매니퓰레이터 헤드 및 이를 구비하는 매니퓰레이터
    11.
    发明公开
    매니퓰레이터 헤드 및 이를 구비하는 매니퓰레이터 有权
    操纵器头和操纵器

    公开(公告)号:KR1020120021542A

    公开(公告)日:2012-03-09

    申请号:KR1020100076027

    申请日:2010-08-06

    Inventor: 송영범

    CPC classification number: B21J13/12 B25J15/00 B25J18/00

    Abstract: PURPOSE: A manipulator head and a manipulator is provided to fix an object at forging with minimizing the damage of surface deformation or the deformation of the shape of the object, and to reduce cost by using material of high strength and thermal resistance only on the part of a head tip. CONSTITUTION: A manipulator head and a manipulator comprise a contact unit(152), a supporting arm part, and a head connecting unit(110). The contact unit comprises a contact side contacting to an object, and the other side comprises an accepting part. The supporting arm part is connected to the accepting part, and comprises a plurality of axes. The supporting arm part supports the contact part by rotating around the axes along the shape of the object surface in case of contacting the contact part for fixing the supporting arm part. The one end of the head connecting part is combined to the supporting arm part, and the other end is combined to the manipulator.

    Abstract translation: 目的:提供操纵器头和操纵器,以最小化物体表面变形或变形形状的损伤,将物体固定在一起,并且仅通过使用高强度和耐热性的材料来降低成本 的头尖。 构成:操纵器头和操纵器包括接触单元(152),支撑臂部分和头部连接单元(110)。 接触单元包括与物体接触的接触侧,另一侧包括接受部。 支撑臂部分连接到接收部分,并且包括多个轴。 在与用于固定支撑臂部分的接触部分接触的情况下,支撑臂部分沿着物体表面的形状围绕轴线旋转来支撑接触部分。 头连接部的一端与支撑臂部结合,另一端与机械手组合。

    티타늄합금의 성형방법
    12.
    发明公开
    티타늄합금의 성형방법 有权
    钛合金成型方法

    公开(公告)号:KR1020110076052A

    公开(公告)日:2011-07-06

    申请号:KR1020090132650

    申请日:2009-12-29

    CPC classification number: C22F1/183 B21D22/14 C22C14/00

    Abstract: PURPOSE: A method for forming titanium alloy is provided to improve productivity by processing a titanium alloyed plate with a high deformation rate. CONSTITUTION: A method for forming titanium alloy comprises a forming process of a titanium alloyed plate. The forming process is performed through hot shear spinning. While the hot shear spinning, the temperature of titanium alloy is more than 800°C, and the surface temperature of a mandrel(1) used for hot shear spinning is more than 300°C.

    Abstract translation: 目的:提供一种形成钛合金的方法,通过加工具有高变形率的钛合金板来提高生产率。 构成:钛合金的形成方法包括钛合金板的成形工序。 成型工艺通过热剪切纺丝进行。 当热剪切纺丝时,钛合金的温度高于800℃,用于热剪切纺丝的心轴(1)的表面温度高于300℃。

    질화 타이타늄 또는 질화 타이타늄 알루미나이드를 포함하는 합금의 제조방법

    公开(公告)号:KR101923477B1

    公开(公告)日:2018-11-29

    申请号:KR1020170031323

    申请日:2017-03-13

    Abstract: 본발명은질소기체를이용하여질화타이타늄또는질화타이타늄알루미나이드를포함하는합금을제조하는방법에관한것이다. 상술한목적을달성하기위해, 본발명은질화타이타늄을포함하는합금의제조방법을제공한다. 본발명에따른제조방법은순도 99.5% 이상의타이타늄금속의적어도일부가질화되도록, 상기타이타늄금속을질소기체와아르곤기체의혼합기체분위기하에서아크용해시키는단계, 상기아크용해된타이타늄금속을응고시키는단계및 상기응고된타이타늄금속에포함된질화물이균일하게혼합되도록, 상기응고된타이타늄금속을아르곤기체분위기하에서아크용해시키는단계를포함한다. 본발명에따른제조방법은저가의질소기체를이용하기때문에, 종래질화타이타늄의제조방법보다저렴한비용으로질화타이타늄을제조할수 있게된다.

    이종 특성을 가진 부재들을 포함하는 일체형 부품 및 그 제조 방법
    15.
    发明授权
    이종 특성을 가진 부재들을 포함하는 일체형 부품 및 그 제조 방법 有权
    包含具有不同性质的成员的整体部分及其制造方法

    公开(公告)号:KR101312317B1

    公开(公告)日:2013-09-27

    申请号:KR1020110119663

    申请日:2011-11-16

    Abstract: 본 발명은 서로 다른 조성, 형태 및 열처리 특성을 갖는 두 가지 초내열 합금을 열간 정수압 압축에 의해 접합되는 일체형 터빈 로터로 제작할 때 부품의 이중 특성(dual property)이 최적화되도록 하는 열처리 방법에 관한 것이다. 본 발명은 열간 정수압 압축에 의해 접합될 두 개의 초내열 합금 중 한 개의 초내열 합금을 먼저 별도로 열처리한 다음, 나머지 한 개의 합금에 적합한 열간 정수압 압축 처리 및 열처리 조건에 따라서 두 개의 초내열 합금을 동시에 열처리함으로써 각각의 합금특성이 최적화되는 특성을 갖는다. 본 발명에 따르면 주조용 초내열 합금과 초내열 분말 합금의 조합(Mar-M247/Rene95 및 Mar-M247/Udimet720)으로 이루어진 일체형 터빈 로터를 구성하는 각각의 합금의 미세조직이 개선되고, 고온 특성(인장 강도 및 크리프 강도)이 향상되므로 우수한 이중 특성을 갖는 일체형 터빈 부품의 제조가 가능하다.

    장갑용 다층 혼합 표면복합재료
    16.
    发明公开
    장갑용 다층 혼합 표면복합재료 有权
    混合多层非晶表面复合材料

    公开(公告)号:KR1020130074205A

    公开(公告)日:2013-07-04

    申请号:KR1020110142133

    申请日:2011-12-26

    Abstract: PURPOSE: A multilayer mixing surface composite for a glove is provided to form an alloy layer mainly including an amorphous base in an upper layer and to form a different alloy layer mainly including a crystalline substance beneath the upper layer, thereby improving protecting performance of the glove. CONSTITUTION: A multilayer mixing surface composite for a glove includes a base material (10) and a surface composite layer formed on the base material. The surface composite layer includes an upper layer formed by including an amorphous alloy and a middle layer formed between the upper layer and the base material by including at least 70 volume% of a crystalline substance. The multilayer mixing surface composite for the glove includes an interface layer formed by including the amorphous ally between the middle layer and the base material. [Reference numerals] (AA,BB,CC,DD) Movement direction

    Abstract translation: 目的:提供用于手套的多层混合表面复合材料,以形成在上层中主要包含非晶基底的合金层,并在上层下形成主要包含结晶物质的不同合金层,从而改善手套的保护性能 。 构成:用于手套的多层混合面复合体包括基材(10)和形成在基材上的表面复合层。 表面复合层包括通过包含至少70体积%的结晶物质而包括非晶合金和形成在上层和基材之间的中间层而形成的上层。 用于手套的多层混合表面复合物包括通过在中间层和基材之间包含无定形粘结而形成的界面层。 (附图标记)(AA,BB,CC,DD)移动方向

    이종 특성을 가진 부재들을 포함하는 일체형 부품 및 그 제조 방법
    17.
    发明公开
    이종 특성을 가진 부재들을 포함하는 일체형 부품 및 그 제조 방법 有权
    包含具有不同性质的成员的整体部分及其制造方法

    公开(公告)号:KR1020130053942A

    公开(公告)日:2013-05-24

    申请号:KR1020110119663

    申请日:2011-11-16

    Abstract: PURPOSE: An integrated part comprising members with different properties and a manufacturing method thereof are provided to enhance the mechanical property and the modified structure of different materials by implementing a preprocess. CONSTITUTION: A manufacturing method of an integrated part comprising members with different properties is as follows. A first member is thermally treated by a pre hot isostatic pressing process and a solution process. The thermally treated first member and alloy powder for a second member are simultaneously charged and are diffusion-bonded by hot isostatic pressing. The diffusion-bonded component is thermally post-processed.

    Abstract translation: 目的:提供包括具有不同性质的构件及其制造方法的集成部件,以通过实施预处理来增强不同材料的机械性能和改进的结构。 构成:包含具有不同性质的构件的整体部件的制造方法如下。 第一构件通过预热等静压压制和溶液工艺进行热处理。 用于第二构件的经热处理的第一构件和合金粉末同时带电,并通过热等静压进行扩散接合。 扩散粘合组分经热后处理。

    매니퓰레이터 헤드 및 이를 구비하는 매니퓰레이터
    18.
    发明授权
    매니퓰레이터 헤드 및 이를 구비하는 매니퓰레이터 有权
    操纵器头和操纵器

    公开(公告)号:KR101210290B1

    公开(公告)日:2012-12-10

    申请号:KR1020100076027

    申请日:2010-08-06

    Inventor: 송영범

    Abstract: 본발명의일 실시예에따르는매니퓰레이터헤드는, 상기매니퓰레이터에결합되는헤드연결부와, 상기헤드연결부에결합되고, 상기헤드연결부에일단이고정되어, 고정되는일단의중심을기준으로회전이가능하도록형성되는제3축과, 일단은상기제3축에결합되고, 타단은복수의고리로형성되는제2회전부를포함하는헤드베이스와, 상기헤드베이스의고리에결합되도록형성되는제2축과제2축에직각방향으로형성되는제1축을포함하는복합축및 일단은상기복합축의제1축에결합되도록형성되는복수의고리로형성되는제1회전부를구비하고, 타단은상기가공물과접촉하는접촉면을가지는접촉부를포함함으로써, 작업대상물의형상의변형이나표면의손상을최소화하면서, 단조작업시작업대상물을고정할수 있다.

    강도와 파괴인성이 우수한 W함유 이차 경화형 합금강 및 그 제조 방법
    19.
    发明授权
    강도와 파괴인성이 우수한 W함유 이차 경화형 합금강 및 그 제조 방법 有权
    含有强力和断裂韧性的铁素体超硬合金的二次硬化合金钢及其制造方法

    公开(公告)号:KR101191763B1

    公开(公告)日:2012-10-16

    申请号:KR1020100107274

    申请日:2010-10-29

    Abstract: 본 발명은 국방 및 우주항공 재료와 같은 첨단 구조 재료로 사용되는 소재에 관한 것으로, 특히 강도와 파괴인성이 우수한 고함량 Co-Ni계 합금강의 제조 방법 및 상기 제조 방법에 의해 제조된 W함유 Co-Ni계 이차 경화형 합금강에 관한 것이다.
    본 발명은 중량 %로, C: 0.23 ~ 0.28%, Cr: 2.00 ~ 3.50%, W: 0.40 ~ 4.05%, Ni: 7.50 ~ 11.05%, Co: 11.00 ~ 13.50%, 잔부 Fe 및 불가피하게 혼입되는 불순물을 함유하는 강재를 진공 유도 용해 및 일렉트로 슬래그 재용해(ESR)를 거쳐 열간 가공 공정을 통해 제조하는 단계와; 상기 강재를 1000 ~ 1200℃의 온도에서 60 ~ 120분간 유지한 후 급랭하는 단계와; 상기 급랭된 강재를 480 ~ 510℃의 온도에서 60 ~ 600분간 시효 처리하는 단계로 이루어진 강도와 파괴인성이 우수한 W함유 이차 경화형 Co-Ni계 합금강의 제조방법과, 상기 제조방법에 의해 제조된 중량 %로, C: 0.23 ~ 0.28%, Cr: 2.00 ~ 3.50%, W: 0.40 ~ 4.05%, Ni: 7.50 ~ 11.05%, Co: 11.00 ~ 13.50%, 잔부 Fe 및 불가피하게 혼입되는 불순물을 함유하는 강도와 파괴인성이 우수한 W함유 이차 경화형 Co-Ni계 합금강을 그 특징으로 한다.

    인듐을 첨가한 2090 알루미늄 합금의 다단 열처리 방법
    20.
    发明公开
    인듐을 첨가한 2090 알루미늄 합금의 다단 열처리 방법 有权
    轴承2090合金的多重加热方法

    公开(公告)号:KR1020120045624A

    公开(公告)日:2012-05-09

    申请号:KR1020100107275

    申请日:2010-10-29

    Inventor: 박태원 송영범

    CPC classification number: C22F1/057 C22C21/12

    Abstract: PURPOSE: A multi-stage heat treating method for 2090 aluminum alloy is provided to improve the elongation ratio of aluminum alloy without the deterioration of strength through two-stage and three-stage heat treatments by adding indium without cold working. CONSTITUTION: A multi-stage heat treating method for 2090 aluminum alloy is as follows. 2090 aluminum alloy comprises lithium of 1.9-2.6wt.%, copper of 2.4-3.0wt.%, zirconium of 0.08-0.15wt.%, and aluminum and inevitable impurities of the remaining amount. Indium of 0.04-0.08wt.% is added to the 2090 aluminum alloy to obtain alloy. Two- or three-stage aging and heat treatment of the alloy is implemented after solution-treating.

    Abstract translation: 目的:提供2090铝合金的多级热处理方法,通过在不进行冷加工的情况下添加铟,通过两级和三级热处理,提高铝合金的伸长率,而不会降低强度。 构成:2090铝合金的多级热处理方法如下。 2090铝合金包含1.9-2.6重量%的锂,2.4-3.0重量%的铜,0.08-0.15重量%的锆,剩余量的铝和不可避免的杂质。 将0.04-0.08重量%的铟添加到2090铝合金中以获得合金。 在溶液处理后进行两相或三阶段老化和热处理。

Patent Agency Ranking