公开(公告)号:DE10156014A1
公开(公告)日:2003-06-05
申请号:DE10156014
申请日:2001-11-15
Applicant: BASF AG
Inventor: GUETTES BERND , HARRE KATHRIN , KNORR GOTTFRIED , SCHUSTER MARITA , WETTERLING MONIKA
Abstract: The present invention relates to a process for the production of polyether alcohols by catalytic addition of alkylene oxides to H-functional initiators using amines as catalysts, wherein the addition of the amines to the reaction mixture is effected prior to or at the commencement of the chemical addition of the alkylene oxides and also at least once during the reaction, said additional addition of the catalyst being carried out at the point of the reaction at which there is an increased occurrence of side reactions and/or when the alkylene oxides undergo a change in the polyether chain.
-
公开(公告)号:DE10029509A1
公开(公告)日:2002-01-03
申请号:DE10029509
申请日:2000-06-21
Applicant: BASF AG
Inventor: GUETTGES BERND , OPPENLAENDER KNUT , KNORR GOTTFRIED , WETTERLING MONIKA
Abstract: Polyetherpolyols (I) are prepared by base catalyzed reaction of H-functional initiator substances with alkylene oxides whereby the H-functional initiator substances are dialkanolamines and diisocyanates and optionally other co-initiators.
-
公开(公告)号:AT241660T
公开(公告)日:2003-06-15
申请号:AT99115957
申请日:1999-08-13
Applicant: BASF AG
Inventor: WETTERLING MONIKA , GUETTES BERND , HOEPPNER GERD , GROSSMANN HANS-JUERGEN
-
公开(公告)号:DE10054065A1
公开(公告)日:2002-05-16
申请号:DE10054065
申请日:2000-10-31
Applicant: BASF AG
Inventor: DINSCH STEFAN , WETTERLING MONIKA , WINKLER JUERGEN , HOEPPNER GERD
Abstract: Preparation of nitrogen-containing polyetherols by catalytically alkoxylation comprises heating a starter compound mixture containing at least one nitrogen atom with at least two reactive hydrogen atoms to 50-100 deg C followed by reaction with alkylene oxides at 90-160 deg C. Preparation of nitrogen-containing polyetherols by catalytically alkoxylation comprises heating a starter compound mixture containing at least one nitrogen atom with at least two reactive hydrogen atoms to 50-100 deg C followed by reaction at 90-160 deg C. An Independent claim is included for the obtained polyetherols.
-
公开(公告)号:DE19935487A1
公开(公告)日:2001-02-08
申请号:DE19935487
申请日:1999-07-28
Applicant: BASF AG
Inventor: BAUER STEPHAN , CHAKRABARTI SARBANANDA , WAGNER KLAUS , WETTERLING MONIKA , WINKLER JUERGEN , TISCHER GERLINDE , HARRE KATHRIN , BOEHME PETER
Abstract: Polyol mixture containing: (i) a polyester-ol obtained from an olefin-unsaturated carboxylic acid copolymer and a mono-alcohol, a 2-9C polyhydroxy compound (VII) or a more than 10C diol (II), or from diol (II), compound (VII) or a poly-carboxylic acid; or (ii) a polyether-ol from diol (II) or an alkylamine and an alkylene oxide. A polyol mixture containing: (A) 0.1-100 wt.% polyester-ol (i) or polyether-ol (ii) with 10-10000 carbon atoms, or at least two of these (not derived from castor oil or dimer fatty acid), in which (i) is obtained from (a) a copolymer (I) of an olefin (IV) with an alpha , beta -unsaturated carboxylic acid (V) and a mono-alcohol (VI) or a 2-9C polyhydroxy compound (VIII) or a diol (II) with 10 or more carbon atoms, or a mixture of two or more of these, or from (b) diol (II) and polyhydroxy compound (VII) or a carboxylic acid (VIII) with at least two COOH groups, or a mixture of two or more of these, and (ii) is obtained from (c) diol (II) and an alkylene oxide (IX) or from (d) an alkylamine (III) and alkylene oxide (IX); (B) 0-99.9 wt.% other polyester-ol(s) or polyether-ol(s); and (C) 0-10 wt.% additives. Independent claims are also included for: (1) a method for the production of polyurethanes by reacting a component containing this polyol mixture or alkylamine (III) with a polyisocyanate component; (2) polyurethanes obtained by this method; (3) polyurethanes containing a polyol mixture as described; (4) formed objects containing polyol mixtures or polyurethanes as described.
-
公开(公告)号:DE102007037643A1
公开(公告)日:2008-03-13
申请号:DE102007037643
申请日:2007-08-10
Applicant: BASF AG
Inventor: GUETTES BERND , PRADEL SILKE , WETTERLING MONIKA
IPC: C08G18/48 , C09D5/34 , C09J175/08
Abstract: A method for the production of polyurethanes (I) for glueing organic building materials, especially natural materials, by reacting (a) polyiso-cyanates with (b) compounds containing isocyanate-reactive hydrogens, in which (b) contains (b1) polyether-alcohol(s) obtained by reacting alkylene oxides with starter substances containing H-functional compounds (II) which are chemically similar to those in the organic building material. Independent claims are included for (1) polyurethanes obtained by this method for processing organic building materials (2) polyurethane adhesives, stoppers and filling compounds obtained by this method .
-
公开(公告)号:DE10357531A1
公开(公告)日:2005-07-07
申请号:DE10357531
申请日:2003-12-08
Applicant: BASF AG
Inventor: GUETTES BERND , ZIELER RALF , WETTERLING MONIKA , SCHUSTER MARITA , KNORR GOTTFRIED , OSTROWSKI THOMAS
Abstract: In the production of polyether alcohols (I) by reacting polyethylene imines (II) with alkylene oxides (III), part or all of (II) is dosed into the reaction mixture during reaction with (III).
-
公开(公告)号:DE59905721D1
公开(公告)日:2003-07-03
申请号:DE59905721
申请日:1999-08-13
Applicant: BASF AG
Inventor: WETTERLING MONIKA , GUETTES BERND , HOEPPNER GERD , GROSSMANN HANS-JUERGEN
-
公开(公告)号:DE19736976A1
公开(公告)日:1999-03-04
申请号:DE19736976
申请日:1997-08-25
Applicant: BASF AG
Inventor: WETTERLING MONIKA , SCHUSTER MARITA , GUETTES BERND , KUHN SIMONE
IPC: B60N2/70 , C08G18/40 , C08G18/48 , C08G18/65 , C08G65/26 , C08G65/28 , C08G18/66 , C08G18/63 , C08G65/32 , C08L75/04 , B60R21/04 , B68G11/04
Abstract: Production of poly:isocyanate-polyaddition flexible foams in presence of foaming agents, flame retardants etc is by catalysed reaction of polyisocyanates with poly:ether:poly:alcohols (I) obtained by: (i) reacting an alkylene oxide, optionally in presence of a catalyst, with a substance (II) containing 2 or 3 active H atoms; (ii) adding a substance (III) containing at least 4 active H atoms and optionally also a further catalyst to the reaction mixture; and (iii) reacting with an alkylene oxide.
-
公开(公告)号:DE102004041125A1
公开(公告)日:2006-03-02
申请号:DE102004041125
申请日:2004-08-24
Applicant: BASF AG
Inventor: GUETTES BERND , WETTERLING MONIKA , IHLE THOMAS , HEINZ MARION , BOEHLER FRANK
Abstract: Preparation of flame-protected polyurethane (I) (preferably polyurethane-foam materials) comprises reaction of polyisocyanate with compounds with at least two hydrogen atoms reactive with isocyanate group, where the reaction is carried out in the presence of (a) foamed melamine formaldehyde condensation products and/or (b) hydroxyl groups containing reaction products of (a) with alkylene oxide. Independent claims are also included for: (1) a hydroxyl group containing compounds (II), producible by reaction of (a) with alkylene oxide; (2) a method for the preparation of (II) comprising reaction of (a) with alkylene oxide; and (3) a flame protected polyurethane, produced by the preparation method.
-
-
-
-
-
-
-
-
-