POLYMER DISPERSIONS COMPRISING HIGHLY BRANCHED POLYCARBONATES

    公开(公告)号:CA2670987C

    公开(公告)日:2016-07-19

    申请号:CA2670987

    申请日:2007-12-14

    Applicant: BASF SE

    Abstract: The invention relates to aqueous polymer dispersions which comprise an emulsion polymer of at least one .alpha.,.beta.-ethylenically unsaturated monomer M and at least one highly branched polycarbonate which is a hyperbranched polycarbonate having a degree of branching of 10% to 95%. The invention also relates to a process for preparing an aqueous polymer dispersion Pd by free-radical emulsion polymerization of at least one monomer M, where at least one highly branched polycarbonate is added before and/or during and/or after the emulsion polymerization. Additionally provided by the invention are methods of modifying the performance properties of an aqueous polymer dispersion Pd, and also the use of at least one aqueous polymer dispersion Pd as a binder in coating materials and paper coating slips.

    14.
    发明专利
    未知

    公开(公告)号:BRPI0719658A2

    公开(公告)日:2014-04-29

    申请号:BRPI0719658

    申请日:2007-10-02

    Applicant: BASF SE

    Abstract: Thermoplastic molding compositions, comprising E) from 10 to 99.9% by weight of a thermoplastic polymer, F) from 0.01 to 10% by weight of a copolymer obtainable via free-radical-initiated aqueous emulsion polymerization of ethylenically unsaturated monomers in the presence of at least one dispersing agent and of at least one free-radical initiator by the feed process, where the emulsion polymerization uses from 70 to 99.5% by weight of alpha,beta-monoethylenically unsaturated compounds [monomers A], and from 0.5 to 30% by weight of compounds having at least two ethylenically unsaturated groups capable of free-radical copolymerization [monomers B], and also, if appropriate, up to 5% by weight of alpha,beta-monoethylenically unsaturated mono- or dicarboxylic acids having from 3 to 6 carbon atoms and/or their amides [monomers C], where the monomers A to C give a total of 100% by weight (entire amount of monomers) and the monomer feeds take place in such a way that >=60% by weight of the entire amount of monomers B are fed to the polymerization mixture under polymerization conditions at a juncture after >=60% by weight of the entire amount of monomer have been fed to the polymerization mixture under polymerization conditions, from 0 to 70% by weight of further additives, where the total of the percentages by weight of components A) to C) gives 100%.

    15.
    发明专利
    未知

    公开(公告)号:BRPI0720198A2

    公开(公告)日:2013-12-31

    申请号:BRPI0720198

    申请日:2007-12-11

    Applicant: BASF SE

    Abstract: Aqueous polymer dispersion having a solids content greater than 50% by weight, obtainable by emulsion polymerization of monomers in the presence of organic polymers (organic particles for short) which are dispersible in the aqueous phase without surface-active assistants.

    Proceso para la preparación de polímeros en emulsión

    公开(公告)号:ES2423897T3

    公开(公告)日:2013-09-25

    申请号:ES08852647

    申请日:2008-11-18

    Applicant: BASF SE

    Abstract: Método para proteger sustratos metálicos frente a la corrosión el cual comprende los pasos de I) producir un polímero mediante polimerización en emulsión el cual contiene como componentes de síntesis enforma copolimerizada (A) al menos un compuesto vinilaromático, (B) al menos un compuesto con dos enlaces dobles conjugados, etilénicamente insaturados, (C) al menos un compuesto etilénicamente insaturado seleccionado del grupo constituido por compuestos con almenos una función amida e hidroxialquil(met)acrilatos, (D) opcionalmente al menos otro compuesto diferente de los compuestos (A) y (C) con un enlace dobleetilénicamente insaturado, y (E) opcionalmente al menos otro compuesto diferente de los compuestos (B) con al menos dos enlaces doblesetilénicamente insaturados, en cuyo caso al menos una parte de los monómeros se dosifican a la mezcla de reacción durante la polimerizaciónpor un cierto lapso de tiempo (tiempo de dosificación) y en cuyo caso en la primera mitad del tiempo de dosificacióna la mezcla de reacción se dosifican menos de la mitad de la cantidad total del monómero (C), II) opcionalmente mezclar el polímero obtenido de esta manera con al menos un producto auxiliar seleccionado delgrupo constituido por agentes de control de flujo, espesantes, antiespumantes, materiales de carga, pigmentos,auxiliares de dispersión para pigmentos, inhibidores de corrosión y pigmentos anticorrosivos activos, III) aplicar la composición de recubrimiento sobre el sustrato metálico y IV) secar el recubrimiento a una temperatura desde temperatura ambiente hasta 100 °C durante un lapso de tiempode algunos minutos a varios días.