METHOD FOR PRODUCING MULTILAYER FILM
    1.
    发明申请

    公开(公告)号:US20200223205A1

    公开(公告)日:2020-07-16

    申请号:US16330631

    申请日:2017-07-25

    Abstract: Embodiments provide a method for producing a multilayer film, the method including: (A) a step for continuously coextruding from a T die (3) a molten film (4) of a multilayer film in which a first acrylic resin layer (α1), an aromatic polycarbonate resin layer (β), and a second acrylic resin layer (α2) are directly laminated in the stated order using a coextrusion apparatus; (B) a step for feeding and pressing the molten film of the multilayer film between a first mirror surface body (5) that rotates or revolves and a second mirror surface body (6) that rotates or revolves so that the first acrylic resin layer (α1) is disposed on the first-mirror-surface-body side; and (C) a step for holding the pressed multilayer film against the first mirror surface body and sends the pressed multilayer film to the subsequent third mirror surface body (8) that rotates or revolves, where TR1 (surface temperature of first mirror surface body), TR2 (surface temperature of second mirror surface body), Tα1 (glass transition temperature of first acrylic resin), Tα2 (glass transition temperature of second acrylic resin), and Tβ (glass transition temperature of aromatic polycarbonate resin) satisfy a prescribed relationship.

    METHOD FOR PRODUCING MULTILAYER FILM

    公开(公告)号:US20220380560A1

    公开(公告)日:2022-12-01

    申请号:US17885880

    申请日:2022-08-11

    Abstract: Embodiments provide a multilayer film, including: a first acrylic resin layer (α1), an aromatic polycarbonate resin layer (β), and a second acrylic resin layer (α2), where the first acrylic resin layer (α1), the aromatic polycarbonate resin layer (β), and the second acrylic resin layer (α2) are directly laminated in the stated order, where a glass transition temperature of an aromatic polycarbonate resin constituting the aromatic polycarbonate resin layer (β) is 100-140° C., and where the following formulae (4-1) and (4-2) and the following properties (i) and (ii) are satisfied: (Tβ−Tα1)≤30 . . . (4-1), (Tβ−Tα2)≤30 . . . (4-2), (i) a total light transmittance of the multilayer film is 85% or more, and (ii) a retardation of the multilayer film is 75 nm or less; and where Tai is a glass transition temperature of an acrylic resin constituting the first acrylic resin layer (α1), Tae is a glass transition temperature of an acrylic resin constituting the second acrylic resin layer (α2), and Tβ is a glass transition temperature of an aromatic polycarbonate resin constituting the aromatic polycarbonate resin layer (β), and all temperature units are ° C.

    MULTILAYER FILM
    4.
    发明申请

    公开(公告)号:US20210122146A1

    公开(公告)日:2021-04-29

    申请号:US16622643

    申请日:2018-05-18

    Abstract: Embodiments provide a multilayer film in which: a first acrylic resin layer (α1), an aromatic polycarbonate resin layer (β), and a second acrylic resin layer (α2) are directly laminated in the stated order; the aromatic polycarbonate resin constituting the aromatic polycarbonate resin layer (β) is a product of ester exchange between a polycarbonic acid ester of an aromatic dihydroxy compound and a low-crystalline or amorphous aromatic polyester; and the relationships (Tβ−Tα1)≤30 and (Tβ−Tα2)≤30 (where Tal is the glass transition temperature of the acrylic resin constituting the first acrylic resin layer (α1), Tα2 is the glass transition temperature of the acrylic resin constituting the second acrylic resin layer (α2), Tβ is the glass transition temperature of the aromatic polycarbonate resin constituting the aromatic polycarbonate resin layer (β), and all of the temperatures are measured in degrees Celsius) are satisfied. The glass transition temperature of the aromatic polycarbonate resin should be 100-140° C.

    MULTILAYER HARD COATING FILM
    5.
    发明申请

    公开(公告)号:US20180072029A1

    公开(公告)日:2018-03-15

    申请号:US15559400

    申请日:2016-02-05

    Abstract: One embodiment provides a multilayer hard coating film which sequentially includes, from the superficial layer side, a first hard coating and a resin film, and wherein: the first hard coating is formed from a coating material that contains a specific amount of (A) a polyfunctional (meth)acrylate and a specific amount of (B) a water repellent agent, while containing no inorganic particles; and the resin film includes at least one layer of (α) an acrylic resin that contains 50-95% by mole of a structural unit derived from methyl methacrylate and 50-5% by mole of a structural unit derived from vinyl cyclohexane when the total of the structural units derived from polymerizable monomers is taken as 100% by mole. Another embodiment provides a multilayer hard coating film which includes a second hard coating in addition to a first hard coating, and wherein: the first hard coating contains (C) a silane coupling agent in addition to the above-described components (A) and (B); and the second hard coating is formed from a coating material that contains a specific amount of (A) a polyfunctional (meth)acrylate and a specific amount of (D) inorganic fine particles having an average particle diameter of 1-300 nm.