초음파 센서 소재용 무연 압전 세라믹스 조성물
    1.
    发明公开
    초음파 센서 소재용 무연 압전 세라믹스 조성물 无效
    用于超声传感器的无铅压电陶瓷的组成

    公开(公告)号:KR1020100012199A

    公开(公告)日:2010-02-08

    申请号:KR1020080073461

    申请日:2008-07-28

    Abstract: PURPOSE: A ceramic composition of lead-free piezoelectric for the ultrasonic sensor is provided to ensure high mechanical quality factor and piezoelectric properties and to realize low-temperature sintering by adding Zn nanopowder in (Na0.5K0.5)NbO3 composition. CONSTITUTION: A ceramic composition of lead-free piezoelectric for the ultrasonic sensor comprises (Na0.5K0.5)NbO3 and 1 ~ 10 mol% of zinc(Zn) nanopowder as an additive. An average particle size of the zinc(Zn)nanopowder is 20 ~ 200nm. A ceramic composition of lead-free piezoelectric is manufactured by setting a sintering temperature to 980 ~ 1060°C and the temperature is lower than the sintering temperature of general PZT powder with 1200°C ~ 1350°C.

    Abstract translation: 目的:提供超声波传感器的无铅压电陶瓷组合物,以确保高机械品质因数和压电性能,并通过在(Na0.5K0.5)NbO3组合物中添加Zn纳米粉末实现低温烧结。 构成:用于超声波传感器的无铅压电陶瓷组合物包括(Na0.5K0.5)NbO3和1〜10mol%的锌(Zn)纳米粉末作为添加剂。 锌(Zn)纳米粉末的平均粒径为20〜200nm。 通过将烧结温度设定为980〜1060℃,温度低于1200℃〜1350℃的普通PZT粉末的烧结温度,制造无铅压电陶瓷组合物。

    초음파 진동자용 무연 압전세라믹스 조성물
    2.
    发明公开
    초음파 진동자용 무연 압전세라믹스 조성물 失效
    用于超声波振动器的无铅压电陶瓷的组成

    公开(公告)号:KR1020100033002A

    公开(公告)日:2010-03-29

    申请号:KR1020080091947

    申请日:2008-09-19

    Abstract: PURPOSE: A free-lead piezoelectric ceramic composition for an ultrasonic oscillator is provided to enhance sintering property and to form the free-lead piezoelectric ceramic composition at a low sintering temperature. CONSTITUTION: A free-lead piezoelectric ceramic composition for an ultrasonic oscillator is composed of (Na0.5K0.5)NbO3. An additive which is added to the composition contains 0.1 ~ 3 mol% of metal oxide selected from Fe2O or NiO and 0.1 ~ 3 mol% of metal oxide selected from MnCO3 or CuO. A sintering temperature of the free-lead piezoelectric ceramic composition which is composed of (Na0.5K0.5)NbO3 is 1000 ~ 1075°C.

    Abstract translation: 目的:提供一种用于超声波振荡器的自由铅压电陶瓷组合物,以提高烧结性能,并在低烧结温度下形成自由铅压电陶瓷组合物。 构成:用于超声波振荡器的自由铅压电陶瓷组合物由(Na0.5K0.5)NbO3组成。 添加到组合物中的添加剂含有选自Fe 2 O或NiO的0.1〜3mol%的金属氧化物和选自MnCO 3或CuO的0.1〜3mol%的金属氧化物。 由(Na0.5K0.5)NbO3组成的自由铅压电陶瓷组合物的烧结温度为1000〜1075℃。

    초음파 진동자용 무연 압전세라믹스 조성물
    3.
    发明授权
    초음파 진동자용 무연 압전세라믹스 조성물 失效
    超声波振动器无铅压电陶瓷的组成

    公开(公告)号:KR101043041B1

    公开(公告)日:2011-06-21

    申请号:KR1020080091947

    申请日:2008-09-19

    Abstract: 본 발명은 초음파 진동자용 무연 압전세라믹스 조성물에 관한 것으로서, (Na
    0.5 K
    0.5 )NbO
    3 압전 세라믹스에 소결 첨가제 CuO, NiO, Fe
    2 O
    3 , MnCO
    3 등을 첨가하여 소결특성을 향상시키며, 높은 기계적 품질계수(Q
    m )와 높은 전기기계결합계수(k
    p )를 갖는 무연 압전세라믹스 조성물을 낮은 소결 온도에서 제공하는 것에 관한 것이다.
    무연 압전 세라믹스, 전기기계결합계수, 기계적 품질계수, 초음파 진동자