公开(公告)号:DE10126363A1
公开(公告)日:2001-12-06
申请号:DE10126363
申请日:2001-05-30
Applicant: BASF AG
Inventor: GRENACHER ARMIN VOLKER , HEIN HANS-GEORG , STEPP HANS , FROEHLICH HANS-JUERGEN , SCHOENMANN WILLI , BORCHERT GERHARD
IPC: B01J3/04 , B01J8/00 , B01J19/26 , C07C29/141 , C07C45/50 , C07C27/20 , C07C47/02 , C07C31/125
Abstract: In the production of 6-30C aldehydes and/or alcohols (A) by hydroformylation, the reaction mixture (olefins, synthesis gas and catalysts, or their precursors) is introduced into the reactor through a nozzle with adjustable transmission cross-section. Reaction is at 120-210 deg C and 100-400 bar and the reaction mixture is introduced at high speed into a high-pressure reactor. An Independent claim is also included for a reactor for production of (A) by the new process.
-
公开(公告)号:DE59004601D1
公开(公告)日:1994-03-24
申请号:DE59004601
申请日:1990-10-26
Applicant: BASF AG
Inventor: JOERG KLAUS DR , MUELLER FRANZ-JOSEF DR , IRGANG MATTHIAS DR , MAROSI LASZLO DR , BORCHERT GERHARD
Abstract: Process for the preparation of methyl formate by reaction of methanol on copper-containing catalysts at elevated temperature and in the gas phase by using a catalyst containing, apart from 30 to 80% by weight of copper, calculated as CuO, 20 to 70% by weight of magnesium silicates, calculated as MgO plus SiO2 in which the MgO/SiO2 molar ratio is 0.3 to 1.5, and which can be additionally doped with the metals zinc, chromium and/or barium in amounts of, in each case, up to 1.5% by weight, calculated as ZnO, Cr2O3 and BaO.
-
公开(公告)号:DE3936854A1
公开(公告)日:1991-05-08
申请号:DE3936854
申请日:1989-11-06
Applicant: BASF AG
Inventor: JOERG KLAUS DR , MUELLER FRANZ-JOSEF DR , IRGANG MATTHIAS DR , MAROSI LASZLO DR , BORCHERT GERHARD
Abstract: Process for the preparation of methyl formate by reaction of methanol on copper-containing catalysts at elevated temperature and in the gas phase by using a catalyst containing, apart from 30 to 80% by weight of copper, calculated as CuO, 20 to 70% by weight of magnesium silicates, calculated as MgO plus SiO2 in which the MgO/SiO2 molar ratio is 0.3 to 1.5, and which can be additionally doped with the metals zinc, chromium and/or barium in amounts of, in each case, up to 1.5% by weight, calculated as ZnO, Cr2O3 and BaO.
-
公开(公告)号:DE10003871A1
公开(公告)日:2001-08-02
申请号:DE10003871
申请日:2000-01-28
Applicant: BASF AG
Inventor: SCHWAHN HARALD , BORCHERT GERHARD , DIEHL KLAUS , GRENACHER ARMIN VOLKER , SAUER FRIEDRICH
Abstract: The invention relates to a method for hydroformylating olefins having between 20 and 400 carbon atoms by reacting the olefins with synthesis gas in the presence of a cobalt carbonyl catalyst, by recovering the cobalt catalyst by extracting the discarded substances resulting from the reaction using an aqueous acidic solution in the presence of oxygen, and by separating the organic and aqueous phases. The inventive method is characterized in that: (a) the aqueous phase is separated away from the organic phase to the greatest possible extent by using mass forces such that the proportion of the aqueous phase dispersed in the organic phase is equal to 2 wt. % or less with regard to the organic phase, and; (b) the organic phase involved in step (a) is subjected to an electric field while effecting the coalescence of the dispersed aqueous phase. This enables the residual cobalt content in the hydroformylation product to be reduced to less than 1 ppm.
-
公开(公告)号:ES2048936T3
公开(公告)日:1994-04-01
申请号:ES90120549
申请日:1990-10-26
Applicant: BASF AG
Inventor: JOERG KLAUS DR , MUELLER FRANZ-JOSEF DR , IRGANG MATTHIAS DR , MAROSI LASZLO DR , BORCHERT GERHARD
Abstract: Process for the preparation of methyl formate by reaction of methanol on copper-containing catalysts at elevated temperature and in the gas phase by using a catalyst containing, apart from 30 to 80% by weight of copper, calculated as CuO, 20 to 70% by weight of magnesium silicates, calculated as MgO plus SiO2 in which the MgO/SiO2 molar ratio is 0.3 to 1.5, and which can be additionally doped with the metals zinc, chromium and/or barium in amounts of, in each case, up to 1.5% by weight, calculated as ZnO, Cr2O3 and BaO.
-
-
-
-