MOLDING OF POLYESTERRPOLYETHER BLOCK COPOLYMER

    公开(公告)号:JPS5495658A

    公开(公告)日:1979-07-28

    申请号:JP188878

    申请日:1978-01-13

    Abstract: PURPOSE:To obtain chips with little dispersion of desired shapes and dimensions, free from mutual cohesion, by making the crystallinity of a block copolymer strand a specific value while cooling and conveying the strand with grooved belts and flat belts in a cooling tank. CONSTITUTION:A molten block copolymer consisting of polytetramethylene terephthalate and poly-tetramethylene glycol components as main structural units is extruded from a die opening into a strand, which is conveyed at a speed of 20- 80 m/min while being separated respectively and cooled with a pair of grooved belts set in a cooling tank, then conveyed at a speed of 40-130 m/min while being held by a pair of flat belts and cooled in the same tank. The speed of the flat belts is 1.5-3.0 times that of the grooved belts to crystallize and draw the strands moderately, thus giving the crystallinity of 5-60%, preferably 10-40%. The cooled strand is then dehydrated and cut.

    RECOVERY OF PACKED FILTER MEDIUM
    7.
    发明专利

    公开(公告)号:JPS60106515A

    公开(公告)日:1985-06-12

    申请号:JP21250683

    申请日:1983-11-14

    Abstract: PURPOSE:To recover and regenerate used packed filter medium comprising metallic powder used in a melt-spinning process to obtain a regenerated filter medium effective like a fresh one by heating the used metallic powder, washing with a solvent, and then with alkali. CONSTITUTION:When metallic powder consisting of stainless steel and having sharp edges and many protrusions is used as a packed filter medium for spinning, a large amt. of polymer sticks to the filter medium. To regenerate and recover the filter medium, it is dismantled and heated in a heating furnace, then charged in a meshed package, dipped in a washing tank contg. triethylene glycol to dissolved and remove the polymer. The dipping is performed at, for example, 230-260 deg.C for 2-4hr. Then, it is washe for ca. 20-40min, and further dipped in aq. alkali of 15-30% concn. in an alkali washing tank to regenerate the metallic powder. Preferred temp. is ca. 100 deg.C. The product is washed finally with water to remove alkali and is dried.

Patent Agency Ranking