직접 및 간접가열 방식을 겸한 폐타이어의 감압 열분해 방법과장치
    1.
    发明授权
    직접 및 간접가열 방식을 겸한 폐타이어의 감압 열분해 방법과장치 有权
    使用直接和间接加热的废轮胎的真空热解方法和设备

    公开(公告)号:KR100305113B1

    公开(公告)日:2001-09-13

    申请号:KR1019990015670

    申请日:1999-04-30

    Abstract: 본발명은폐타이어를열분해하여생성가스를응축, 오일화하기위하여직접가열과간접가열을연속적으로할 수있는방법과장치에관한것이다. 현재까지개발된폐타이어열분해공정을크게구분하면 1)폐타이어가들어있는반응기내로연소가스및 가열가스를직접주입시키는직접가열방식과 2) 폐타이어가들어있는반응기의외벽을가열하는간접가열방식이있다. 전자의경우는연소가스를직접주입함에따라에너지소모는적은반면과잉공기(산소)의주입에따른열분해생성오일수율의감소및 반응기폭발의위험성이있으며후자의경우는안전한공정의운전및 안정적인생성오일의수율유지등의장점이있으나 50% 미만의저에너지효율에의한단점이있다. 따라서본 발명은도 1의공정도와같이두가지의장점을혼합한연결공정을고안되었으며에너지를많이소모하는 1단계의폐타이어열분해직전온도(300℃)까지는직접가열방식을사용하고그 후 2단계에서는열매체유(Heat Medium Oil)에의한간접가열을실시함으로서안전한운전및 열분해오일의고수율이유지되도록하였다.

    직접 및 간접가열 방식을 겸한 폐타이어의 감압 열분해 방법과장치
    2.
    发明公开
    직접 및 간접가열 방식을 겸한 폐타이어의 감압 열분해 방법과장치 有权
    用于减少包含两种直接和间接加热方法的废弃轮胎的热分解的方法和装置

    公开(公告)号:KR1020000067663A

    公开(公告)日:2000-11-25

    申请号:KR1019990015670

    申请日:1999-04-30

    Abstract: PURPOSE: A method and apparatus capable of carrying out safe operation and maintaining high yield by using a direct heating method just before a thermal decomposition of natural rubber begins and then using an indirect heating method by heat medium oil in the process of carrying out a pressure reduction thermal decomposition of waste tire are provided which reduce operation and equipment cost. CONSTITUTION: In a thermal decomposition process of waste tire that recoveries oil by thermal cracking waster tire, waste tires are directly heated using combustion gas until a temperature in a waste tire charged reactor reaches 300°C and then they are indirectly heated using heat medium oil heated in a heating furnace. The method can reduce the capacity of a vacuum pump to 1/2 or lower as compared with that of a direct heating method.

    Abstract translation: 目的:一种在天然橡胶开始热分解之前使用直接加热方法进行安全操作并保持高产率的方法和装置,然后在进行压力的过程中使用间接加热方法 提供废轮胎的还原热分解,降低了操作和设备成本。 构成:在通过热裂纹轮胎回收油的废轮胎的热分解过程中,废轮胎使用燃烧气体直接加热直到废轮胎加载反应器中的温度达到300℃,然后使用热介质油间接加热 在加热炉中加热。 与直接加热方法相比,该方法可以将真空泵的容量降低到1/2或更低。

    폐타이어 열분해 카본블랙의 고품위화를 위한 가공방법.
    4.
    发明申请
    폐타이어 열분해 카본블랙의 고품위화를 위한 가공방법. 审中-公开
    通过在废弃轮胎上进行热分解过程生产的炭黑加工处理方法

    公开(公告)号:WO2011074811A2

    公开(公告)日:2011-06-23

    申请号:PCT/KR2010/008643

    申请日:2010-12-03

    Inventor: 정수현 나정걸

    Abstract: 본 발명은 폐타이어 열분해 카본블랙의 고품위화를 위한 가공방법에 관한 것으로, 더욱 상세하게는 폐타이어의 열분해 후 생성되는 카본블랙을 자석식 분리기 및 비중 분리기 등을 이용하여 철심 및 섬유질을 제거한 후, 미분쇄, 가열 및 산처리를 통해 카본블랙의 고품위화를 유도하는 것이다. 본 발명의 폐타이어 열분해 카본블랙의 고품위화를 위한 가공방법은, 폐타이어의 열분해를 통해 얻어진 카본블랙을 산용액으로 처리하여 카본블랙 중의 무기물이 무기염으로 생성되도록 하는 무기염 생성단계를 포함하여 이루어지는 것을 특징으로 한다.

    Abstract translation: 本发明涉及一种通过对废轮胎进行热解处理而生产的炭黑的升级处理方法,更具体地,涉及一种使用磁选机和重力分离器除去来自炭黑的铁丝和纤维的方法 通过对废轮胎进行热解处理而制造,对炭黑进行精细研磨处理,加热处理和酸处理,从而提高炭黑的质量。 通过对根据本发明的废轮胎进行热解处理而生产的炭黑的升级处理方法包括无机盐生产步骤,用酸溶液处理对废轮胎进行热解过程产生的炭黑,以便 从碳黑中含有的无机物生成无机盐。

    초중질원유의 정제방법 및 초중질원유의 정제장치
    5.
    发明授权
    초중질원유의 정제방법 및 초중질원유의 정제장치 有权
    超重油的净化方法和超重油的净化装置

    公开(公告)号:KR101239083B1

    公开(公告)日:2013-03-06

    申请号:KR1020100030421

    申请日:2010-04-02

    Abstract: 본 발명은 추출탑 내부에 고전압의 전기장을 인가하여 초중질원유 내 아스팔텐을 효과적으로 제거하는 초중질원유의 정제방법 및 정제장치에 관한 것으로, 더욱 상세하게는 탄소수 3~8개의 탄화수소로 구성된 용매와 초중질원유를 혼합하고 이에 고전압의 전기장을 인가하여 초중질원유 내의 아스팔텐 분산 특성을 변화시킴으로써 초중질원유의 응집을 유도하고 이와 동시에 용매와 초중질원유의 접촉을 원활히 하여 용매 추출 효과를 극대화한 다음, 전기장 인가를 중지하여 상부의 아스팔텐 제거 오일 층과 하부의 아스팔텐 층으로 분리시킴으로써 아스팔텐이 제거된 원유를 회수하는 방법 및 장치에 관한 것이다.
    즉, 본 발명은 간단한 공정 구성과 온화한 조업 조건을 특징으로 하므로 기존의 탈아스팔텐 용매 추출 공정이 안고 있던 막대한 장치비 및 에너지 다소비 문제를 해결하여 초중질원유 고도화에 소요되는 설치, 운전 비용을 감소할 수 있는 것이다.

    석탄비산재를 이용한 폐플라스틱 열분해용 비정질 실리카알루미나 촉매의 제조공정
    6.
    发明公开
    석탄비산재를 이용한 폐플라스틱 열분해용 비정질 실리카알루미나 촉매의 제조공정 有权
    来自煤粉的非晶二氧化硅 - 氧化铝催化剂的生产工艺用于催化热分解

    公开(公告)号:KR1020120139276A

    公开(公告)日:2012-12-27

    申请号:KR1020110059000

    申请日:2011-06-17

    Inventor: 정수현 나정걸

    CPC classification number: B01J37/06 B01J21/12 B01J37/08 B09B3/00

    Abstract: PURPOSE: A manufacturing process of amorphous silica alumina catalysts for pyrolyzing waste plastic using coal fly ash is provided to repeatedly pulverize coal fly ash and alkali and high temperature plasticizing the resultant product of the coal fly ash and the alkali. CONSTITUTION: A manufacturing process of amorphous silica alumina catalysts for pyrolyzing waste plastic using coal fly ash includes the following steps: coal fly ash and alkali are pulverized using a fine pulverizer; the primarily pulverized fly ash and alkali is primarily plasticized; the primarily plasticized product is secondarily pulverized; the secondarily pulverized product is washed; and the washed product is secondarily plasticized to obtain amorphous pyrolysis catalyst. [Reference numerals] (AA) Primary pulverizing process; (BB) Primary high temperature plasticizing process; (CC) Secondary pulverizing process; (DD) Coal fly ash, alkali; (EE) Ammonium chloride supplying bath; (FF) Raw material supplying unit; (GG) Dehydrated liquid; (HH) Solid-liquid separator; (II) Completely filtered product; (JJ) Amorphous silica alumina catalyst; (KK) Secondary high temperature plasticizing process; (LL) Supplementary water supplying bath; (MM) Supplementary water supplying pump; (NN) Washing process; (OO) Circulating pump; (PP) Acid; (QQ) Draining; (RR) Adjusting bath; (SS) Exhausting pump

    Abstract translation: 目的:提供使用煤飞灰热解废塑料的无定形二氧化硅氧化铝催化剂的制造工艺,以反复粉碎煤飞灰和碱,并高温地对煤飞灰和碱的产物进行增塑。 构成:使用煤飞灰热解废塑料的无定形二氧化硅氧化铝催化剂的制造方法包括以下步骤:使用细粉碎机将煤飞灰和碱粉碎; 主要粉碎的粉煤灰和碱主要被塑化; 将主要增塑的产品二次粉碎; 将二次粉碎的产物洗涤; 将洗涤后的产物二次塑化,得到无定形热解催化剂。 (附图标记)(AA)一次粉碎工序; (BB)初级高温塑化工艺; (CC)二次粉碎工艺; (DD)煤飞灰,碱; (EE)氯化铵供应浴; (FF)原料供应单元; (GG)脱水液体; (HH)固液分离器; (二)完全过滤产品; (JJ)无定形二氧化硅氧化铝催化剂; (KK)二次高温塑化工艺; (LL)补充供水浴; (MM)补充供水泵; (NN)洗涤过程; (OO)循环泵; (PP)酸; (QQ)排水; (RR)调节浴; (SS)排气泵

    생물체 유래 지질의 탈산소 반응 공정에서 반응 산물 내 산소 함량의 실시간 분석 방법
    8.
    发明公开

    公开(公告)号:KR1020120054990A

    公开(公告)日:2012-05-31

    申请号:KR1020100116426

    申请日:2010-11-22

    Abstract: PURPOSE: A real time analysis method the oxygen content in a reaction product in an organism originated lipid deoxygenation reaction process is provided to easily and rapidly measure the oxygen content in a reaction product which is a performance index and a key of a deoxygenation reaction so that a real time diagnosis can be easy. CONSTITUTION: A real time analysis method the oxygen content in a reaction product in an organism originated lipid deoxygenation reaction process is as follows. A part of a reaction product is inserted into a Fourier transform infrared rays analysis device. The oxygen content is calculated by converting measured an absorbance with respect to a carbonyl functional group at a specific frequency into the oxygen content. The measured absorbance with respect to the carbonyl functional group is 1,720cm. The absorbance with respect to the carbonyl functional group is converted so that the oxygen content is calculated according to a predetermined equation.

    Abstract translation: 目的:实时分析方法,提供生物体中产生的反应产物中的氧含量来自脂质脱氧反应过程,以容易且快速地测量作为性能指标和脱氧反应关键的反应产物中的氧含量,使得 实时诊断可以很容易。 构成:实时分析方法,生物体中反应产物中的氧含量起源于脂质脱氧反应过程如下。 将反应产物的一部分插入傅里叶变换红外线分析装置。 通过将特定频率处的相对于羰基官能团的吸光度测定为氧含量来计算氧含量。 测定的相对于羰基官能团的吸光度为1720cm。 转化相对于羰基官能团的吸光度,使得根据预定方程计算氧含量。

    초중질원유의 경질화 방법
    10.
    发明公开
    초중질원유의 경질화 방법 无效
    升级超重油原油的方法

    公开(公告)号:KR1020110111588A

    公开(公告)日:2011-10-12

    申请号:KR1020100030734

    申请日:2010-04-05

    CPC classification number: C10G21/18 C10G21/02 C10G2300/1077 C10G2300/201

    Abstract: 본 발명은 특정의 용매인 화학식 1의 용매를 사용하여 상온(15~30)에서 초중질원유를 용해시키고, 극성 유기용매와 비극성 용매를 가함으로써 초중질원유를 경질화하는 방법에 관한 것으로서, 더욱 상세하게는 상온(15~30)에서 오일샌드 비튜멘, 천연역청, 감압잔사유 등의 초중질원유에 특정의 용매 및 극성 유기용매를 가하여, 상부의 아스팔텐 분산제와 극성 유기용매, 레진 성분이 용해된 극성 유기용매층과 하부의 고농축 초중질원유 층으로 분리한 다음, 하부에 탄화수소비극성 유기용매를 가하여 다시 상부의 탈아스팔텐 오일 층과 하부의 아스팔텐 층으로 분리함으로써 초중질원유를 경질화하는 방법에 관한 것이다.
    즉, 본 발명은 기존의 초중질원유의 경질화공정이 안고 있던 막대한 장치비 및 에너지 다소비 문제를 해결하여 초중질원유의 경질화에 소요되는 설치, 운전 비용을 감소할 수 있는 것이다.

Patent Agency Ranking