公开(公告)号:KR20180040676A
公开(公告)日:2018-04-20
申请号:KR20187007391
申请日:2016-08-10
Applicant: BASF SE
Inventor: SCHROEDLE SIMON , RYLL THOMAS MICHAEL , VOLKOV ALEKSEI , SHIN JI YONG , LAMPERT JORDAN
CPC classification number: C01G53/50 , C01G53/006 , C01P2002/50 , C01P2002/52 , C01P2002/54 , C01P2004/32 , C01P2004/50 , C01P2004/51 , C01P2004/61 , C01P2006/11 , C01P2006/12 , C01P2006/40 , H01M4/131 , H01M4/505 , H01M4/525 , H01M10/052 , H01M10/0567 , H01M10/4235
Abstract: 본발명은일반식 (I) 에따른미립자물질의제조방법으로서, NiCoMnM(O)(OH)(I) [식중, M 은 Al 및 Ti 로부터선택되고, x 는 0.01 내지 0.9 의범위에있고, y 는 1.1 내지 1.99 의범위에있고, a 는 0.3 내지 0.85 의범위에있고, b 는 0.05 내지 0.4 의범위에있고, c 는 0.1 내지 0.5 의범위에있고, d 는 0.001 내지 0.03 의범위에있으며, 여기서 a + b + c + d = 1 임], (a) 알루미늄히드록시드또는티타늄디옥시드입자의수성슬러리를제공하는단계, (b) 니켈, 코발트및 망간의수용성염의수용액과알칼리금속히드록시드의용액을단계 (a) 에따른슬러리에첨가하여, 단계 (a) 에따른입자상에니켈및 코발트및 망간히드록시드의혼합히드록시드층을공침시키는단계, (c) 상기와같이하여수득된 (NiCoMnAl)(OH)또는 (NiCoMnTi)(OH)의입자를제거하고, 산소존재하에서상기입자를건조시키는단계를 포함하는, 미립자물질의제조방법에관한것이다.
-
公开(公告)号:WO2016083205A3
公开(公告)日:2016-07-21
申请号:PCT/EP2015076941
申请日:2015-11-18
Applicant: BASF SE
Inventor: VOLKOV ALEKSEI , SCHULZ-DOBRICK MARTIN , SCHRÖDLE SIMON , LAMPERT JORDAN
CPC classification number: H01M4/364 , C01G53/50 , C01P2004/50 , C01P2004/51 , C01P2004/61 , C01P2004/62 , C01P2006/11 , C01P2006/12 , C01P2006/14 , C01P2006/40 , H01M4/505 , H01M4/525 , H01M4/5825 , H01M4/623 , H01M4/625 , H01M10/0525 , H01M2004/028
Abstract: The present invention is directed towards a process for making a lithiated transition metal oxide, said process comprising the following steps: (a) providing a precursor selected from mixed oxides, hydroxides, oxyhydroxides, and carbonates of nickel and at least one transition metal selected from manganese and cobalt, wherein at least 45 mole-% of the cations of the precursor are Ni cations, (b) mixing said precursor with at least one lithium salt selected from LiOH, Li2O, Li2CO3, and LiNO3, thereby obtaining a mixture, (c) adding at least one phosphorus compound of general formula (I) XyH3-yPO4 (I) wherein X is selected from NH4 and Li, y is 1 or 2, to the mixture obtained in step (b), wherein steps (b) and (c) may be performed consecutively or simultaneously, treating the mixture so obtained at a temperature in the range of from 650 to 950°C.
Abstract translation: 本发明涉及一种制备锂化过渡金属氧化物的方法,所述方法包括以下步骤:(a)提供一种选自镍的混合氧化物,氢氧化物,羟基氧化物和碳酸盐的前体和至少一种选自以下的过渡金属: 锰和钴,其中前体的至少45摩尔%的阳离子是Ni阳离子,(b)将所述前体与至少一种选自LiOH,Li 2 O,Li 2 CO 3和LiNO 3的锂盐混合,从而得到混合物( c)向步骤(b)中获得的混合物中加入至少一种其中X选自NH 4和Li,y为1或2的通式(I)XyH 3-y PO 4(I)的磷化合物,其中步骤(b) 和(c)可以连续或同时进行,在650-950℃的温度范围内处理如此获得的混合物。
-
3.
公开(公告)号:HUE044387T2
公开(公告)日:2019-10-28
申请号:HUE16753325
申请日:2016-08-10
Applicant: BASF SE
Inventor: SCHROEDLE SIMON , RYLL THOMAS MICHAEL , VOLKOV ALEKSEI , SHIN JI-YONG , LAMPERT JORDAN K
IPC: C01G53/00
-
公开(公告)号:PL3652112T3
公开(公告)日:2021-11-22
申请号:PL18734601
申请日:2018-07-05
Applicant: BASF SE
Inventor: ERK CHRISTOPH , RYLL THOMAS MICHAEL , VOLKOV ALEKSEI , LONG BRANDON RAY , HAAG JACOB
IPC: C01G53/00
-
公开(公告)号:PL3337763T3
公开(公告)日:2019-12-31
申请号:PL16753325
申请日:2016-08-10
Applicant: BASF SE
Inventor: SCHROEDLE SIMON , RYLL THOMAS MICHAEL , VOLKOV ALEKSEI , SHIN JI-YONG , LAMPERT JORDAN K
IPC: C01G53/00
-
公开(公告)号:PL3161885T3
公开(公告)日:2021-11-22
申请号:PL15729856
申请日:2015-06-19
Applicant: BASF SE
Inventor: VOLKOV ALEKSEI , LAMPERT JORDAN , RYLL THOMAS MICHAEL , SHIN JI-YONG , HOELZLE MARKUS , EDER MICHAEL
IPC: H01M4/131 , C01G53/00 , H01M4/505 , H01M4/525 , H01M10/052 , H01M10/0567 , H01M10/42
-
公开(公告)号:PL3047531T3
公开(公告)日:2018-04-30
申请号:PL14771247
申请日:2014-09-16
Applicant: BASF SE
Inventor: KRKLJUS IVANA , VOLKOV ALEKSEI , SÜLING CARSTEN
-
公开(公告)号:PL3020084T3
公开(公告)日:2017-09-29
申请号:PL14734470
申请日:2014-06-30
Applicant: BASF SE
Inventor: KRKLJUS IVANA , VOLKOV ALEKSEI , SÜLING CARSTEN
-
-
-
-
-
-
-