公开(公告)号:KR1019960007736B1
公开(公告)日:1996-06-11
申请号:KR1019930014265
申请日:1993-07-27
Applicant: 한국과학기술연구원
IPC: C10K3/00
CPC classification number: C10K1/00 , C07C51/12 , C07C51/56 , C07C67/36 , C07C53/08 , C07C53/12 , C07C69/14
Abstract: The ferric carbonyl compound in raw gas is removed by (a) converting ferric carbonyl compound to ferric halogen compound through reaction of raw gas with halogen gas such as chlorine gas or bromine gas or iodin gas; (b) passing through packed tower with inactive adsorbent such as activated carbon, clay, alumina, sillica or sillica-alumina. The raw gas purified by this method contains ferric carbonyl compound below ppb, and the contamination of catalyst by iron or the inactivation of catalyst can be prevented.
Abstract translation: 通过(a)通过原料气体与氯气或溴气或碘气等卤素气体的反应将铁羰基化合物转化为卤化铁化合物,除去原料气体中的铁羰基化合物; (b)通过填料塔与惰性吸附剂如活性炭,粘土,氧化铝,硅藻土或硅藻土氧化铝。 通过该方法纯化的原料气体含有低于ppb的羰基羰基化合物,并且可以防止催化剂被铁污染或催化剂失活。
-
-
公开(公告)号:KR101566471B1
公开(公告)日:2015-11-05
申请号:KR1020140019652
申请日:2014-02-20
Applicant: 한국과학기술연구원
CPC classification number: Y02A50/2342
Abstract: 본발명은실리콘나노선및 피리딘을사용하는이산화탄소의선택적환원방법에관한것이다. 본발명의여러구현예에따르면, 본발명의용액에칭법으로제조된실리콘나노선의표면은종래실리콘나노선보다매우거친구조를하고있고, 이렇게표면이거친실리콘나노선표면으로태양광이입사되면, 빛을흡수할수 있는부분이증가하고, 피리딘을함께사용함에따라이산화탄소환원반응에경쟁적으로일어나는수소생성과같은부반응이많이일어나는문제점을해결함과동시에이산화탄소를선택적으로환원효율이증가될수 있을뿐만아니라, 종래태양광에너지를이용하여이산화탄소를연료로전환하는기술에있어서, 높은전압이필요한문제점을해결할수 있다.
-
公开(公告)号:KR1020150098408A
公开(公告)日:2015-08-28
申请号:KR1020140019652
申请日:2014-02-20
Applicant: 한국과학기술연구원
CPC classification number: Y02A50/2342 , C25B3/04 , B01J19/08 , C01B32/50
Abstract: 본 발명은 실리콘 나노선 및 피리딘을 사용하는 이산화탄소의 선택적 환원 방법에 관한 것이다. 본 발명의 여러 구현예에 따르면, 본 발명의 용액 에칭법으로 제조된 실리콘 나노선의 표면은 종래 실리콘 나노선보다 매우 거친 구조를 하고 있고, 이렇게 표면이 거친 실리콘 나노선 표면으로 태양광이 입사되면, 빛을 흡수할 수 있는 부분이 증가하고, 피리딘을 함께 사용함에 따라 이산화탄소 환원 반응에 경쟁적으로 일어나는 수소 생성과 같은 부반응이 많이 일어나는 문제점을 해결함과 동시에 이산화탄소를 선택적으로 환원 효율이 증가될 수 있을 뿐만 아니라, 종래 태양광에너지를 이용하여 이산화탄소를 연료로 전환하는 기술에 있어서, 높은 전압이 필요한 문제점을 해결할 수 있다.
Abstract translation: 本发明涉及使用硅纳米线和吡啶选择性还原二氧化碳的方法。 根据本发明的各种实施例,通过本发明的溶液蚀刻方法制造的硅纳米线的表面比硅纳米线更加粗糙,并且当阳光到达阳光的粗糙表面时增加能够吸收光的部分的面积 硅纳米线。 通过一起使用吡啶,可以解决通常产生对二氧化碳的还原反应产生竞争性的副反应,如氢气的产生,可以提高选择性还原二氧化碳的效率。 此外,本发明可以消除对通过使用太阳能将二氧化碳转化为燃料的传统技术的高电压的需要。
-
35.
公开(公告)号:KR101270162B1
公开(公告)日:2013-05-31
申请号:KR1020110094777
申请日:2011-09-20
Applicant: 한국과학기술연구원
CPC classification number: B01J21/04 , B01J23/8926 , B01J35/1019 , B01J37/0201 , B01J37/031 , C07C5/3337 , C07C2521/04 , C07C2523/42 , C07C2523/44 , C07C2523/72 , C07C2523/89 , C07C11/08
Abstract: 본발명은특정의담지촉매를이용한직접탈수소화반응에의하여노르말-부탄으로부터부텐을제조하는방법에관한것이다. 본발명의담지촉매는알루미나담지체에백금, 팔라듐, 또는백금과팔라듐의주촉매와구리조촉매가담지되어있음으로써, 노르말-부탄을직접탈수소화하여부텐을제조하는반응에사용되어서는크래킹과이성화반응에의해생성되는부산물, 탄소침적, 촉매의비활성화를효과적으로억제하고, 노르말-부탄전환율과부텐에대한선택도를크게향상시키는효과가있다.
-
36.
公开(公告)号:KR1020110085611A
公开(公告)日:2011-07-27
申请号:KR1020100005486
申请日:2010-01-21
Applicant: 한국과학기술연구원
Inventor: 주오심 , 정광덕 , 조티프라카쉬비.야다브
CPC classification number: C23C18/08 , C23C18/1216 , C23C18/1241 , C23C18/1287 , C23C18/1291 , Y10T428/12028 , Y10T428/12875
Abstract: PURPOSE: A method of manufacturing the white gold film using the electric spray method and a white gold film manufactured thereby are provided to form the white god film on supporter without pre-processing. CONSTITUTION: The method of manufacturing the white gold film using the electric spray method includes the step of manufacturing the precursor solution for spraying by melting platinum (Pt) precursor in the ethanol. After the white gold film formation sanctions the DC voltage between the supporter holder(30) and nozzle(12) of the electric spray apparatus, the manufactured precursor solution is sprayed on the supporter maintaining by 100 - 180 °C. The formed white gold film is heat-treated.
Abstract translation: 目的:提供使用电喷雾法制造白金膜的方法和由其制造的白金膜,以在预处理的情况下在支撑体上形成白色神经膜。 构成:使用电喷雾法制造白金膜的方法包括通过熔化乙醇中的铂(Pt)前体来制造用于喷射的前体溶液的步骤。 在白金膜形成之后,对电动喷雾装置的支撑架(30)和喷嘴(12)之间的直流电压进行制动,将制成的前体溶液喷射到保持在100-180℃的支撑体上。 形成的白金膜被热处理。
-
公开(公告)号:KR100635303B1
公开(公告)日:2006-10-19
申请号:KR1020050036994
申请日:2005-05-03
Applicant: 한국과학기술연구원
Abstract: A method of preparing a crystalline Mo-Co mixture thin film with excellent catalytic activity efficiently in mild conditions is provided. A method of preparing a molybdenum-cobalt mixture thin film by electrodeposition comprises: immersing a counter electrode and a working electrode into an aqueous weak basic solution with a pH of 7 to 10 containing a cobalt salt and molybdic acid((NH4)6Mo7O24+85%MoO3) that respectively have concentrations of 10 to 200 mM; and impressing a voltage of -1.0 to -1.5 V to both electrodes at a temperature of 0 to 80 deg.C to form a Mo-Co mixture thin film on the working electrode. The aqueous weak basic solution is prepared by mixing an aqueous cobalt salt solution with an aqueous molybdic acid solution at a volume ratio of 20:1 to 1:20. The cobalt salt is selected from the group consisting of cobalt nitrate(Co(NO3)2), cobalt acetate(Co(C2H3O2)3), cobalt sulfate(CoSO4) and cobalt chloride(CoCl2). The working electrode and the counter electrode are substrates respectively selected from the group consisting of titanium(Ti), nickel(Ni), molybdenum(Mo), cadmium(Cd), platinum(Pt), gold(Au), Indium-Tin-Oxide(ITO) coated glass, stainless steel, and carbon substrate.
Abstract translation: 提供了在温和条件下有效地制备具有优异催化活性的结晶Mo-Co混合物薄膜的方法。 通过电沉积制备钼 - 钴混合物薄膜的方法包括:将对电极和工作电极浸入pH值为7至10的含有钴盐和钼酸((NH 4)6 Mo 7 O 24 +85 %MoO 3),其分别具有10至200mM的浓度; 并在0至80℃的温度下对两个电极施加-1.0至-1.5V的电压以在工作电极上形成Mo-Co混合物薄膜。 通过将钴盐水溶液与钼酸水溶液以20:1至1:20的体积比混合来制备弱碱性水溶液。 钴盐选自硝酸钴(Co(NO 3)2),乙酸钴(Co(C 2 H 3 O 2)3),硫酸钴(CoSO 4)和氯化钴(CoCl 2)。 工作电极和反电极是分别选自由钛(Ti),镍(Ni),钼(Mo),镉(Cd),铂(Pt),金(Au),铟锡合金 氧化物(ITO)镀膜玻璃,不锈钢和碳基板。
-
公开(公告)号:KR100635300B1
公开(公告)日:2006-10-19
申请号:KR1020050036995
申请日:2005-05-03
Applicant: 한국과학기술연구원
Abstract: A method of preparing a Mo-Co alloy thin film with excellent catalytic activity efficiently in mild conditions is provided. A method of preparing a molybdenum-cobalt alloy(Co2Mo3) thin film by electrodeposition comprises: immersing a counter electrode and a working electrode into an aqueous acidic solution with a pH of 3 to 6 containing a complexing agent, a cobalt salt and molybdic acid((NH4)6Mo7O24+85%MoO3) that respectively have concentrations of 10 to 200 mM; and impressing a voltage of -1.0 to -1.5 V to both electrodes at a temperature of 0 to 80 deg.C to form a Mo-Co alloy thin film on the working electrode. The complexing agent is citric acid. The aqueous acidic solution is prepared by mixing an aqueous complexing agent solution, an aqueous cobalt salt solution and an aqueous molybdic acid solution. The cobalt salt is selected from the group consisting of cobalt nitrate(Co(NO3)2), cobalt acetate(Co(C2H3O2)3), cobalt sulfate(CoSO4) and cobalt chloride(CoCl2). The working electrode and the counter electrode are substrates respectively selected from the group consisting of titanium(Ti), nickel(Ni), molybdenum(Mo), cadmium(Cd), platinum(Pt), gold(Au), Indium-Tin-Oxide(ITO) coated glass, stainless steel, and carbon substrate.
Abstract translation: 提供了在温和条件下有效地制备具有优异催化活性的Mo-Co合金薄膜的方法。 通过电沉积制备钼 - 钴合金(Co 2 Mo 3)薄膜的方法包括:将对电极和工作电极浸入含有络合剂,钴盐和钼酸的pH为3至6的酸性水溶液( (NH 4)6 Mo 7 O 24 + 85%MoO 3),其浓度分别为10至200mM; 在0〜80℃的温度下对两个电极施加-1.0〜-1.5V的电压,在工作电极上形成Mo-Co合金薄膜。 络合剂是柠檬酸。 通过混合络合剂水溶液,钴盐水溶液和钼酸水溶液来制备酸性水溶液。 钴盐选自硝酸钴(Co(NO 3)2),乙酸钴(Co(C 2 H 3 O 2)3),硫酸钴(CoSO 4)和氯化钴(CoCl 2)。 工作电极和反电极是分别选自由钛(Ti),镍(Ni),钼(Mo),镉(Cd),铂(Pt),金(Au),铟锡合金 氧化物(ITO)镀膜玻璃,不锈钢和碳基板。
-
39.
公开(公告)号:KR100599874B1
公开(公告)日:2006-07-13
申请号:KR1020030082025
申请日:2003-11-19
Applicant: 한국과학기술연구원
CPC classification number: H01G11/28 , H01G9/016 , H01G9/155 , H01G11/36 , H01G11/46 , H01G11/86 , Y02E60/13
Abstract: 본 발명은 탄소나노물질과 나노크기의 금속산화물이 조합된 전기화학 캐패시터용 전극의 제조방법에 관한 것으로서, 집전체 표면을 수소와 탄화수소의 혼합기체와 접촉시켜 집전체 위에 탄소나노물질을 화학증착시키고, 이 탄소나노물질에 나노크기의 금속산화물을 분산 담지시키는, 본 발명의 방법에 의하면, 낮은 저항 및 높은 캐패시턴스 값을 갖는 전기화학 캐패시터용 전극을 제조할 수 있다.
-
公开(公告)号:KR100576934B1
公开(公告)日:2006-05-10
申请号:KR1020040007149
申请日:2004-02-04
Applicant: 한국과학기술연구원
IPC: C01G11/00
Abstract: 본 발명은 화학적 방법을 이용한 카드뮴셀레나이드 막의 제조방법에 관한 것으로서, 황산카드뮴(CdSO
4 ) 수용액에 시트르산나트륨(Na
3 C
6 H
5 O
7 ·3H
2 O) 수용액을 첨가하여 pH를 7 내지 9로 조절한 다음, 이를 셀레노아황산나트륨(Na
2 SeSO
3 ) 수용액과 혼합한 후 여기에 증착용 기재를 침지시키는 본 발명의 화학적 방법에 의하면, 미세 육방결정구조의 카드뮴셀레나이드 막을 암모니아를 사용하지 않고 온화한 조건에서 간단하게 제조할 수 있으며, 이 막은 광에너지를 전기 또는 화학에너지로 전환하는 공정의 전극으로 유용하게 사용된다.
-
-
-
-
-
-
-
-
-