公开(公告)号:DE2659338A1
公开(公告)日:1978-07-13
申请号:DE2659338
申请日:1976-12-29
Applicant: BASF AG
-
公开(公告)号:DE2512503A1
公开(公告)日:1976-10-07
申请号:DE2512503
申请日:1975-03-21
Applicant: BASF AG
-
公开(公告)号:DE2419968A1
公开(公告)日:1975-12-18
申请号:DE2419968
申请日:1974-04-25
Applicant: BASF AG
Inventor: HORN PETER DIPL CHEM DR , WURMB ROLF DIPL CHEM DR , WOLFF DIETRICH DIPL CHEM DR , SEYDL WOLFGANG DIPL CHEM DR
IPC: C08L67/00 , C08G18/42 , C08G18/79 , C08K5/29 , C08K5/3442 , C08K5/36 , C08L1/00 , C08L23/00 , C08L27/00 , C08L33/00 , C08L33/02 , C08L59/00 , C08L71/00 , C08L71/12 , C08L77/00 , C08L101/00 , C08K5/43
Abstract: Thermoplastic molding compositions based on polybutylene terephthalate having a relative viscosity of from 1.3 to 2.0, as measured in a phenol/o-dichlorobenzene mixture at 25 DEG C, and which contain, to increase the thermo-aging stability and toughness and also to improve the processing stability, from 0.1 to 10% by weight, based on the polybutylene terephthalate, of isocyanates or isothiocyanates and/or carbodiimides and/or compounds forming isocyanate groups or isothiocyanate groups and/or carbodiimide groups.
-
公开(公告)号:DE2416844A1
公开(公告)日:1975-10-23
申请号:DE2416844
申请日:1974-04-06
Applicant: BASF AG
Inventor: HORN PETER DIPL CHEM DR , SEYDL WOLFGANG DIPL CHEM DR
-
公开(公告)号:DE2650924A1
公开(公告)日:1978-05-11
申请号:DE2650924
申请日:1976-11-06
Applicant: BASF AG
-
公开(公告)号:DE2647120A1
公开(公告)日:1978-04-27
申请号:DE2647120
申请日:1976-10-19
Applicant: BASF AG
-
公开(公告)号:DE2533097A1
公开(公告)日:1977-02-24
申请号:DE2533097
申请日:1975-07-24
Applicant: BASF AG
Inventor: SCHLICHTING KARL DIPL CHEM DR , HORN PETER DIPL CHEM DR , SEYDL WOLFGANG DIPL CHEM DR , HERZOG REINHARD DIPL CHEM DR
IPC: C08K5/3412 , C08L67/02 , C08K5/34
Abstract: Stabilisation is achieved against heat and oxidn. by adding aziridines (I) (where R is a 1-18C aliphatic gp. opt. substd. by Oh, CN, carbamido or carboxyalkyl. R can also be alkylene, aryl, cycloalkyl or acyl. No.n= 1-3). Stabiliser quantity may be 0.01-5 (0.1-1) wt. % wrt. polymer. Polybutylene terephthalate used has relative viscosity 1.3-2 (1.5-1.7), measured in 0.5% soln. at 25 degrees C in phenol/o-dichlorobenzene mixt. having wt. ratio 3:2. Injection-moulded articles and films resist heat-ageing.
-
公开(公告)号:DE2450673A1
公开(公告)日:1976-05-06
申请号:DE2450673
申请日:1974-10-25
Applicant: BASF AG
Inventor: JESERICH WOLFGANG-DIETER DIPL , CORDES CLAUS DIPL CHEM DR , SEYDL WOLFGANG DIPL CHEM DR , WEISS HANS-PETER DIPL CHEM DR
Abstract: Process for the continuous manufacture of polymeric starting materials for high-grade transparent thin sheeting, wherein A. epsilon -CAPROLACTAM IS CONTINUOUSLY AGITATED IN A FIRST REACTION ZONE UNDER POLYAMIDE-FORMING CONDITIONS AT TEMPERATURES OF FROM 240 DEG TO 290 DEG C until at least 20% and preferably at least 35% of the epsilon -caprolactam has reacted, B. MAGNESIUM SILICATE HAVING A PARTICLE SIZE OF LESS THAN 30 mu M IS THEN ADDED TO THE MELT TO GIVE MAGNESIUM SILICATE CONCENTRATIONS IN THE REACTION MIXTURE OF FROM 0.0005 TO 0.5% AND PREFERABLY FROM 0.001 TO 0.
-
公开(公告)号:DE2417002A1
公开(公告)日:1975-10-23
申请号:DE2417002
申请日:1974-04-08
Applicant: BASF AG
Inventor: HORN PETER DIPL CHEM DR , SEYDL WOLFGANG DIPL CHEM DR
-
公开(公告)号:DE2408531A1
公开(公告)日:1975-10-02
申请号:DE2408531
申请日:1974-02-22
Applicant: BASF AG
Abstract: Glass-fiber-reinforced molding compositions of reduced flammability consisting of (A) a linear saturated polyester resin, (B) from 10 to 60 per cent by weight of glass fibers and (C) from 3 to 30 per cent by weight of a flame retardant. The compositions contain from 2 to 20 per cent by weight, based on the total weight of the molding composition, of a particulate water-insoluble silicate having a bulk density of more than 100 g/l, which prevents dripping of the composition when in contact with an open flame.
-
-
-
-
-
-
-
-
-