Abstract:
The invention relates to a method for producing a supported hydrogenation catalyst having increase hydrogenation activity, comprising a hydrogenation metal and/or an oxide of a hydrogenation metal on a support material comprising Al2O3, wherein the calcined supported hydrogenation catalyst is treated with a base solution having a pH value of > 10 at a temperature in the range of 20 to 120°C for 1 to 300 hours prior to final shaping and prior to the use thereof in hydrogenation.
Abstract:
The invention relates to a method for the hydrogenation of oligo- and/or polyesters which can be obtained by the esterification of a dicarboxylic acid solution with a diol or diol mixture, the hydrogenation being carried out in the presence of a catalyst, the precursor of said catalyst containing copper oxide, aluminum oxide and at least one oxide of lanthanum, iron, tungsten, molybdenum, titanium or zirconium. The invention also relates to a method for producing 1,6-hexanediol by the catalytic hydrogenation of ester mixtures which contain oligo- and polyesters of the adipic acid and 6-hydroxycaproic acid as the main components and which can be obtained by the esterification of a dicarboxylic acid solution with diols and especially 1,6-hexanediol or diol mixtures.
Abstract:
La invención se refiere a un método para producir un catalizador de hidrogenación soportado que tiene actividad de hidrogenación incrementada, que comprende un metal de hidrogenación y/o un óxido de un metal de hidrogenación en un material de soporte que comprende Al2O3, en donde el catalizador de hidrogenación soportado calcinado se trata con una solución base que tiene un valor de pH de > 10 a una temperatura en el margen de 20 a 120°C durante 1 a 300 horas antes de la configuración final y antes del uso del mismo en hidrogenación.
Abstract:
Die Erfindung betrifft ein Verfahren zur Herstellung einer auf einem Trägermaterial geträgerten oxidischen Zusammensetzung enthaltend Vanadium, Wolfram, Phosphor und Sauerstoff, umfassend (i) Bereitstellen einer vanadiumhaltigen wässrigen Tartratlösung mit einem pH-Wert im Bereich von 5 bis 9; (ii) Zugeben einer wolframhaltigen Verbindung und einer phosphorhaltigen Verbindung zur vanadiumhaltigen wässrigen Tartratlösung gemäß (i); (iii) Imprägnieren eines Trägermaterials mit der wässrigen Tartratlösung gemäß (ii).
Abstract:
The invention relates to a method for producing a supported hydrogenation catalyst having increase hydrogenation activity, comprising a hydrogenation metal and/or an oxide of a hydrogenation metal on a support material comprising Al2O3, wherein the calcined supported hydrogenation catalyst is treated with a base solution having a pH value of > 10 at a temperature in the range of 20 to 120°C for 1 to 300 hours prior to final shaping and prior to the use thereof in hydrogenation.
Abstract:
The invention relates to a method for the hydrogenation of oligo- and/or polyesters which can be obtained by the esterification of a dicarboxylic acid solution with a diol or diol mixture, the hydrogenation being carried out in the presence of a catalyst, the precursor of said catalyst containing copper oxide, aluminum oxide and at least one oxide of lanthanum, iron, tungsten, molybdenum, titanium or zirconium. The invention also relates to a method for producing 1,6-hexanediol by the catalytic hydrogenation of ester mixtures which contain oligo- and polyesters of the adipic acid and 6-hydroxycaproic acid as the main components and which can be obtained by the esterification of a dicarboxylic acid solution with diols and especially 1,6-hexanediol or diol mixtures.
Abstract:
Oxidische Zusammensetzung, enthaltend Vanadium, Wolfram, Phosphor, Sauerstoff und gegebenenfalls Zinn, wobei in der oxidischen Zusammensetzung das molare Verhältnis von Phosphor zur Summe aus Vanadium, Wolfram und gegebenenfalls Zinn im Bereich von 1,4:1 bis 2,4:1 liegt.
Abstract:
Proceso para la hidrogenación de oligo- y/o poliésteres que pueden obtenerse mediante esterificación de una solución de ácido dicarboxílico con un diol o mezcla de dioles, en cuyo caso a la mezcla de ésteres producida se dosifica una base seleccionada del grupo constituido por alcoholato de litio, de potasio y de sodio, y en cuyo caso la hidrogenación se realiza por medio de un cuerpo moldeado de catalizador cuyo precursor puede producirse según proceso en el que (i) se proporciona un material de óxido que comprende óxido de cobre, óxido de aluminio y al menos uno de los óxidos de lantano, volframio, molibdeno, titanio, circonio o hierro, (ii) al material de óxido se adiciona cobre metálico pulverulento, hojuelas de cobre, cemento pulverulento, grafito o una mezcla de los mismos (iii) la mezcla resultante de (ii) se moldea en un cuerpo moldeado en cuyo caso el material de óxido puede obtenerse mediante precipitación simultánea o sucesiva del componente activo cobre, el componente aluminio y el componente al menos uno de los óxidos de lantano, volframio, molibdeno, titanio o circonio y secado y calcinación subsiguientes y después del moldeamiento según la etapa (iii) el cuerpo moldeado del catalizador se calcina una vez más.
Abstract:
Procedimiento para la producción de un catalizador de hidrogenación soportado con actividad de hidrogenación aumentada, que contiene metal de cobre y óxido de cobre sobre un material de soporte que contiene Al2O3, en donde el catalizador de hidrogenación soportado calcinado se trata antes o después de su conformación definitiva así como antes de su uso en la hidrogenación con una solución de una base con un valor de pH de > 10 a una temperatura en el intervalo de 20 a 120 °C durante 1 a 300 horas, y donde que se proporciona un material oxídico, que comprende óxido de cobre y óxido de aluminio y al menos uno de los óxidos del hierro, lantano, wolframio, molibdeno, titanio, zirconio, estaño o manganeso, se añaden al material oxídico cobre metálico en forma de polvo y/o laminillas de cobre y de manera opcional adicionalmente cemento en polvo, grafito o una mezcla de los mismos y la mezcla así resultante se conforma dando un cuerpo moldeado y en donde el cuerpo moldeado se activa antes del uso como catalizador mediante tratamiento con medios reductores.