公开(公告)号:US11718732B2
公开(公告)日:2023-08-08
申请号:US17127149
申请日:2020-12-18
Applicant: OTSUKA CHEMICAL CO., LTD
Inventor: Kousuke Inada , Masagoro Okada , Akira Takarada
IPC: C08K7/04 , B33Y10/00 , C08K7/10 , C08K3/34 , C08L101/00 , B29C64/153 , C08K3/24 , B33Y70/10 , B29C64/118 , C08K3/22 , C08K9/06
CPC classification number: C08K7/10 , B29C64/118 , B29C64/153 , B33Y70/10 , C08K3/24 , C08K3/34 , C08K7/04 , C08L101/00 , B33Y10/00 , C08K3/22 , C08K9/06 , C08K2003/2237 , C08K2201/004
Abstract: Provided is a resin composition, a filament and resin powder for a three-dimensional printer, a shaped object, and a production method for the shaped object, all of which make it easy to produce a shaped object and can improve, in shaping using a three-dimensional printer, the resistance to delamination of the shaped object and the resistance to warpage and shrinkage of the shaped object. A resin composition contains: inorganic fibers having an average fiber length of 1 μm to 300 μm and an average aspect ratio of 3 to 200; and a thermoplastic resin and serves as a shaping material for a three-dimensional printer.
-
公开(公告)号:US20190237632A1
公开(公告)日:2019-08-01
申请号:US16378985
申请日:2019-04-09
Applicant: NICHIA CORPORATION
Inventor: Yuji AKAZAWA , Koichi OKADA
CPC classification number: H01L33/486 , C01P2004/10 , C01P2004/54 , C01P2004/61 , C01P2006/60 , C08K3/34 , C08K9/02 , C08K2201/003 , C08K2201/004 , C08K2201/016 , C09C1/28 , H01L33/56 , H01L33/60 , H01L2933/0033 , H01L2933/005
Abstract: A filling material for a resin composition includes a base material and a coating material coating at least a portion of a surface of a particle of the base material. The base material comprises a first inorganic compound containing a Group II element. The coating material comprises a second inorganic compound containing the Group II element and is different from the first inorganic compound. A method of manufacturing the filling material is provided. A resin composition comprising the filling material, a package, a light-emitting device, and methods of manufacturing them are also provided.
-
213.
公开(公告)号:US20190185596A1
公开(公告)日:2019-06-20
申请号:US16279677
申请日:2019-02-19
Inventor: Huayi LI , Qian LI , Tongbing SUN , Caizhen ZHU , Ruigang LIU , Ning ZHAO , Jian XU
IPC: C08F110/02 , B29B7/90 , B29C48/00 , B29C48/09 , B29C48/07 , B29C55/00 , B29C55/12 , D01D5/12 , D01D5/06 , D01F6/46 , C08J5/24 , C08K3/40 , C08J5/18 , C08K7/14 , C08F255/02
CPC classification number: C08F110/02 , B29B7/90 , B29C48/0018 , B29C48/022 , B29C48/07 , B29C48/09 , B29C55/005 , B29C55/12 , B29K2023/0683 , B29K2309/08 , B29L2007/002 , B29L2023/22 , C08F4/658 , C08F255/02 , C08F2500/01 , C08F2500/24 , C08F2500/26 , C08J5/18 , C08J5/24 , C08J2323/06 , C08K3/40 , C08K7/14 , C08K2201/004 , D01D5/06 , D01D5/12 , D01F6/46
Abstract: An ultra-high molecular weight, ultra-fine particle size polyethylene has a viscosity average molecular weight (Mv) greater than 1×106. The polyethylene is spherical or are sphere-like particles having a mean particle size of 10-100 μm, having a standard deviation of 2-15 μm and a bulk density of 0.1-0.3 g/mL. Using the polyethylene as a basic polyethylene, a grafted polyethylene can be obtained by means of a solid-phase grafting method; and a glass fiber-reinforced polyethylene composition comprising the polyethylene and glass fibers, and a sheet or pipe prepared therefrom; a solubilized ultra-high molecular weight, ultra-fine particle size polyethylene; and a fiber and a film prepared from the solubilized ultra-high molecular weight, ultra-fine particle size polyethylene may also be obtained. The method has simple steps, is easy to control, has a relatively low cost and a high repeatability, and can realize industrialisation.
-
214.
公开(公告)号:US20180371190A1
公开(公告)日:2018-12-27
申请号:US15776828
申请日:2016-11-11
Applicant: Nitin CHOPRA , Saad ALHUSSAIN , Ihab N. ODEH , SABIC Global Technologies B.V.
Inventor: Nitin Chopra , Saad Alhussain , Ihab N. Odeh
CPC classification number: C08J5/18 , B82Y30/00 , C08J3/201 , C08J2323/06 , C08J2323/12 , C08J2379/08 , C08J2423/06 , C08J2423/12 , C08J2479/08 , C08K3/013 , C08K7/00 , C08K7/06 , C08K7/18 , C08K2003/0806 , C08K2201/001 , C08K2201/004 , C08K2201/011 , C08L23/06 , C08L23/12 , C08L79/08 , C08L2203/16 , C08L2205/025 , C08L2205/035 , C08L2207/02 , C08L2207/062 , C08L2207/066 , C08L2314/00 , C08L67/02
Abstract: Polymeric materials, method of making the polymeric material, and uses thereof are disclosed. The polymeric material can include ordered arrangements of crystalline domains and ordered arrangements of amorphous domains.
-
公开(公告)号:US20180264884A1
公开(公告)日:2018-09-20
申请号:US15899809
申请日:2018-02-20
Applicant: SUMITOMO RUBBER INDUSTRIES, LTD.
Inventor: Daisuke SATO
CPC classification number: B60C1/0025 , B60C1/00 , B60C1/0016 , B60C5/14 , B60C9/12 , B60C11/005 , B60C13/00 , B60C2011/0025 , B60C2011/145 , B60C2013/006 , B60C2013/007 , C08B15/02 , C08J3/215 , C08J3/22 , C08J2307/02 , C08J2323/22 , C08J2401/04 , C08J2407/02 , C08J2423/22 , C08K7/04 , C08K2201/004 , C08L7/00 , C08L9/00 , C08K3/04 , C08K7/02 , C08L7/02
Abstract: The present invention provides a pneumatic tire having excellent fuel efficiency, handling stability, and ride quality while maintaining a good balance between them. Provided is a pneumatic tire including a tire component formed from a rubber composition, the rubber composition having cured rubber properties satisfying predetermined values.
-
公开(公告)号:US10059835B2
公开(公告)日:2018-08-28
申请号:US15505718
申请日:2015-08-26
Applicant: ZEON CORPORATION
Inventor: Tomonori Nakashima
IPC: C08L1/00 , C08L9/02 , C08J3/22 , C08F236/12
CPC classification number: C08L9/02 , C08F236/12 , C08F2800/20 , C08F2810/20 , C08J3/22 , C08J2309/02 , C08J2401/02 , C08K5/0025 , C08K5/17 , C08K7/02 , C08K2201/003 , C08K2201/004 , C08L1/02 , C08L15/00 , C08L2205/16 , C08L2310/00 , C08L2312/00 , C08L15/005
Abstract: A cross-linkable nitrile rubber composition including a highly saturated nitrile rubber (A) containing α,β-ethylenically unsaturated nitrile monomer units in a ratio of 5 to 50 wt % and having an iodine value of 120 or less, a polysaccharide polymer staple fiber (B) having an average fiber diameter of 1 μm or less, and a cross-linking agent (C), wherein a ratio of content of the polysaccharide polymer staple fiber (B) is 0.5 to 30 parts by weight with respect to 100 parts by weight of the highly saturated nitrile rubber (A).
-
公开(公告)号:US20180134893A1
公开(公告)日:2018-05-17
申请号:US15856237
申请日:2017-12-28
Applicant: BULLSONE MATERIAL CO., LTD.
Inventor: Jong Gil LEE , Soo Hyung HUR , Min Young PARK , Byung Rok KANG , Ji Hun KANG
IPC: C08L69/00 , B29C70/88 , H01Q17/00 , C08K9/02 , H01Q1/52 , C08K3/22 , B29K105/16 , B29K507/04 , B29L31/34 , C08K3/04 , C08K7/06
CPC classification number: C08L69/00 , B29C70/882 , B29K2105/162 , B29K2507/04 , B29L2031/3481 , C08K3/041 , C08K3/22 , C08K7/06 , C08K9/02 , C08K2201/001 , C08K2201/004 , H01Q1/526 , H01Q17/004
Abstract: The present invention relates to a preparation method for an electromagnetic wave shield composite material and the electromagnetic wave shield composite material prepared by the method. The present invention uses a highly conductive carbon fiber prepared by electroless and electrolytic continuous processes, and thus is suitable for an EMI shield due to having an excellent conductivity and low surface resistance, and is capable of providing the electromagnetic wave shield composite material having an excellent productivity and economic value. Furthermore, the electromagnetic wave shield composite material of the present invention can be used for blocking electromagnetic waves by being inserted into a cell phone cover and a cell phone pouch, and can also be applied to a bracket for protecting an LCD of a portable display product.
-
公开(公告)号:US20180079917A1
公开(公告)日:2018-03-22
申请号:US15823623
申请日:2017-11-28
Applicant: FUJIFILM CORPORATION
Inventor: Naoharu KIYOTO
IPC: C09D7/12 , C09D5/33 , C09D5/24 , C09D165/00 , C09D133/20 , G02B5/20 , G02B5/26
CPC classification number: C09D7/61 , C08G2261/3324 , C08G2261/418 , C08G2261/76 , C08K3/36 , C08K7/00 , C08K7/06 , C08K9/06 , C08K2003/0806 , C08K2003/2227 , C08K2003/2241 , C08K2003/2244 , C08K2201/001 , C08K2201/004 , C08K2201/011 , C09D5/004 , C09D5/24 , C09D7/62 , C09D7/70 , C09D133/20 , C09D165/00 , C09D201/00 , G02B5/208 , G02B5/26
Abstract: A heat insulation paint includes fibrous conductive particles and a binder that would exhibit an average transmittance of 50% or more for far infrared rays having a wavelength of 5 μm to 25 μm when the binder is formed into a coated film having a film thickness of 2 μm, and the content of the fibrous conductive particles with respect to the total solid content is from 2% by mass to 30% by mass.
-
公开(公告)号:US09908997B2
公开(公告)日:2018-03-06
申请号:US14669039
申请日:2015-03-26
Applicant: LANXESS Deutschland GmbH
Inventor: Jochen Endtner , Matthias Bienmueller , Fabio Passeri
CPC classification number: C08K13/02 , C08K3/22 , C08K5/34924 , C08K7/14 , C08K9/06 , C08K2003/2241 , C08K2201/004 , C08K2201/005 , H01H3/00 , H01H9/00 , H01H71/025 , H01H71/0257 , C08L77/02 , C08L77/06
Abstract: Flame resistant compositions based on nylon-6 (PA 6) or nylon-6,6 (PA 66) may include melamine cyanurate, titanium dioxide, glass fibers, and non-fibrous and non-foamed ground glass having a specific particle size distribution, geometry and optionally sizing. Methods for producing the composition are also provided, as well as use of the compositions for production of products for the electrical industry, preferably electrical components such as residual current circuit breakers and other circuit breakers.
-
公开(公告)号:US20170253729A1
公开(公告)日:2017-09-07
申请号:US15505718
申请日:2015-08-26
Applicant: ZEON CORPORATION
Inventor: Tomonori NAKASHIMA
IPC: C08L9/02 , C08F236/12 , C08J3/22
CPC classification number: C08L9/02 , C08F236/12 , C08F2800/20 , C08F2810/20 , C08J3/22 , C08J2309/02 , C08J2401/02 , C08K5/0025 , C08K5/17 , C08K7/02 , C08K2201/003 , C08K2201/004 , C08L1/02 , C08L15/00 , C08L2205/16 , C08L2310/00 , C08L2312/00 , C08L15/005
Abstract: A cross-linkable nitrile rubber composition including a highly saturated nitrile rubber (A) containing α,β-thylenically unsaturated nitrile monomer units in a ratio of 5 to 50 wt % and having an iodine value of 120 or less, a polysaccharide polymer staple fiber (B) having an average fiber diameter of 1 μm or less, and a cross-linking agent (C), wherein a ratio of content of the polysaccharide polymer staple fiber (B) is 0.5 to 30 parts by weight with respect to 100 parts by weight of the highly saturated nitrile rubber (A).
-
-
-
-
-
-
-
-
-