1.
    发明专利
    未知

    公开(公告)号:DE59107220D1

    公开(公告)日:1996-02-22

    申请号:DE59107220

    申请日:1991-03-20

    Applicant: BASF AG

    Abstract: Stabilised polyaryl ether ketone moulding compositions containing, as essential components, …… A) from 50 to 99.99% by weight of a polyaryl ether ketone prepared by electrophilic polycondensation and comprising at least 50 mol% of units of the formula I … … or ring-substituted C1- to C8-alkyl, C6- to C20-aryl or halogen derivatives thereof, where s and t may each adopt the value 0, 1, 2 or 3, and T and T' are -O- or -CO-, … B) from 0.01 to 4% by weight of at least one organic compound which has a base constant pKb of between 2 and 12 and has a boiling point of above 300 DEG C, … C) from 0 to 50% by weight of a further thermoplastic which is different from A), and … D) from 0 to 45% by weight of fibrous or particulate fillers, or mixtures thereof. …

    3.
    发明专利
    未知

    公开(公告)号:DE3880911D1

    公开(公告)日:1993-06-17

    申请号:DE3880911

    申请日:1988-07-21

    Applicant: BASF AG

    Abstract: A reinforced moulding compsn. contains (A) a polyoxymethylene (co)polymer, (B) wollastonite with average thickness not above 5 microns and average length:thickness ratio at least 5, and opt. (C) additives. Pref. the compsn. contains 95-50 pts. wt. of polyoxymethylene, 5-50 pts. of wollastonite, and 0-60 pts. of additives. The polymer has Mw 2,000-100,000, and MFI of 0.5-200 at 190 deg.C and 21.17N. The wollastonite crystals are added by means of an extruder to the polymer melt, esp. at 180-260 deg.C.

    6.
    发明专利
    未知

    公开(公告)号:DE3580516D1

    公开(公告)日:1990-12-20

    申请号:DE3580516

    申请日:1985-04-22

    Applicant: BASF AG

    Abstract: Fiber-reinforced materials are produced by a process in which a heat-stable thermoplastic aromatic polyether A which contains reactive groups, preferably nitrile groups and/or sulfur bridges and/or arylthio or alkylthio groups, if necessary together with a heat-stable thermoplastic polymer B which does not contain any reactive groups, is applied onto reinforcing fibers, the resulting semi-finished product is molded and, in the molding obtained, the plastic matrix is crosslinked so that the glass transition temperature increases and it becomes virtually insoluble.