公开(公告)号:JPH06157024A
公开(公告)日:1994-06-03
申请号:JP13724591
申请日:1991-05-13
Applicant: AGENCY IND SCIENCE TECHN
Inventor: SHIBAZAKI YASUO , WATAMURA SHINJI , ITO HIROSHI , TONE YUKIHITO , KUMAGAI NOBUFUMI
IPC: C01B33/26 , C04B35/00 , C04B35/18 , C04B35/628
Abstract: PURPOSE:To produce the subject mineral moldable without requiring addition of an organic additive by applying a hydrothermal treatment to a powdery two-component system mineral of silica-alumina in an acidic or neutral solution and forming a thin kaolinite film. CONSTITUTION:A powdery two-component system mineral of silica-alumina such as mullite and an acidic or neutral solution is tightly sealed in a pressure tank such as an autoclave. A hydrothermal reaction is carried out by heating to convert the surface of the powdery mineral into a clay-like material exhibiting plasticity. The particle size of the powdery mineral is not especially restricted and about 3 to 10mum is preferable. As the condition of the hydrothermal reaction, the reaction temperature is preferably 200 to 250 deg.C in the case of 7 day reaction period and the most favorable result can be obtained especially at about 230 deg.C. Further, an acidic solution is preferably used as the solution and a 0.1 N to 0.01 N hydrochloric acid solution is especially preferable. As the result of this hydrothermal treatment, a thin kaolinite film can be formed on the surface of a mineral such as mullite.