Abstract:
PURPOSE: An electrode paste composition is provided to improve electric conductivity without increase of resistance even after increasing content of glass frit, and to increase film density of an electrode. CONSTITUTION: An electrode paste composition includes 30-80 wt% of a conductive powder, 1-30 wt% of an organic binder, 1-20 wt% of a photopolymerizable compound, 5-40 wt% of a glass frint, and 0.1-10 wt% of an initiator, and residual solvent. The glass frit includes MgO and Na2O. The amount of the MgO and Na2O are 1-10 wt%. The glass frit includes Bi2O3, B2O3, SiO2, Al2O3, MgO and Na2O. An electrode is manufactured by using the electrode paste composition.
Abstract:
PURPOSE: A backplane substrate and a plasma display panel including the same are provided to prevent gas leak by forming a double layer in which an aluminum containing layer and a silver containing layer are laminated. CONSTITUTION: A double layer is formed on a substrate(150). The double layer is formed by laminating an aluminum containing layer and a silver containing layer. The aluminum including layer is comprised of a first portion and a second portion based on the longitudinal direction of an address electrode. The silver containing layer is comprised of a third portion(3) and a fourth portion(4) based on the longitudinal direction of the address electrode. The double layer is formed by laminating the third portion and the second portion.
Abstract:
The present invention relates to a method for manufacturing an electrode for a display device which comprises the steps of: printing and drying a conductive paste on a substrate; and printing and patterning a glass paste on a dry matter of the conductive paste, an electrode for a display device manufactured thereby, and a display device comprising the same.
Abstract:
본 발명은 (a) 전도성 분말, (b) 유기바인더, (c) 유리 프릿 및 (d) 용제를 포함하는 전극 형성용 조성물에 있어서, 상기 유리 프릿(c)은 Sr2O3 및 Zr2O3 중 적어도 1종을 포함하는 것을 특징으로 한다. 본 발명은 특정 유리프릿을 도입하여 전극 보호를 위한 별도의 추가 공정없이 산 노출 공정에서의 안정성을 확보할 수 있고, Ag이온화를 방지할 수 있어 향후 패널 조립시 Ag migration 발생에 의한 수직줄 불량을 억제 시킬 수 있다.
Abstract:
PURPOSE: A composition for forming electrode and an electrode formed therefrom are provided to obtain acid-resistance while maintaining fundamental properties of electrode including resistance and line width at sintering temperature of 560-590 deg. Celsius. CONSTITUTION: A composition for forming electrode comprises conductive powder, organic binder, glass frit, and solvent. In the glass frit, 0.5-20 weight% of at least one kind of Sr2O3 and Zr2O3 is included. The glass frit comprises 15-45 weight% of Bi2O3, 25~50 weight% SiO2, 10-25 weight% of B2O3, 1-15 weight% of Al2O3, 0.5-20 weight% of one or more of Sr2O3 and Zr2O3, and 1-20 weight% of ZnO. The glass frit has 3-20:1 weight ratio of at least one of SiO2 : Sr2O3 and Zr2O3.
Abstract translation:目的:提供用于形成电极和由其形成的电极的组合物以获得耐酸性,同时保持电极的基本特性,包括在烧结温度为560-590度的电阻和线宽。 摄氏度。 构成:用于形成电极的组合物包括导电粉末,有机粘合剂,玻璃料和溶剂。 在玻璃料中,包含0.5-20重量%的至少一种Sr 2 O 3和Zr 2 O 3。 玻璃料包含15-45重量%的Bi 2 O 3,25-50重量%的SiO 2,10-25重量%的B 2 O 3,1-15重量%的Al 2 O 3,0.5〜20重量%的一种或多种Sr 2 O 3和Zr 2 O 3,以及 1-20重量%的ZnO。 玻璃料的SiO 2 :Sr 2 O 3和Zr 2 O 3中的至少一种的重量比为3-20:1。
Abstract:
전극과 유전체의 일괄 소성이 가능한 플라즈마 디스플레이 패널 전극 형성용 조성물이 개시되어 있다. 본 발명의 일 측면에 따르면, 도전성 물질, 유리 프릿, 유기 바인더, 광중합성 화합물, 광개시제 및 용매를 포함하는 전극 형성용 조성물에 있어서, 평균입경(D50)이 1~3㎛이고 광 파장 400㎚에서 10% 이상의 투과도를 가지는 유리 프릿을 포함하는 전극 형성용 조성물을 제시한다. 어드레스(ADDRESS) 전극, 플라즈마 디스플레이 패널, 유전체, 투과도
Abstract:
An apparatus for coating and curing a panel and a coated panel manufactured by the apparatus are provided to press and heat a panel coated with a coating solution to form a coating layer before the UV curing process to prevent the oxygen from being contacted with the coating layer to suppress the bad effect by oxygen during a UV curing process, thereby improving the surface strength of the panel. A film(16) is transferred along one surface or both surfaces of a panel. A storing tank(10) supplies a coating solution on the film. A coater(12) coats the film with the coating solution to the film. A pressing roll(18) presses the coated film. A heater(20) heats the panel, onto which the film is attached by the pressing roll, to disperse the coating solution of the film in a surface of the panel. A thickness controlling roll(21) controls the thickness of a coating layer, which is formed by pressing the panel passed by the heater. A UV irradiator(22) irradiates UV to the coating layer to cure the coating layer on the surface of the panel.