公开(公告)号:KR3004344220000S
公开(公告)日:2006-12-20
申请号:KR3020060038524
申请日:2006-09-19
Applicant: 코오롱글로텍주식회사
-
公开(公告)号:KR3004338610000S
公开(公告)日:2006-12-13
申请号:KR3020060038526
申请日:2006-09-19
Applicant: 코오롱글로텍주식회사
-
公开(公告)号:KR3004338600000S
公开(公告)日:2006-12-13
申请号:KR3020060038525
申请日:2006-09-19
Applicant: 코오롱글로텍주식회사
-
公开(公告)号:KR101795155B1
公开(公告)日:2017-11-08
申请号:KR1020150143827
申请日:2015-10-15
Applicant: 현대자동차주식회사 , 코오롱글로텍주식회사
Abstract: 본발명은소정구조의 3차원입체구조원단을자동차통풍시트표피재용원단에적용한것으로, 통기성능및 열확산작용으로인해탑승자의청량감을극대화할수 있다.
-
公开(公告)号:KR101597191B1
公开(公告)日:2016-03-08
申请号:KR1020090113374
申请日:2009-11-23
Applicant: 코오롱글로텍주식회사
IPC: D06M15/256 , D06M13/395 , D06B3/10
Abstract: 본발명은원단을불소수지계방오제(고형분 20~30중량%) 1.5~5%o.w.s, 이소시아네이트계가교제(고형분 20~30중량%) 0.3~0.5%o.w.s가함유된조성물에서 2~10초간침지하는딥핑(dipping)공정; 상기딥핑된원단을함수율 35~85%이하로탈수하는탈수공정; 상기탈수된원단을 120~140℃에서건조하는건조공정; 및상기건조된원단을 140~170℃에서처리하는열처리공정을포함하는마찰내구성이향상된방오성원단및 그의제조방법에관한것이다.
-
公开(公告)号:KR1020120059282A
公开(公告)日:2012-06-08
申请号:KR1020100120953
申请日:2010-11-30
Applicant: 코오롱글로텍주식회사
Abstract: PURPOSE: A multi-stage anti-fouling fabric with different depth is provided to save manufacturing time and cost. CONSTITUTION: A method for fabricating multi-stage anti-fouling fabric with different depth comprises: a step of performing partial anti-fouling process on a fabric(S1000); a step of partially treating the fabric with anti-fouling coating agent in 1-80 g/m^2(S2000); a step of laminating form at the lower portion of the processed fabric(S3000); and a step of embossing the laminated fabric using embo roll(S4000).
Abstract translation: 目的:提供不同深度的多级防污布,以节省制造时间和成本。 构成:制造具有不同深度的多级防污布的方法包括:对织物进行部分防污处理的步骤(S1000); 以1-80g / m 2(S2000)的防污涂料部分处理织物的步骤; 在加工织物的下部层压形成步骤(S3000); 以及使用电刷辊压花叠层织物的步骤(S4000)。
-
公开(公告)号:KR1020120040609A
公开(公告)日:2012-04-27
申请号:KR1020100102124
申请日:2010-10-19
Applicant: 현대자동차주식회사 , 코오롱글로텍주식회사
IPC: D06M13/348 , D06M13/03 , D06M13/395
CPC classification number: D06M15/277 , D06M15/263 , D06N3/042 , D06N3/047 , D06N3/183 , D06N2209/067 , D06N2209/142 , D06N2209/145 , D06N2209/147 , D06N2213/03 , Y10T442/2098 , Y10T442/2279 , Y10T442/2631
Abstract: PURPOSE: An anti-fouling method of a sheet fabric by simple and effective method is provided. CONSTITUTION: An anti-fouling method for a fabric comprises: a step of dipping a fabric into a solution containing 2-10% o.w.s of telomerized perfluorinated acrylate copolymer and 0.3-1% o.w.s of isocyanate crosslinking agent; a step of dehydrating and drying the fabric; a step of performing thermal treatment; and a step of coating acryl flame retardant on the fabric.
Abstract translation: 目的:提供一种通过简单有效的方法对片织物进行防污的方法。 构成:织物的防污染方法包括:将织物浸入含有2-10%(重量)调聚的全氟化丙烯酸酯共聚物和0.3-1%(重量)异氰酸酯交联剂的溶液中的步骤; 脱水干燥织物的步骤; 进行热处理的步骤; 以及在织物上涂布丙烯酸阻燃剂的步骤。
-
公开(公告)号:KR1020110125889A
公开(公告)日:2011-11-22
申请号:KR1020100045518
申请日:2010-05-14
Applicant: 코오롱글로텍주식회사
CPC classification number: D04H1/435 , D01D5/24 , D01D5/34 , D01F1/07 , D01F8/14 , D02G1/18 , D04H13/00 , D10B2401/061 , D10B2401/062 , D10B2503/06 , D10B2505/12
Abstract: PURPOSE: A non-woven fabric is provided to replace polyurethane foam used as a cushion material and to ensure excellent elasticity and resilience. CONSTITUTION: A non-woven fabric(20) is formed by a blend fiber comprising polyester fiber of high melting point, polyester fiber containing modified copolymer polyester with 110-200°C of melting point, and elastic conjugate fiber containing two or more kinds of polyester with different thermal shrinkage. The polyester fiber of high melting point is a hollow fiber.
Abstract translation: 目的:提供无纺布来代替用作缓冲材料的聚氨酯泡沫,并确保优异的弹性和弹性。 构成:通过包含高熔点聚酯纤维的共混纤维,含有110-200℃熔点的改性共聚物聚酯的聚酯纤维和含有两种或更多种的共聚物的弹性复合纤维形成无纺布(20) 聚酯具有不同的热收缩率。 高熔点聚酯纤维是中空纤维。
-
公开(公告)号:KR1020110056876A
公开(公告)日:2011-05-31
申请号:KR1020090113374
申请日:2009-11-23
Applicant: 코오롱글로텍주식회사
IPC: D06M15/256 , D06M13/395 , D06B3/10
Abstract: PURPOSE: A method for fabricating an antifouling fabric is provided to improve friction durability and to ensure excellent water repellency and oil repellency. CONSTITUTION: A method for fabricating an antifouling fabric with improved friction durability comprises: a step of dipping an antifouling fabric in a composition containing 1.5-5% o.w.s of fluorine resin antifouling agent(20-30 weight% of solid powder) and 0.3-0.5% o.w.s of isocyanate crosslinking agent(20-30 weight% of solid powder); a step of dehydrating the antifouling fabric; a step of drying the fabric at 120-140°C and performing thermal treatment at 140~170°C; and a step of coating with flame retardant. The antifouling fabric is flat woven, flat tricot, double raschel, tricot suede, tricot cut, circular knit, mesh, and sinker pile fabric.
Abstract translation: 目的:提供一种制造防污织物的方法,以提高摩擦耐久性并确保优异的防水性和拒油性。 构成:具有改善摩擦耐久性的防污布制造方法包括:将防污布浸渍在含有1.5-5%(重量)氟树脂防污剂(固体粉末20-30重量%)和0.3-0.5 %的异氰酸酯交联剂(固体粉末的20-30重量%); 使防污布脱水的步骤; 在120-140℃干燥织物并在140〜170℃下进行热处理的步骤; 和用阻燃剂涂布的步骤。 防污面料为平编织物,平纹经编织物,双拉氏绒毛,特里科经绒面革,经编切割,圆针织,网眼和沉降片织物。
-
公开(公告)号:KR100963573B1
公开(公告)日:2010-06-15
申请号:KR1020080062970
申请日:2008-06-30
Applicant: 코오롱글로텍주식회사
Abstract: 본 발명은 천연자개를 이용한 고주파 웰딩제품의 제조방법에 관한 것으로서, 다수개의 천연자개를 준비하는 제 1단계, 상기 천연자개의 한면 또는 양면에 필름시트를 부착하여 코팅된 자개시트를 형성하는 제 2단계, 상기 자개시트에 크랙을 형성하는 제 3단계 및 상기 자개시트를 고주파 웰딩장치로 압착하여 원단에 부착시키는 제 4단계를 포함하는 천연자개를 이용한 고주파 웰딩제품 제조방법을 제공한다.
고주파웰딩(welding), 천연자개, 필름시트(film sheet), 크랙(crack)
-
-
-
-
-
-
-
-
-