公开(公告)号:DE502004012115D1
公开(公告)日:2011-02-24
申请号:DE502004012115
申请日:2004-11-16
Applicant: BASF SE
Inventor: BOECKH DIETER , PFEIFFER THOMAS , BECKER STEFAN , GUZMANN MARCUS , REDDY PARMOD KAKUMANU , AIKEN JOHN DAVIS III
IPC: C08F220/00 , C08F220/28 , C11D3/00 , C11D3/37
-
公开(公告)号:AT466924T
公开(公告)日:2010-05-15
申请号:AT04734247
申请日:2004-05-21
Applicant: BASF SE
Inventor: MOCK-KNOBLAUCH CORDULA , WAGNER NORBERT , OETTER GUENTER , VOELKEL LUDWIG , PETROVIC SUSANNE , FECHTENKOETTER ANDREAS , CHRISSTOFFELS LYSANDER , KLUEGLEIN MATTHIAS , BECKER STEFAN
Abstract: A mixture comprising a surfactant and a cosurfactant is proposed wherein the cosurfactant used is an amphiphilic comb polymer having a backbone with two or more side chains attached to the backbone, where the side chains differ from one another and/or the side chains differ from the backbone in their amphiphilic character.
-
23.
公开(公告)号:MX2009005532A
公开(公告)日:2009-06-05
申请号:MX2009005532
申请日:2007-12-03
Applicant: BASF SE
Inventor: PAKUSCH JOACHIM , BECKER STEFAN , HAREMZA SYLKE , GOETZ THOMAS , AROCHA PAOLA URIBE , GULDEN ROLF
Abstract: Un método para producir ésteres de ácidos carboxílicos polimerizables radicalmente haciendo reaccionar ácidos carboxílicos etilénicamente insaturados, anhídridos de ácido carboxílico o halogenuros de ácidos carboxílicos (denominados colectivamente como componentes de ácidos carboxílicos) con un compuesto de hidroxilo que comprende grupos alcoxi de C2 a C4 de por lo menos 60 % en peso (denominado como un compuesto polialcoxi), caracterizado porque la reacción ocurre en presencia de un inhibidor de polimerización y un agente reductor.
-
公开(公告)号:AU2009331576B2
公开(公告)日:2014-11-13
申请号:AU2009331576
申请日:2009-12-21
Applicant: BASF SE
Inventor: TERRENOIRE ALEXANDRE , REINHOLD FRANK , AMTHOR STEPHAN , GROSS MICHAEL , ROSCHMANN KONRAD , BECKER STEFAN , VYAKARANAM KAMESH , HARTIG JENS
IPC: C08F2/22 , C08F220/18 , C08K3/38 , C09D133/00 , C09J133/00
Abstract: The present invention relates to polymer dispersion-based binder compositions comprising boric acid or salts of boric acid as cross-linking agents, to a method for the production thereof and to use thereof. The aqueous binder composition comprises: a) a water-insoluble polymer (P) in the form of dispersed polymer particles with a glass transition temperature in the range of -50°C to 50°C, obtained through radical polymerization of ethylenically unsaturated monomers M, wherein the monomers M contain: 80 to 99.9 wt %, relative to the total amount of monomers M, of at least one slightly soluble neutral monoethylenically unsaturated monomer M1; and 0.1 to 20 wt %, relative to the total amount of monomers M, of at least one monoethylenically unsaturated monomer M2 that contains at least one carboxyl group and/or at least one carboxylic acid amide group (CONH
-
公开(公告)号:ES2358116T3
公开(公告)日:2011-05-05
申请号:ES04797919
申请日:2004-11-16
Applicant: BASF SE
Inventor: BOECKH DIETER , PFEIFFER THOMAS , BECKER STEFAN , GUZMANN MARCUS , REDDY PARMOD KAKUMANU , AIKEN III JOHN DAVIS
IPC: C08F220/00 , C08F220/28 , C11D3/00 , C11D3/37
Abstract: Copolímeros solubles en agua que contienen copolimerizados (a) 60 a 99 % en peso de por lo menos un monómero de óxido de polialquileno monoetilénicamente insaturado de la fórmula general I en la cual las variables tienen el siguiente significado: X es -CH2- o -C(O)-, cuando Y representa -O-; es -C(O)-, cuando Y representa -NH-; es -O- o -O- (CH2)4-, cuando Y representa un enlace químico; Y es -O-, -NH- o un enlace químico; R 1 es hidrógeno o metilo; R 2 son radicales alquileno C2-C4, los cuales pueden ser iguales o diferentes así como lineales o ramificados, donde sin embargo por lo menos 50% de los radicales R 2 representan etileno; R 3 es alquilo C1-C22, fenilo, p-(alquil C1-C12)fenilo o hidrógeno; n es un número entero de 6 a 50, (b) 1 a 40 % en peso de por lo menos un monómero dipolar no cuaternizado que contiene por lo menos un átomo de nitrógeno, elegido de entre el grupo de N-vinilpirrolidonas, N-vinilimidazoles, N-vinilcaprolactamas, vinilpiridinas, N-vinilformamidas, N-vinilacetamidas, ésteres básicos del ácido acrílico con aminoalcoholes, ésteres básicos del ácido metacrilico con aminoalcoholes, N,N-di(alquil C1-C4)amino(alquil C2-C6)amidas del ácido acrílico y N,N-di (alquil C1-C4)amino(alquil C2-C6)amidas del ácido metacrilico, (c) 0 a 39 % en peso de otros monómeros no iónicos monoetilénicamente insaturados y (d) 0 a 10 % en peso de otros monómeros aniónicos monoetilénicamente insaturados y exhiben un peso molecular promedio Mw de 2 000 a 500 000 D.
-
公开(公告)号:CA2746600A1
公开(公告)日:2010-07-01
申请号:CA2746600
申请日:2009-12-21
Applicant: BASF SE
Inventor: TERRENOIRE ALEXANDRE , REINHOLD FRANK , AMTHOR STEPHAN , GROS MICHAEL , ROSCHMANN KONRAD , BECKER STEFAN , VYAKARANAM KAMESH , HARTIG JENS
IPC: C08F2/22 , C08F220/18 , C08K3/38 , C09D133/00 , C09J133/00
Abstract: The present invention relates to polymer dispersion-based binder compositions comprising boric acid or salts of boric acid as cross-linking agents, to a method for the production thereof and to use thereof. The aqueous binder composition comprises: a) a water-insoluble polymer (P) in the form of dispersed polymer particles with a glass transition temperature in the range of -50°C to 50°C, obtained through radical polymerization of ethylenically unsaturated monomers M, wherein the monomers M contain: 80 to 99.9 wt %, relative to the total amount of monomers M, of at least one slightly soluble neutral monoethylenically unsaturated monomer M1; and 0.1 to 20 wt %, relative to the total amount of monomers M, of at least one monoethylenically unsaturated monomer M2 that contains at least one carboxyl group and/or at least one carboxylic acid amide group (CONH2); and b) boric acid and/or at least one salt of boric acid.
-
公开(公告)号:DE502004011130D1
公开(公告)日:2010-06-17
申请号:DE502004011130
申请日:2004-05-21
Applicant: BASF SE
-
公开(公告)号:ES2328404T3
公开(公告)日:2009-11-12
申请号:ES06754774
申请日:2006-04-20
Applicant: BASF SE
Inventor: HARING DIETMAR , HAUER BERNHARD , BECKER STEFAN
IPC: C12P13/02
Abstract: Procedimiento para la síntesis enzimática de poli(oxialquilen)acrilamidas, según el cual se hace reaccionar una poli(oxialquilen)amina alifática, en presencia de una hidrolasas, en substancia o en un medio de la reacción líquido, que comprenda un disolvente orgánico, con un compuesto del ácido acrílico o con un éster de alquilo del mismo y se aísla(n) de la mezcla de la reacción, en caso dado, la (las) poli(oxialquilen)acrilamida(s) formada(s), una vez concluida la reacción.
-
公开(公告)号:DE502004009623D1
公开(公告)日:2009-07-30
申请号:DE502004009623
申请日:2004-07-03
Applicant: BASF SE
Inventor: HUEFFER STEPHAN , WOLF GERHARD , KLUEGLEIN MATTHIAS , BECKER STEFAN
IPC: C14C3/22 , C08F220/06
Abstract: Preparation of leather involves treating unhaired hide, pickled unhaired hide or semi-finished leather with a polymer (A) obtained by copolymerization of: one or more of 3-8C monoethylenically unsaturated mono- or dicarboxylic acids or their anhydrides; vinyl aromatic compound(s); alkoxylated unsaturated ether(s) (I); and optionally further monoethylenically unsaturated monomers. The copolymers (A) are new. Preparation of leather involves treating unhaired hide, pickled unhaired hide or semi-finished leather with a polymer (A) obtained by copolymerization of: (1) one or more of 3-8C monoethylenically unsaturated mono- or dicarboxylic acids or their anhydrides, (2) vinyl aromatic compound(s), (3) alkoxylated unsaturated ether(s) of formula (I) and optionally (4) further monoethylenically unsaturated monomers. [Image] R 1>- R 5>H or Me; R 6>H, SO 3M, PO 3M 2, CHO, (1-20C) alkylcarbonyl or (6-14C) arylcarbonyl; M : alkali metal, NH 4+>or Me; n : 3-100; y : 0-10. Independent claims are included for: (a) the polymers (A) as new; (b) the preparation of (A); and (c) aqueous dispersions containing up to 50 wt. % (A).
-
-
-
-
-
-
-
-