公开(公告)号:US3883468A
公开(公告)日:1975-05-13
申请号:US42602973
申请日:1973-12-19
Applicant: BASF AG
Inventor: SCHMIDT FRANZ , SCHENK WOLFGANG , WURMB ROLF , MEYER-SIMON EUGEN , THURN FRIEDRICH M , WILL WERNER
CPC classification number: C08J5/08 , C03C25/40 , C08J2359/00 , C08J2359/02
Abstract: Thermoplastic molding compositions of polyoxymethylene, glass fibers and adhesion promoting substances. The adhesion promoters used are polymeric organosilanes. The molding compositions show improved toughness and strength properties.
Abstract translation: 聚甲醛,玻璃纤维和粘附促进物质的热塑性成型组合物。 所用的粘合促进剂是聚合的有机硅烷。 成型组合物显示改进的韧性和强度性能。
-
公开(公告)号:FI885098A
公开(公告)日:1989-05-08
申请号:FI885098
申请日:1988-11-04
Applicant: BASF AG
Inventor: STREIT WERNER , SCHENK WOLFGANG , KUMMER MATTHIAS , DIX JOHANNES PETER , OFTRING ALFRED
IPC: D06L1/12 , C11D7/56 , D06L3/00 , D06L3/02 , D06L4/12 , D06M13/244 , D06M13/292 , D06L
Abstract: Process for the pretreatment of textile materials in aqueous media by alkaline scouring and/or bleaching using as auxiliary a compound of the formula I … … where R is C6-C10-alkyl, X is H, Na, K or NR R R R , and R , R , R and R are each H, C1-C4-alkyl or -CH2-CH2-OH.
-
公开(公告)号:FI885098A0
公开(公告)日:1988-11-04
申请号:FI885098
申请日:1988-11-04
Applicant: BASF AG
Inventor: STREIT WERNER , SCHENK WOLFGANG , KUMMER MATTHIAS , DIX JOHANNES PETER , OFTRING ALFRED
IPC: D06L1/12 , C11D7/56 , D06L3/00 , D06L3/02 , D06L4/12 , D06M13/244 , D06M13/292 , D06L
Abstract: Process for the pretreatment of textile materials in aqueous media by alkaline scouring and/or bleaching using as auxiliary a compound of the formula I … … where R is C6-C10-alkyl, X is H, Na, K or NR R R R , and R , R , R and R are each H, C1-C4-alkyl or -CH2-CH2-OH.
-
4.
公开(公告)号:CA1128249A
公开(公告)日:1982-07-20
申请号:CA300155
申请日:1978-03-31
Applicant: BASF AG
Inventor: SCHENK WOLFGANG , STEDEFEDER JOACHIM , LEITNER HEINZ , SCHENCK HANS-UWE
IPC: C08F220/00 , C08F220/04 , C08F220/06 , C08F220/42 , D06M15/263 , D06M15/285 , C08F220/46 , C08F220/56 , D06M15/38
Abstract: A process for sizing staple fiber yarns by applying an aqueous sizing liquor which contains an alkaline earth metal salt of a copolymer containing from 90 to 30% by weight of acrylic acid and/or methacrylic acid and from 10 to 70% by weight of acrylonitrile and/or methacrylonitrile, which copolymer has a viscosity of from 50 to 1,000 cp in 15% strength aqueous solution at 85.degree.C, and drying the treated yarns. The sized films obtained are moistureinsensitive and have good heat stability.
-
-
-