티타늄 붕화물을 포함하는 알루미늄 주조재 및 그의 제조 방법
    54.
    发明公开
    티타늄 붕화물을 포함하는 알루미늄 주조재 및 그의 제조 방법 有权
    包含钛硼化物的铝铸造材料及其制造方法

    公开(公告)号:KR1020120059256A

    公开(公告)日:2012-06-08

    申请号:KR1020100120927

    申请日:2010-11-30

    CPC classification number: C22C21/02 C22C1/026 C22C1/03 C22C1/1036 C22C32/0073

    Abstract: PURPOSE: An aluminum casting material including titanium boride and a manufacturing method thereof are provided to enable the application of an aluminum casting material in general casting processes including high-pressure casting. CONSTITUTION: An aluminum casting material including titanium boride comprises aluminum of 81-93 weight%, silicon of 5-13 weight%, titanium of 1-3 weight%, and boron of 1-3 weight%. The aluminum casting material also comprises iron, copper, manganese, magnesium, nickel or zinc, 0.1-5 parts by weight. A method for manufacturing the aluminum casting material includes a step of putting an aluminum mother alloy, comprising aluminum of 80-96 weight%, titanium of 2-10 weight%, and boron of 2-10 weight%, into molten metal including aluminum and silicon.

    Abstract translation: 目的:提供包括硼化钛的铝铸造材料及其制造方法,以能够在包括高压铸造的普通铸造工艺中应用铝铸造材料。 构成:包括硼化钛的铝铸造材料包括81-93重量%的铝,5-13重量%的硅,1-3重量%的钛和1-3重量%的硼。 铝铸造材料还包含铁,铜,锰,镁,镍或锌,0.1-5重量份。 铝铸造材料的制造方法包括将包含80-96重量%的铝,2-10重量%的铝和2-10重量%的硼的铝母合金放入包括铝和 硅。

    전자후방산란회절(EBSD)을 이용한 펄라이트 콜로니 크기의 분석방법
    55.
    发明授权
    전자후방산란회절(EBSD)을 이용한 펄라이트 콜로니 크기의 분석방법 失效
    使用电子背散射衍射分析珍珠岩尺寸的方法

    公开(公告)号:KR101112027B1

    公开(公告)日:2012-02-24

    申请号:KR1020090071270

    申请日:2009-08-03

    Abstract: 본 발명은 펄라이트 콜로니의 크기를 측정하기 위해서 전자후방산란회절(EBSD) 및 입계연결 개념을 이용한 측정방법에 관한 것으로서, 전자후방산란회절(EBSD)을 이용하여 펄라이트상을 갖는 강재의 결정방위를 측정하는 단계;
    상기 측정된 결정방위를 이용하여 결정방위 사이의 방위차를 계산하여 방위차 맵(또는 패턴질 맵, pattern quality map)을 작성하는 단계;
    상기 방위차를 이용하여 콜로니 구분 기준값(θ
    st )과 입계완성 기준값(θ
    gb )을 설정하는 단계; 및
    상기 설정된 콜로니 구분 기준값 및 입계완성 기준값과 상기 방위차를 비교하여 펄라이트 콜로니 입계(boundary)를 결정하는 단계를 포함한다.
    펄라이트 콜로니(pearlite colony), 전자후방산란회절(electron back scattered diffraction), 입계연결(boundary completion)

    수소저장재료 및 그 제조 방법
    56.
    发明公开
    수소저장재료 및 그 제조 방법 有权
    氢储存材料及其制造方法

    公开(公告)号:KR1020110032928A

    公开(公告)日:2011-03-30

    申请号:KR1020090090690

    申请日:2009-09-24

    CPC classification number: Y02E60/324

    Abstract: PURPOSE: A hydrogen storage material and a producing method thereof are provided to prevent the reduction of the hydrogen storage capacity by adding a catalyst. CONSTITUTION: A hydrogen storage material contains lithium boron hydride and yttrium hydride. The yttrium hydride is selected from either yttrium dihydride or yttrium trihydride. The molar ratio of the lithium boron hydride for the yttrium hydride is 2~8. The lithium boron hydride and the yttrium hydride inter-react with each other when discharging hydrogen from the storage material, and changes into lithium hydride and yttrium boride.

    Abstract translation: 目的:提供一种储氢材料及其制备方法,以防止通过加入催化剂降低储氢能力。 构成:储氢材料含有硼氢化锂和氢化钇。 氢化钇选自二氢钇或三钇钇。 硼氢化锂对于氢化钇的摩尔比为2〜8。 当从储存材料中排出氢时,硼氢化锂和氢化钇相互相互反应,并变成氢化锂和硼化钇。

    전기 전도도 및 내산화성이 우수하고 Cr 휘발성이 낮은 연료전지 금속접속자 및 그 제조방법
    57.
    发明公开
    전기 전도도 및 내산화성이 우수하고 Cr 휘발성이 낮은 연료전지 금속접속자 및 그 제조방법 有权
    具有良好电导率,耐氧化性和低铬挥发性的燃料电池互连器及其制造方法

    公开(公告)号:KR1020110030141A

    公开(公告)日:2011-03-23

    申请号:KR1020090088133

    申请日:2009-09-17

    CPC classification number: H01M8/021 H01M8/0228 Y02P70/56

    Abstract: PURPOSE: A fuel cell interconnector and a method for manufacturing the same are provided to improve the performance of a fuel cell by forming a chromium manganese oxide-based spinel oxide layer on ferrite-based steel. CONSTITUTION: A method for manufacturing a fuel cell interconnector includes the following: Ferrite-based steel for a fuel cell interconnector is prepared. A surface deformed layer is formed on the surface of the ferrite-based steel. A Cr_2MnO_4-based spinel oxide layer is formed on the surface deformed layer by implementing a thermal treatment process at the driving temperature of a solid oxide-based fuel cell.

    Abstract translation: 目的:提供燃料电池互连器及其制造方法,通过在铁素体系钢上形成铬锰氧化物系尖晶石氧化物层来提高燃料电池的性能。 构成:燃料电池互连器的制造方法包括:制备燃料电池互连器用的铁素体系钢。 在铁素体系钢的表面上形成表面变形层。 通过在固体氧化物系燃料电池的驱动温度下实施热处理工艺,在表面变形层上形成Cr 2 MnO 4系的尖晶石氧化物层。

    텅스텐 복합 분말, 이로부터 형성된 코팅재, 및 텅스텐복합 분말의 제조 방법
    58.
    发明公开
    텅스텐 복합 분말, 이로부터 형성된 코팅재, 및 텅스텐복합 분말의 제조 방법 失效
    TUNGSTEN复合粉末,由其形成的涂层材料和制造TUNGSTEN复合粉末的方法

    公开(公告)号:KR1020080114475A

    公开(公告)日:2008-12-31

    申请号:KR1020080005374

    申请日:2008-01-17

    Abstract: Tungsten composite powder which can be used for parts of a fusion reactor facing plasma due to the excellent corrosion resistance and high temperature strength, a coating material made of the same and a method of manufacturing the tungsten composite powder are provided. A manufacturing method of tungsten composite powder comprises a step for providing a mixture in which W(tungsten) particles and SiC(silicon carbide) particles having a diameter of 0.1~30mum to be formed into W1-xSiCx composition by the weight ratio(S10), a step for providing composite powder by spraying and drying the mixture(S20), and a step for heat-treating the composite powder(S30).

    Abstract translation: 提供了可以用于由于优异的耐腐蚀性和高温强度而面对等离子体的熔融反应器的部件的钨复合粉末,由其制成的涂层材料和制造钨复合粉末的方法。 钨复合粉末的制造方法包括通过重量比(S10)提供其中W(钨)颗粒和直径为0.1〜30μm的SiC(碳化硅))颗粒形成W1-xSiCx组合物的混合物的步骤, ,通过喷雾和干燥混合物来提供复合粉末的步骤(S20)和用于热处理复合粉末的步骤(S30)。

    초미세 결정립 질화티타늄/붕화티타늄 복합 서메트제조방법
    59.
    发明授权
    초미세 결정립 질화티타늄/붕화티타늄 복합 서메트제조방법 失效
    超细晶氮化钛/硼化钛复合金属陶瓷的制造方法

    公开(公告)号:KR100714978B1

    公开(公告)日:2007-05-04

    申请号:KR1020050070841

    申请日:2005-08-03

    Abstract: 본 발명은 초미세 결정립 질화티타늄/붕화티타늄 복합 서메트 제조방법에 관한 것으로, 특히 티타늄(Ti)과 질화붕소(BN) 및 스테인레스강(stainless steel) 분말을 원료분말로 하여 반응밀링법(reaction milling)에 의해 질화티타늄(TiN)/붕화티타늄(TiB
    2 )/스테인레스강 나노 복합분말을 제조하고, 제조된 나노 복합분말을 액상소결하여 초미세 질화티타늄/붕화티타늄 서메트를 제조하는 방법에 관한 것이다.
    본 발명의 초미세 결정립 질화티타늄/붕화티타늄 복합 서메트 제조방법은 티타늄 분말과 질화붕소 분말을 3:2의 몰비로 혼합하는 제1공정;상기 혼합 분말에 스테인레스강 분말 5 ~ 60 중량 %를 추가로 혼합하는 제2공정; 상기 혼합 분말을 소정 직경의 볼과 함께 반응용기에 투입한 후 하이에너지볼밀링을 수행하여 질화티타늄/붕화티타늄/스테인레스강 나노 복합분말을 생성하는 제3공정; 및 상기 생성된 나노 복합분말을 성형 및 소결하는 제4공정;을 포함한다.
    초미세, 결정립, 질화티타늄, 붕화티타늄, 복합 서메트

    Abstract translation: 涉及一种氮化钛/硼化钛复合金属陶瓷的制造方法的本发明的超细晶粒,特别是钛(Ti)和氮化硼(BN)和由(不锈钢)的不锈钢反应研磨方法粉作为原料粉末(反应球磨 ),氮化钛(TiN)/硼化钛(TiB

    반응 밀링에 의한 Ti2AlC 분말의 제조방법
    60.
    发明授权
    반응 밀링에 의한 Ti2AlC 분말의 제조방법 失效
    通过反应研磨制备Ti2AlC粉末

    公开(公告)号:KR100531428B1

    公开(公告)日:2005-11-28

    申请号:KR1020030037402

    申请日:2003-06-11

    Inventor: 심재혁 조영환

    Abstract: 본 발명은 티타늄(Ti)과 알루미늄(Al) 및 탄소(C) 분말을 원료로 하여 반응밀링법에 의해 Ti
    2 AlC 분말을 제조하는 방법에 관한 것이다.
    본 발명에 의하면, Ti 분말과 Al 분말 및 C 분말을 각각 Ti 45 ~ 55 원자%, Al 25 ~ 35 원자%, C 15 ~ 25 원자%의 비율로 혼합하는 단계와; 상기 혼합물을 반응용기에 직경 5 ~ 30mm 볼과 함께 투입하는 단계와; 상기 반응용기에 아르곤(Ar)을 충진하는 단계와; 상기 혼합물을 하이에너지볼밀링을 하는 단계를 포함하는 반응 밀링에 의한 Ti
    2 AlC 분말의 제조방법을 제시한다.
    따라서, 본 발명은 Ti, Al 및 C 분말을 원료로 하고 이를 반응밀링하여 TiC가 포함되지 않는 단일상의 Ti
    2 AlC 분말을 상온에서 단시간 내에 제조할 수 있다.