Abstract:
Catalyst components for the(co)polymerization of ethylene comprising Ti, Mg, halogen, ORI groups, where RI is a C1-C12 hydrocarbon group optionally containing heteroatoms, having ORI/Ti molar ratio in the range 0.1-1.5, a Mg/Ti molar ratio of less than 8, an amount of titanium, with respect to the total weight of said solid catalyst component, higher than 4% by weight characterized by a specific SS-NMR pattern are particularly useful for preparing narrow MWD crystalline ethylene polymers.
Abstract translation:含有Ti,Mg,卤素,ORI基团的乙烯(共)聚合的催化剂组分,其中RI是任选含有杂原子的C 1 -C 12烃基,ORI / Ti摩尔比在0.1-1.5范围内,Mg / Ti 摩尔比小于8,相对于所述固体催化剂组分的总重量,钛的量高于4重量%,其特征在于特定的SS-NMR图案,特别适用于制备窄MWD晶体乙烯聚合物。
Abstract:
Process for preparing TiO 2 powders starting from a liquid comprising chlorinated titanium compounds, the process comprising: a) atomizing said liquid and reacting the atomized liquid with a flow of steam and air at a temperature of 100-250°C for converting said chlorinated titanium compounds to titanium dioxide TiO 2 ; b) the gaseous phase and the entrained TiO 2 powders obtained from step a) are then fed to an oven operated at a temperature in the range 400-900°C to remove the residual organic compounds and hydrochloridic acid from said powders.
Abstract:
A thermoplastic polyolefm composition comprising: (1) 30-70 wt.% of an heterophasic propylene polymer; (2) 20-60 wt.% of a copolymer of ethylene with a comonomer selected from the group consisting of C 3-6 α,ß -unsaturated carboxylic acids, C 1-8 alkyl esters of a C 3-6 α,ß - unsaturated carboxylic acid and mixtures thereof; and (3) 2-20 wt.% of a metal compound selected from the group consisting of: acetates, stearates, hydroxides and oxides of zinc, magnesium, calcium, sodium and mixture thereof.
Abstract translation:一种热塑性聚烯烃组合物,其包含:(1)30-70重量%的多相丙烯聚合物; (2)20-60重量%的乙烯与共聚单体共聚物的共聚物,所述共聚单体选自C 3-6 N a,β-不饱和羧酸,C 1-8 - C 3-6不饱和羧酸的烷基酯及其混合物; 和(3)2-20重量%的选自以下的金属化合物:乙酸盐,硬脂酸盐,氢氧化物和锌,镁,钙,钠及其混合物的氧化物。
Abstract:
Pipe systems having at least one layer comprising a semi-crystalline random polymer of propylene and 0.2 to 5 wt% 1-hexen and optionally a recurring unit selected from ethylene and a C 4 -C 10 α-olefin in an amount from more than 0 to 9 % by moles. The polymer exhibits broad molecular weight distribution, in terms of the ratio of weight average molecular weight to numeric average molecular weight formula (I), ranging from 5 to 11, molecular weight distribution of monomodal type and hexen-1 content in the fraction with an intrinsic viscosity of equal to or higher than 3.3 dl/g lower than the hexen-1 content in the fraction with an intrinsic viscosity of less than 3.3 dl/g.
Abstract:
A masterbatch composition comprising (percent by weight): A) 15%-50% of a polypropylene component having a melt flow rate of from 1 to 250 g/10 min.; and B) 50%-85% of an olefin polymer partially soluble in xylene at room temperature, containing from 60% to 85% by weight of ethylene; said masterbatch composition having (i) a value of the intrinsic viscosity [rl] of the fraction soluble in xylene at room temperature ([rl] SO l) equal to or lower than 2.9 dl/g, and (ii) a value of the ratio MFR / [TI],,,, equal to or lower than 4, is added to polyolefin materials to obtain final compositions suitable for injection molding.
Abstract:
A polymer composition comprising: A) from 70 wt% to 95 wt% of a propylene ethylene copolymer having: - an ethylene derived units content measured by 13C NMR ranging from 2.2 wt% and 9.8 wt% B) from 5.0 wt% to 30.0 wt% of a copolymer of 1-butene and ethylene containing from 3.0 wt% to 4.2 wt% of ethylene derived units the sum of the amounts of A) and B) being 100 wt%.
Abstract:
A polypropylene composition comprising: A) from 71 wt% to 91 wt% of a propylene homopolymer B) from 5 wt% to 15 wt%, of a copolymer of propylene and ethylene containing from 18 wt% to 32.0 wt%, of ethylene derived units; C) from 4 wt% to 15 wt%, of a copolymer of propylene and ethylene containing from 75 wt% to 90.0 wt%, of ethylene derived units.
Abstract:
A method of depolymerizing plastic waste using a doped silica catalyst is described herein. The method provides with high efficiency a high quality liquid depolymerization product which can be used as cracker feedstock.
Abstract:
Disclosed is a filled polyolefin composition comprising a blend of a 20-50 wt.% of an heterophasic polypropylene (a), 10-25 wt.% of a propylene polymer (b) having MFR (ISO1133 230°C/2.16Kg) higher than 800 g/10 min., 5-35 wt.% of a propylene polymer (c) having MFR (ISO1133 230°C/2.16Kg) of 0.5-20 and a tensile modulus (ISO 527-1,-2) equal to or greater that 1000 MPa, 5-35 wt.% of glass fibers (d) and 0-5 wt.% of a compatibilizer (e). The filled polyolefin composition has a high fluidity in the molten state, good balance of mechanical properties and improved thermal properties. The filled composition finds use in injection molding applications.
Abstract:
The present disclosure refers to a process for the hydrodepolymerization of polymeric waste ma- terial at a hydrogen pressure from 20 to 500 bar employing a hydrocracking catalyst comprising a hydrogenating component which comprises at least one of Fe, Mo, W, Ti, Ni, Cr, V, Co, Zr and mixtures thereof supported on an inorganic carrier and comprising a depolymerizing component which is an acidic compound, and a process for the production of olefins using the product of the hydrodepolymerization process as feedstock.