公开(公告)号:AU2002367905A8
公开(公告)日:2004-01-23
申请号:AU2002367905
申请日:2002-08-12
Applicant: MICROCOATING TECHNOLOGIES INC
Inventor: MCENTYRE ERIC J , ZHAO ZHIYONG , HUNT ANDREW T , VINSON MATTHEW SCOTT
-
公开(公告)号:AU2002367905A1
公开(公告)日:2004-01-23
申请号:AU2002367905
申请日:2002-08-12
Applicant: MICROCOATING TECHNOLOGIES INC
Inventor: ZHAO ZHIYONG , HUNT ANDREW T , VINSON MATTHEW SCOTT , MCENTYRE ERIC J
-
3.
公开(公告)号:WO2004006293A3
公开(公告)日:2004-04-01
申请号:PCT/US0225350
申请日:2002-08-12
Applicant: MICROCOATING TECHNOLOGIES INC , ZHAO ZHIYONG , HUNT ANDREW T , VINSON MATTHEW SCOTT , MCENTYRE ERIC J
Inventor: ZHAO ZHIYONG , HUNT ANDREW T , VINSON MATTHEW SCOTT , MCENTYRE ERIC J
CPC classification number: C23C16/56 , C23C16/407
Abstract: The electrical conductivity of a zinc oxide layer (15) is improved by annealing (15) the layer at a temperature of between about 500°C and about 600°C in an inert atmosphere having sufficient levels of entrained ZnO to permit reduction of oxygen levels in the lattice structure of the zinc oxide layer (15) while maintaining zinc levels in the lattice structure.
Abstract translation: 氧化锌层(15)的导电性通过在具有足够含量的夹带ZnO的惰性气氛中在约500℃至约600℃之间的温度下退火(15)来改善,以允许氧水平降低 在氧化锌层(15)的晶格结构中,同时保持晶格结构中的锌含量。
-
-