公开(公告)号:JP4641316B2
公开(公告)日:2011-03-02
申请号:JP2007528178
申请日:2006-04-19
Applicant: 黒崎播磨株式会社
IPC: C04B35/00 , C04B35/101
CPC classification number: C04B35/013 , B82Y30/00 , C04B35/103 , C04B35/63 , C04B35/66 , C04B2235/3217 , C04B2235/3241 , C04B2235/3244 , C04B2235/3272 , C04B2235/3275 , C04B2235/3289 , C04B2235/402 , C04B2235/404 , C04B2235/405 , C04B2235/424 , C04B2235/425 , C04B2235/428 , C04B2235/441 , C04B2235/444 , C04B2235/48 , C04B2235/5248 , C04B2235/5288 , C04B2235/5436 , C04B2235/5445 , C04B2235/96 , C04B2235/9607 , C04B2235/9669
-
-
-
公开(公告)号:JP4433514B2
公开(公告)日:2010-03-17
申请号:JP12390299
申请日:1999-04-30
IPC: B01D19/00 , C21C7/10 , C04B35/043 , C21C7/00 , F27D1/00
Abstract: PROBLEM TO BE SOLVED: To improve wear resistance of magnesia-carbon unburned refractory brick without adversely affecting corrosion resistance and spalling resistance of the brick. SOLUTION: This refractory brick has a blending composition that comprises a refractory aggregate composition containing 1-12 wt.% of thin expanded graphite having a
-
公开(公告)号:JP4394144B2
公开(公告)日:2010-01-06
申请号:JP2007526071
申请日:2006-07-21
Applicant: 黒崎播磨株式会社
CPC classification number: C04B35/043 , C04B35/013 , C04B35/103 , C04B35/6269 , C04B35/62839 , C04B35/634 , C04B2235/3821 , C04B2235/401 , C04B2235/402 , C04B2235/425 , C04B2235/428 , C04B2235/5436 , C04B2235/96 , C04B2235/9669 , C04B2235/9676
-
公开(公告)号:JPWO2006112485A1
公开(公告)日:2008-12-11
申请号:JP2007528178
申请日:2006-04-19
Applicant: 黒崎播磨株式会社
CPC classification number: C04B35/013 , B82Y30/00 , C04B35/103 , C04B35/63 , C04B35/66 , C04B2235/3217 , C04B2235/3241 , C04B2235/3244 , C04B2235/3272 , C04B2235/3275 , C04B2235/3289 , C04B2235/402 , C04B2235/404 , C04B2235/405 , C04B2235/424 , C04B2235/425 , C04B2235/428 , C04B2235/441 , C04B2235/444 , C04B2235/48 , C04B2235/5248 , C04B2235/5288 , C04B2235/5436 , C04B2235/5445 , C04B2235/96 , C04B2235/9607 , C04B2235/9669
Abstract: 耐酸化性を低下させることなく耐熱衝撃性、耐摩耗性、耐食性を高めることのできる炭素含有耐火物を提供する。耐火骨材、炭素基質原料、及び前記耐火骨材又は前記炭素基質原料の間を結合するカーボンボンドで構成された炭素含有耐火物において、前記カーボンボンドに、粒子径が1000nm以下の遷移金属を含む遷移金属含有ナノ粒子を分散された状態で含有させた。これを熱処理すれば、カーボンボンド内部に直径50nm以下の炭素繊維状組織の柔構造が形成され、高強度化、低弾性率化、及び低熱膨張率化が図られる。従って、耐熱衝撃性、耐摩耗性、耐食性の高い炭素含有耐火物が提供される。
-
-
公开(公告)号:JP5016609B2
公开(公告)日:2012-09-05
申请号:JP2008543081
申请日:2007-11-06
Applicant: 黒崎播磨株式会社
IPC: C04B35/043 , C21C5/44 , C21C5/46 , F27D3/14
CPC classification number: C04B35/043 , B22F2003/248 , B22F2998/10 , C04B35/013 , C04B35/0435 , C04B35/62665 , C04B35/63496 , C04B2235/3206 , C04B2235/3217 , C04B2235/3222 , C04B2235/3244 , C04B2235/3418 , C04B2235/3804 , C04B2235/3808 , C04B2235/3813 , C04B2235/3821 , C04B2235/3826 , C04B2235/401 , C04B2235/402 , C04B2235/404 , C04B2235/421 , C04B2235/422 , C04B2235/424 , C04B2235/425 , C04B2235/428 , C04B2235/48 , C04B2235/5292 , C04B2235/5427 , C04B2235/5436 , C04B2235/5472 , C04B2235/77 , C04B2235/94 , C04B2235/95 , C04B2235/96 , C21C5/4653 , C22C29/12 , F27D1/0006 , C22C1/05 , B22F1/0059 , B22F3/04 , B22F3/24
-
公开(公告)号:JP4856513B2
公开(公告)日:2012-01-18
申请号:JP2006284094
申请日:2006-10-18
Applicant: 黒崎播磨株式会社
IPC: C04B35/00 , C04B35/043 , C04B35/103 , F27D1/00
Abstract: PROBLEM TO BE SOLVED: To provide a carbon-containing refractory having excellent slag resistance as well as excellent thermal shock resistance by a means where uniform dispersion is relatively simply made possible when carbon nanofibers are dispersed into a refractory for reducing carbon in a carbon-containing refractory. SOLUTION: Using, as raw materials, a catalyst-covered refractory raw material in which the surface of a refractory raw material is coated with one or more kinds of metals selected from the group consisting of V, Fe, Co, Ni, Cu, Mo, Pd, Rh, W and Pt, the oxide or metal salt of the metal(s), and an organic polymer resin or the precursor thereof, they are kneaded, molded and heat-treated, so as to be a nanocarbon-containing refractory in which nanocarbon tubes are uniformly dispersed into the structure. COPYRIGHT: (C)2008,JPO&INPIT
-
公开(公告)号:JP4791761B2
公开(公告)日:2011-10-12
申请号:JP2005151442
申请日:2005-05-24
Applicant: 黒崎播磨株式会社
IPC: C04B35/00 , B22D11/10 , C01B31/02 , C04B35/043 , F27D1/00
CPC classification number: B82Y30/00
Abstract: PROBLEM TO BE SOLVED: To provide a carbon-containing refractory having both excellent strength and thermal shock resistance, keeping excellent slag infiltration resistance and having sufficient durability. SOLUTION: The carbon-containing refractory is produced by adding ≤5 mass% fullerene in outer percentage and 0.5-5 mass% pitch in outer percentage with a thermosetting organic resin as an organic binder into magnesia based, spinel based, alumina based refractory raw material powder, kneading, forming and heat-treating. In the carbon-containing refractory, carbon nanofiber having 5-10 nm diameter and 100-300 nm length and is present in a bonded structure and the carbon-containing refractory is used suitably for a dipping nozzle or a long nozzle. COPYRIGHT: (C)2006,JPO&NCIPI
-
-
-
-
-
-
-
-
-