公开(公告)号:DE4123051A1
公开(公告)日:1993-01-14
申请号:DE4123051
申请日:1991-07-12
Applicant: BASF AG
-
公开(公告)号:DE3834547A1
公开(公告)日:1990-04-19
申请号:DE3834547
申请日:1988-10-11
Applicant: BASF AG
-
公开(公告)号:DE4007767A1
公开(公告)日:1991-09-19
申请号:DE4007767
申请日:1990-03-12
Applicant: BASF AG
Inventor: BOHNET SIEGBERT DR , GOERRISSEN HEINER DR , HILT ALBRECHT DR , SAENGER DIETRICH DR
-
-
公开(公告)号:DE4030694A1
公开(公告)日:1992-04-02
申请号:DE4030694
申请日:1990-09-28
Applicant: BASF AG
Inventor: MC KEE GRAHAM EDMUND DR , GOETZ WALTER DR , BOHNET SIEGBERT DR , ZEINER HARTMUT DR
Abstract: Thermoplastic moulding compositions based on A) from 2 to 97.5% by weight of polyoxymethylene homopolymer or copolymer, B) from 2 to 97.5% by weight of a polyamide, C) from 0.5 to 25% by weight of a product of the polycondensation of 2,2-di(4-hydroxyphenyl)propane and epichlorohydrin, D) from 0 to 60% by weight of an impact-modifying polymer, E) from 0 to 60% by weight of fibrous or particulate fillers or mixtures thereof.
-
6.
公开(公告)号:DE3802753A1
公开(公告)日:1989-08-10
申请号:DE3802753
申请日:1988-01-30
Applicant: BASF AG
Inventor: GOERRISSEN HEINER DR , BOHNET SIEGBERT DR , HEINZ GERHARD DR , SAENGER DIETRICH DR
Abstract: The invention relates to impact-resistant polymer moulding compositions based on (A) polyoxymethylenes, (B) thermoplastic polyurethanes and (C) polyalkylene terephthalates and optionally (D) additives, which expediently comprise from 95 to 40 parts by weight of at least one polyoxymethylene homopolymer and/or copolymer (A), from 5 to 60 parts by weight of a mixture of from 60 to 98% by weight of at least one thermoplastic polyurethane (B) and from 2 to 40% by weight of at least one polyalkylene terephthalate (C), where the percentages by weight are based on the total weight of (B) and (C) and the parts by weight of (A) + (B) + (C) add up to 100 parts by weight and from 0 to 60 parts by weight of an additive (D), to a process for their preparation and to their use. In order to prepare the polymer moulding compositions, by the preferred method, components (A) to (C) and, if used, (D) are introduced individually or as mixtures, into an extruder and melted together at temperatures in the range from 150 to 260@C. The polymer moulding compositions are suitable for the production of films, sheeting or mouldings which are used, for example, in the vehicle, electrical appliance and electrical industries.
-
公开(公告)号:DE3729144A1
公开(公告)日:1989-03-09
申请号:DE3729144
申请日:1987-09-01
Applicant: BASF AG
Inventor: BRONSTERT KLAUS DR , BOHNET SIEGBERT DR , HIMMELE WALTER DR , BOTT KASPAR DR
IPC: C07F1/00 , C07F1/02 , C07F1/04 , C08F4/42 , C08F4/46 , C08F4/48 , C08F12/00 , C08F12/08 , C08F36/00 , C08F36/06
Abstract: Bifunctional initiators for anionic polymerization are prepared by reacting an alkenylaromatic compound of the general formula I (I) where Ar is aromatic hydrocarbyl which may be substituted by alkyl or another group inert toward organoalkali metal compounds and may contain nitrogen, R1 is linear or branched alkyl, cycloalkyl, alkenyl or aralkyl or from 1 to 22 carbon atoms where at least the carbon adjacent to the double bond is saturated and aliphatic, R2 is hydrogen or is likewise linear or branched alkyl, cycloalkyl, alkenyl or aralkyl or from 1 to 22 carbon atoms where at least the carbon adjacent to the double bond is saturated and aliphatic, and where R1 and R2 may be part of a common cycloaliphatic ring, in the presence of one or more ethers and of tertiary amines and in the presence or absence of a further inert aliphatic, alicyclic or aromatic solvent, at from -20 DEG to +70 DEG C. with preferably lithium and with dimerization, with the use in addition of poly-cyclic aromatic hydrocarbons which catalytically promote the dimerization in amount of from 0.001 to 50, preferably 20, mol % and with or without the removal of the ethers and/or tertiary amines after the preparation, and are used for polymerizing anionically polymerizable monomers such as styrene.
-
公开(公告)号:DE4319190A1
公开(公告)日:1994-01-05
申请号:DE4319190
申请日:1993-06-09
Applicant: BASF AG
Inventor: MCKEE GRAHAM EDMUND DR , WELZ MARTIN , ZEINER HARTMUT DR , BOHNET SIEGBERT DR
Abstract: The use of polymer mixt. (I) for the prodn. of moulded prods. which are inscribed with the aid of high-energy radiation is claimed. (I) contains (A) 40-99 wt.% polyoxymethylene homo- or co-polymer, (B) 1-30 wt.% polycarbonate, (C) 0-50 wt.% impact-modifying polymer and (D) 0-50 wt.% fibrous and/or particulate fillers. The prodn. of moulded prods. with markings, comprises exposing a moulded prod. made from (I) to high-energy radiation. Also claimed are moulde prods. with markings obtd. by this process. The markings are made with laser radiation pref. using a Nd/YAG laser. USE/ADVANTAGE - The polyoxymethylene-based mouldings have a good surface structure and good contrast between markings and background.
-
公开(公告)号:DE3885646D1
公开(公告)日:1993-12-23
申请号:DE3885646
申请日:1988-03-29
Applicant: BASF AG
Inventor: BRONSTERT KLAUS DR , BOHNET SIEGBERT DR
IPC: C07F1/02 , C08C19/44 , C08F2/38 , C08F4/00 , C08F4/42 , C08F4/48 , C08F8/00 , C08F12/00 , C08F36/00 , C08F36/04 , C08F297/04
Abstract: Oligomeric polyfunctional initiators for anionic polymerization of dienes and/or alkenylaromatics are prepared by a process in which a mixture of dialkenylaromatics and alkenylaromatics in a molar ratio of from 1:4 to 1:100, in an inert solvent, is run, at from 25 DEG to 100 DEG C., continuously or in small portions, with thorough mixing, into an initially taken mixture which contains from 1.2 to 3.0 molar equivalents, based on the dialkenylaromatics, of one or more organolithium compounds and an inert solvent, and is polymerized completely. The resulting oligomeric initiators are used for the preparation of unfunctionalized or functionalized polymers or block copolymers from dienes and/or alkenylaromatics, and the functionalized polymers thus prepared are used as prepolymers for other resins.
-
公开(公告)号:DE4007766A1
公开(公告)日:1991-09-19
申请号:DE4007766
申请日:1990-03-12
Applicant: BASF AG
Inventor: BOHNET SIEGBERT DR , GOERRISSEN HEINER DR , DECKERS ANDREAS DR
Abstract: Electrically conductive polyoxymethylene moulding materials (I) are cliamed, contg. (A) 70-90 wt.% polyoxymethylene homo-or copolymer, (B) 5-26 wt.% impact modifier, (C) 4-8 wt.% conductive carbon black with BET surface area 400-1000 m2/g and (D) 0-2 wt.% polyamide and/or Bisphenol A/epichlorhydrin polycondensate. Pref. (B) is a thermoplastic polyurethane (TPU) and/or a graft copolymer rubber.
-
-
-
-
-
-
-
-
-