴 수지를 사용함으로써 수산화기-이소시아네이트 우레탄 결합을 통한 내산성 및 내스크래치성 등의 기계적 물성을 만족하여 기존의 아크릴-멜라민 타입의 클리어 의 물성을 재현하고, 또한 기존의 자외선 경화의 지나친 단단함 보다는 스크래치와 내산성을 고르게 만족하여 보다 나은 물리적 및 기계적 특성을 구현함과 동시에 클리어 코트의 경화는 열경화 및 자외선 경화를 동시에 적용하므로써, 자동차 내부 자외선이 조사되지 않는 쉐도우 영역에서도 원할한 클리어 코트 도막을 형성할 수 있는 장점이 있다.
    또한, 본 발명은 자외선을 1분 이상 조사하고, 자외선이 도달되지 않은 쉐도우 영역을 경화시키기 위해 100~120℃에서 30분 이상의 열경화를 실시해야 하거나, 1분 이상의 자외선을 조사하여야 하는 자외선 경화해야 하는 종래의 클리어 코트 조성물에 비해 단축된 10~15분 이내의 열경화 및 30초 정도의 매우 짧은 자외선 경화 반응으로 균일한 클리어 코트 도막을 형성할 수 있어 작업 공정 시간 단축뿐만 아니라, 에너지 절감과 유해 가스 발생을 감소시킬 수 있는 장점이 있다.
    자동차, 상도도장, 클리어 코트, 아크릴 수지, 반응성 희석제, 광개시제, 열개시제, 듀얼 경화, 쉐도우 영역(shadow zone)

    후도막 일액형 폴리우레탄 도료 조성물
    8.
    发明授权
    후도막 일액형 폴리우레탄 도료 조성물 有权
    单组分型聚氨酯涂料组合物形成厚度薄膜

    公开(公告)号:KR101029489B1

    公开(公告)日:2011-04-18

    申请号:KR1020080113282

    申请日:2008-11-14

    Abstract: 본 발명은 폴리에스테르폴리올 수지와 블록폴리이소시아네이트 수지 및 폴리우레탄 수지의 혼합수지에 무기계 피그먼트, 기타 첨가제 및 고비점의 신너를 첨가하여 이루어진 것을 특징으로 하는 후도막 일액형 폴리우레탄 수지 조성물 및 이를 포함한 도료 조성물에 관한 것으로, 후도막 작업에 대한 우수한 작업성을 가지고 있고, 또한 내수성, 내식성, 내후성, 가공성 및 충격성 등의 물성이 우수하고, 또한 기존 제품과 동등한 물성을 보유한 상태에서 다양한 후도막 두께의 도장이 가능해져 폭 넓은 건축내외장용 코일 강판을 생산 할 수 있게 되어 새로운 수요 창출이 가능한 것이 장점이다.
    후도막, 일액형, 폴리우레탄 수지, 도료 조성물, 일액형, 폴리에스테르폴리올, 이소시아네이트

    도료 조성물
    9.
    发明公开
    도료 조성물 无效
    涂料组合物

    公开(公告)号:KR1020000041335A

    公开(公告)日:2000-07-15

    申请号:KR1019980057186

    申请日:1998-12-22

    CPC classification number: C09D123/28 C09D5/00 C09D123/286 C09D133/00

    Abstract: PURPOSE: A paint composition is provided which has excellency in weather resistance, gasoline resistance, scratch resistance and painting workability, and permits direct painting without a surface treatment such as flame treatment, ozone treatment, corona-discharge treatment and plasma treatment, thereby contributing to improvement in environmental problem (reduction of waste water at the time of painting) and cost. CONSTITUTION: A paint composition comprises 80 - 90 parts by weight of a composition consisting of 15 - 30 parts by weight of an acrylic polyol, 20 - 35 parts by weight of a chlorinated polyolefin effective in improving adhesion to a polyolefin resin, and various additives added thereto, and 10 - 20 parts by weight of a polyisocyanate.

    Abstract translation: 目的:提供耐候性,耐汽油性,耐刮擦性和喷涂加工性优异的涂料组合物,并且允许直接喷涂而不进行火焰处理,臭氧处理,电晕放电处理和等离子体处理等表面处理,从而有助于 改善环境问题(减少喷漆时的废水)和成本。 构成:涂料组合物包含80-90重量份的由15-30重量份丙烯酸多元醇组成的组合物,20-35重量份有效提高与聚烯烃树脂粘附性的氯化聚烯烃和各种添加剂 和10〜20重量份的多异氰酸酯。

    이액형 열경화성 도료조성물
    10.
    发明授权
    이액형 열경화성 도료조성물 失效
    双组分型热固化涂料组合物

    公开(公告)号:KR101365053B1

    公开(公告)日:2014-02-21

    申请号:KR1020120001080

    申请日:2012-01-04

    Abstract: 본 발명은 이액형 열경화성 도료조성물에 관한 것으로, 더욱 상세하게는 주제와 경화제를 포함하는 이액형 도료 조성물을 제조하되, 먼저 주제(a)로써, 측쇄 말단에 인산기가 부가된 아크릴 단량체, 수산기를 갖는 아크릴 단량체 및 비관능성 아크릴 단량체를 이용하여 제조된 인산기 함유 아크릴 수지 조성물을 적용하고, 다음으로 경화제(b)로써, 측쇄 말단에 글리시딜기가 부가된 아크릴 단량체, 비 관능성 아크릴 단량체를 이용하여 제조된 글리시딜기 함유 아크릴 수지 조성물 및 1종 이상의 디이소시아네이트 또는 폴리이소시아네이트로 구성된 우레탄 경화제를 적용함으로써, 상기 종래기술과 같은 단순한 기계적 부착 외에 추가로 화학적 부착이 가능하여 매우 다양한 소재에 대한 도료의 부착성에 대한 활용이 가능하고, 글리시딜기가 부가된 아크릴 단량체와 비관능성 아크릴 단량체를 이용하므로 균일한 최종 물성을 가진 아크릴레이트 수지 조성물의 제조가 가능할 수 있도록 하고, 아울러, 상기 종래기술과 같은 전처리 공정(인산기와 글리시딜기를 미리 반응시키는 공정) 없이, 글리시딜기를 따로 분리하여 우레탄 경화제에 혼합하여 도막의 소부 과정에서 부가되는 열을 이용하여 글리시딜기와 인산기가 반응됨에 따라 강한 화학적 부착을 추가로 구현할 수 있도록 하며, 또한, 글리시딜기가 부가된 아크릴 단량체의 함량을 손쉽게 조절하여 제조가 가능하므로 우레탄 경화제에 브랜딩하는 글리시딜기 함유 아크릴레이트 수지 조성물의 함량을 손쉽게 조절가능하며, 이로 인해 주제의 인산기와 반응할 수 있는 충분한 글리시딜기를 용이하게 조절하여 포함시킬 수 있도록 하고, 상기와 같은 주제(a)와 경화제(b)를 이용하여 이액형 도료 조성물(A)을 제조함으로써, 일반적인 경화제의 이소시아네이트와 주제의 수산기 간의 우레탄 반응에 추가로, 도막의 소부 과정에서 인산기와 글리시딜기의 반응을 통해 얻어지는 가교 결합으로 인해 일반적인 우레탄 경화제를 사용한 도료의 도막 경도에 비해 우수한 경도의 경화도막을 확보할 수 있도록 하며, 아울러, 일반적으로 도료의 부착성이 개선되면 내식성, 내화학성, 내알칼리성, 내염수 분무성 등의 전반적인 도료 물성의 향상을 달성할 수 있는데, 본 발명은 기존의 도료가 보여주는 부착성능보다 향상된 부착성능을 구현할 수 있음에 따라 상기와 같은 도료의 제반 물성을 더욱 향상시킬 수 있도록 하고, 또한, 도료에 있어 경화 도막의 경도 개선은 가공성과 굴곡성등과 같은 도막의 유연성이 필요한 도막 특성과는 반대적인 특성이나, 상기와 같은 주제(a)와 경화제(b)를 이용하여 제조된 이액형 도료 조성물(A)은 기계적, 화학적 부착과 가교밀도의 증가를 통해 도막 경도가 개선됨에 따라 가공성 및 굴곡성 등의 도막 특성까지 종래의 도료에 비해 매우 개선될 수 있도록 할 뿐만 아니라 금속, 비철금속, 유리, 프라스틱등 도료가 적용되는 다양한 소재에 매우 우수한 부착 특성을 가지기 때문에 전착 전처리 또는 기타 전처리 공정 없이 하도, 중도와 같은 도장 공정을 삭제하고, 상도 도장만으로도 양호한 부착성을 가진 도막을 형성 할 수 있도록 하는 이액형 열경화성 도료조성물에 관한 것이다.

Patent Agency Ranking