公开(公告)号:DE3700248A1
公开(公告)日:1988-07-21
申请号:DE3700248
申请日:1987-01-07
Applicant: BASF AG
Inventor: VIETMEIER JUERGEN DR , PFOEHLER PETER DR , BRAUCH GUNDO DR , DRUSCHKE WOLFGANG DR , ZOSEL ALBRECHT DR
IPC: C08L33/08 , C08F20/10 , C08F220/18 , C08L33/04 , C09J7/02 , C09J133/04 , C09J133/08 , C08J3/06 , C09J3/14
Abstract: Aqueous dispersions of copolymers having a glass transition temperature of not more than -45 DEG C. and a K value greater than 80 consist of not less than 80% by weight of acrylates of alkanols of 8 to 12 carbon atoms, from 1 to 4% by weight of alpha , beta - monoolefinically unsaturated carboxylic acids and/or their amide derivatives and from 0.1 to 3% by weight of alpha -methylstyrene, and are used for the production of self-adhesive structures having good tack at as low as -40 DEG C.
-
公开(公告)号:ES2064793T3
公开(公告)日:1995-02-01
申请号:ES91104862
申请日:1991-03-27
Applicant: BASF AG
Inventor: SEITZ FRIEDRICH DR , RUPPMICH KARL , VIETMEIER JUERGEN DR
IPC: C08L25/00 , C08L25/02 , C08L25/12 , C08L33/00 , C08L33/04 , C08L33/12 , C08L33/24 , C08L35/00 , C08L35/06 , C08L51/00 , C08L51/04 , C08L51/06
Abstract: Thermoplastic molding materials which have high gloss and are readily colored and comprise a first graft copolymer A of an elastomeric, crosslinked acrylate polymer as the graft base and a graft shell made from a vinyl-aromatic monomer and a polar, copolymerizable, ethylenically unsaturated monomer, and a second separately prepared graft copolymer B of an elastomeric crosslinked acrylate polymer as the graft base, which is different from that in A and has a larger mean particle diameter than the graft base of copolymer A, having a first graft shell of a vinyl-aromatic monomer and a second graft shell of a mixture of a vinyl aromatic monomer and a polar-copolymerizable, ethylenically unsaturated monomer, and a hard matrix C.
-
公开(公告)号:DE4011162A1
公开(公告)日:1991-10-10
申请号:DE4011162
申请日:1990-04-06
Applicant: BASF AG
Inventor: SEITZ FRIEDRICH DR , RUPPMICH KARL , VIETMEIER JUERGEN DR
IPC: C08L25/00 , C08L25/02 , C08L25/12 , C08L33/00 , C08L33/04 , C08L33/12 , C08L33/24 , C08L35/00 , C08L35/06 , C08L51/00 , C08L51/04 , C08L51/06
Abstract: Thermoplastic molding materials which have high gloss and are readily colored and comprise a first graft copolymer A of an elastomeric, crosslinked acrylate polymer as the graft base and a graft shell made from a vinyl-aromatic monomer and a polar, copolymerizable, ethylenically unsaturated monomer, and a second separately prepared graft copolymer B of an elastomeric crosslinked acrylate polymer as the graft base, which is different from that in A and has a larger mean particle diameter than the graft base of copolymer A, having a first graft shell of a vinyl-aromatic monomer and a second graft shell of a mixture of a vinyl aromatic monomer and a polar-copolymerizable, ethylenically unsaturated monomer, and a hard matrix C.
-
公开(公告)号:DE3839060A1
公开(公告)日:1990-05-31
申请号:DE3839060
申请日:1988-11-18
Applicant: BASF AG
Inventor: NEUMANN RAINER DR , VIETMEIER JUERGEN DR , BAUMGARTNER EHRENFRIED DR
Abstract: A thermoplastic moulding composition containing, based on components A, B and C, A: from 10 to 85 % by weight of at least one polycarbonate A, B: from 10 to 50 % by weight of a graft copolymer B comprising, in each case based on B, b1) from 20 to 80 % by weight of at least one rubber having a glass transition temperature of in which R is hydrogen or a methyl radical and X is a cyclohexyl, methylcyclohexyl, benzyl or phenyl radical, and C: from 5 to 50 % by weight of a thermoplastic polymer of a C1-C4-alkyl ester of methacrylic acid (C1-C4-alkyl methacrylate).
-
公开(公告)号:DE3834549A1
公开(公告)日:1990-04-12
申请号:DE3834549
申请日:1988-10-11
Applicant: BASF AG
Inventor: NEUMANN RAINER DR , VIETMEIER JUERGEN DR , BAUMGARTNER EHRENFRIED DR
-
公开(公告)号:DE3829828A1
公开(公告)日:1990-03-15
申请号:DE3829828
申请日:1988-09-02
Applicant: BASF AG
Inventor: NEUMANN RAINER DR , VIETMEIER JUERGEN DR , BAUMGARTNER EHRENFRIED DR
-
公开(公告)号:DE59103615D1
公开(公告)日:1995-01-12
申请号:DE59103615
申请日:1991-03-27
Applicant: BASF AG
Inventor: SEITZ FRIEDRICH DR , RUPPMICH KARL , VIETMEIER JUERGEN DR
IPC: C08L25/00 , C08L25/02 , C08L25/12 , C08L33/00 , C08L33/04 , C08L33/12 , C08L33/24 , C08L35/00 , C08L35/06 , C08L51/00 , C08L51/04 , C08L51/06
Abstract: Thermoplastic molding materials which have high gloss and are readily colored and comprise a first graft copolymer A of an elastomeric, crosslinked acrylate polymer as the graft base and a graft shell made from a vinyl-aromatic monomer and a polar, copolymerizable, ethylenically unsaturated monomer, and a second separately prepared graft copolymer B of an elastomeric crosslinked acrylate polymer as the graft base, which is different from that in A and has a larger mean particle diameter than the graft base of copolymer A, having a first graft shell of a vinyl-aromatic monomer and a second graft shell of a mixture of a vinyl aromatic monomer and a polar-copolymerizable, ethylenically unsaturated monomer, and a hard matrix C.
-
公开(公告)号:DE58905021D1
公开(公告)日:1993-09-02
申请号:DE58905021
申请日:1989-05-27
Applicant: BASF AG
Inventor: PFOEHLER PETER DR , SEYFFER HERMANN DR , VIETMEIER JUERGEN DR , TUERK JOHANNES , DRUSCHKE WOLFGANG DR , SCHAGERER KLAUS DR
IPC: C08L33/06 , C08F220/00 , C08F220/10 , C08F220/12 , C08F220/18 , C08F220/26 , C08F220/28 , C08F220/44 , C08L33/04 , C09D133/06 , C09J7/02 , C09J133/00 , C09J133/04
Abstract: Aqueous dispersions of copolymers of (a) from 70 to 85% by weight of nontertiary butyl (meth)acrylates, (b) from 8 to 27.2% by weight of (meth)acrylates (A) whose homopolymers have a glass transition temperature greater than that of the polybutyl (meth)acrylate up to 0 DEG C. and (meth)acrylates (B) whose homopolymers have a glass transition temperature below that of the polybutyl (meth)acrylate, the weight ratio of the (meth)acrylates (A) to the (meth)acrylates (B) being from 3:1 to 1:3, (c) from 2 to 15% by weight of methyl methacrylate, styrene and/or acrylonitrile and (d) 0.8 to 5% by weight of monoolefinically unsaturated mono- and/or dicarboxylic acids of 3 to 5 carbon atoms and/or their amides which are unsubstituted or substituted at the nitrogen atoms by alkyl and/or alkylol radicals of 1 to 4 carbon atoms and/or hydroxyalkyl (meth)acrylates where the alkyl groups are of 2 to 5 carbon atoms, are used for coating sheet-like substrates.
-
公开(公告)号:DE3834129A1
公开(公告)日:1990-04-19
申请号:DE3834129
申请日:1988-10-07
Applicant: BASF AG
Inventor: NEUMANN RAINER DR , VIETMEIER JUERGEN DR , BAUMGARTNER EHRENFRIED DR
Abstract: The thermoplastic moulding composition which contains, based on the sum of A, B and C, A) 10-85% by weight of at least one polycarbonate A, B) 10-50% by weight of a graft copolymer B comprising, in each case based on B, b1) from 20 to 80% by weight of at least one rubber having a glass transition temperature of below 0@C and b2) from 80 to 20% by weight of a shell grafted thereto and comprising, in each case based on b2, b21) from 70 to 95% by weight of methyl methacrylate and b22) from 5 to 30% by weight of an N-substituted (meth)acrylamide of the formula I in which R is hydrogen or a methyl radical, and X is the cyclohexyl, methylcyclohexyl, benzyl or phenyl radical, C) 5-50% by weight of a thermoplastic copolymer comprising, in each case based on C, c1) from 60 to 95% by weight of copolymerised units of methyl methacrylate c2) from 40 to 5% by weight of copolymerised units of an N-substituted (meth)acrylamide of the formula I, preparation thereof, and the use thereof for conversion into mouldings.
-
公开(公告)号:DE3827568A1
公开(公告)日:1990-02-15
申请号:DE3827568
申请日:1988-08-13
Applicant: BASF AG
Inventor: LAUSBERG DIETRICH DR , VIETMEIER JUERGEN DR , MC KEE GRAHAM EDMUND DR , BRAUN HANS-GEORG DR , HILDENBRAND PETER DR
Abstract: Thermoplastic polyester molding materials essentially contain (A) from 20 to 89% by weight of one or more aliphatic polyesters of an aromatic dicarboxylic acid, (B) from 10 to 79% by weight of one or more aromatic polycarbonates and (C) from 1 to 40% by weight of an elastomer or of a mixture of elastomers consisting of CA from 5 to 100% by weight of an elastomeric graft polymer composed of CA1 not less than 50% by weight of a grafting base having a glass transition temperature Tg of less than -20 DEG C., CA2 from 5 to 20% by weight of a first graft shell consisting of a mixture of a C1-C8-alkyl ester of acrylic acid and a vinylaromatic in a weight ratio of from 5:95 to 70:30 and CA3 from 10 to 30% by weight of a second graft shell consisting of one or more polymers having a glass transition temperature Tg above 20 DEG C. and CB from 0 to 95% by weight of an ethylene copolymer composed of CB1 from 40 to 99% by weight of ethylene and CB2 from 1 to 60% by weight of one or more comonomers containing carboxyl groups and/or carboxyl group derivatives, the sum of A to C, CA and CB, CA1 to CA3 and of CB1 and CB2 being 100% by weight in each case.
-
-
-
-
-
-
-
-
-