公开(公告)号:DE3314711A1
公开(公告)日:1983-10-27
申请号:DE3314711
申请日:1983-04-22
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DIPL CHEM DR , MUENCH VOLKER DIPL CHEM DR , NAARMANN HERBERT DIPL CHEM DR , RIEBER NORBERT DIPL CHEM DR , SWOBODA JOHANN DIPL CHEM DR
IPC: C08G65/44
Abstract: The invention relates to a process for the preparation of high-molecular-weight polyphenylene ethers from monohydric phenols containing alkyl substituents, by oxidative coupling reaction with oxygen at temperatures between 10 and 50 DEG C, in the presence of a copper salt/amine catalyst complex and in the presence of an aromatic C6-to C10-hydrocarbon as solvent, where the amine component employed is a diamine of the formula R NH-R -NHR where R and R are tertiary alkyl and/or cycloalkyl groups having 4 to 12 carbon atoms, and R is an alkylene group having 2 to 4 carbon atoms in the connecting chain, in amounts of from 0.1 to 5% by weight, based on the phenol. Suitable amine components are N,N'-di-tert-alkylethylenediamines, in particular N,N'-di-tert-butylethylenediamine.
-
公开(公告)号:DE3212925A1
公开(公告)日:1983-10-13
申请号:DE3212925
申请日:1982-04-07
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DIPL CHEM DR , NAARMANN HERBERT DIPL CHEM DR , MUENCH VOLKER DIPL CHEM DR , BRANDT HERMANN DIPL ING DR , SWOBODA JOHANN DIPL CHEM DR
IPC: C08G65/44
-
公开(公告)号:DE2846754A1
公开(公告)日:1980-05-08
申请号:DE2846754
申请日:1978-10-27
Applicant: BASF AG
-
公开(公告)号:DE3219047A1
公开(公告)日:1983-11-24
申请号:DE3219047
申请日:1982-05-21
Applicant: BASF AG
Inventor: MUENCH VOLKER DIPL CHEM DR , HAMBRECHT JUERGEN DIPL CHEM DR , BOEHLKE KLAUS DIPL CHEM DR , HENNE ANDREAS DIPL CHEM DR , SWOBODA JOHANN DIPL CHEM DR , NAARMANN HERBERT DIPL CHEM DR
IPC: C08K5/5313 , C08K5/5399 , C08L71/04 , C08K5/53 , C08L25/02 , C08L25/10 , C08L51/04
-
公开(公告)号:DE3149358A1
公开(公告)日:1983-06-16
申请号:DE3149358
申请日:1981-12-12
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DIPL CHEM DR , SCHMITT BURGHARD DIPL CHEM DR , SWOBODA JOHANN DIPL CHEM DR , WASSMUTH GEORG DIPL CHEM DR , BERNHARD CLAUS DIPL CHEM DR , STEPHAN RUDOLF DIPL CHEM DR
Abstract: The invention relates to a thermoplastic molding material of an elastomeric polymer A, a shell B grafted to the polymer A, and a copolymer C as rigid matrix. The amount of polymer A is 1 to 25 percent by weight based on the weight of A+B+C. It has a glass transition temperature, Tg, of less than 0 DEG C. and an average particle size of 200 to 750 nanometers (d50 value of the integral mass distribution) and is composed of: 50 to 99.9 percent by weight of at least one alkylacrylate with 1 to 8 carbon atoms in the alkyl radical and 0.1 to 5 percent by weight of a polyfunctional monomer which has a crosslinking action. Grafting shell B represents 5 to 40 percent by weight based on A+B+C and is composed of at least one of the monomers of the group of (b1) vinylaromatic monomers, and (b2) the ethylenically unsaturated monomers. Grafting shell B is prepared in two stages with 30 to 70 percent by weight of the monomers b1 being used in the first stage, and 30 to 70 percent by weight of a mixture of monomers b1 and b2 in a weight ratio of 90:10 to 60:40 being used in the second stage. Copolymer C is added in an amount of 35 to 94 percent by weight based on A+B+C and consists of a vinylaromatic monomer and an ethylenically unsaturated monomer. The molding material may contain commonly used additives in effective amounts and is used for the preparation of molded parts.
-
公开(公告)号:DE3214425A1
公开(公告)日:1983-11-10
申请号:DE3214425
申请日:1982-04-20
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DIPL CHEM DR , NAARMANN HERBERT DIPL CHEM DR , SCHUSTER HANS H DIPL CHEM DR , ECHTE ADOLF DIPL CHEM DR , SWOBODA JOHANN DIPL CHEM DR , HEILIG JEAN-CLAUDE DIPL CHEM D
IPC: C08G65/44
Abstract: The invention relates to a process for the preparation of high-molecular-weight polyphenylene ethers from monohydric phenols having alkyl substituents, by oxidative coupling reaction with oxygen in the presence of a copper salt/amine catalyst complex and in the presence of an aromatic C6- to C10-hydrocarbon as solvent, where the amine component is a combination of a N-hydrocarbon-substituted imidazole and a diamine of the formula R HN-R -NHR and/or a secondary monoamine of the formula R NH-R and/or a primary and/or a tertiary amine, and where the substituents R and R of the diamine and of the secondary monoamine and the substituents of the primary and tertiary amine are lower alkyl and/or cycloalkyl groups having 1 to 12 carbon atoms, and the radicals R are alkylene groups having 2 to 4 carbon atoms. Particularly suitable N-hydrocarbon-substituted imidazoles are N-methyl-, N-ethyl-, N-isopropyl-, N-n-butyl-, N-cyclohexyl-, N-octyl- and N-phenylimidazole, particularly suitable diamines are N,N'-di-tert-butylethylenediamine, particularly suitable secondary monoamines are di-n-butylamine and di-n-propylamine, particularly suitable primary amines are ethylhexylamine, octylamine and decylamine, and particularly suitable tertiary amines are butyldimethylamine and n-propyldimethylamine.
-
公开(公告)号:DE3149046A1
公开(公告)日:1983-06-16
申请号:DE3149046
申请日:1981-12-11
Applicant: BASF AG
Inventor: HAMBRECHT JUERGEN DIPL CHEM DR , SCHMITT BURGHARD DIPL CHEM DR , ECHTE ADOLF DIPL CHEM DR , WASSMUTH GEORG DIPL CHEM DR , SWOBODA JOHANN DIPL CHEM DR , SCHWAAB JOSEF DIPL CHEM DR , MCKEE GRAHAM EDMUND DIPL CHEM
Abstract: The invention relates to a weathering-resistant, thermoplastic moulding composition which contains an elastomer phase comprising a core A) and an elastomeric shell B), and a graft shell C) on the core. The elastomer phase A) makes up 95 to 60% by weight, based on A + B, and is built up from 60 to 100% by weight of at least one conjugated diene. It is prepared by polymerisation in aqueous emulsion and agglomeration with the aid of an acrylate dispersion to give particles having a mean diameter in the range from 0.16 to 0.45 mu m (d50 value of the cumulative weight distribution), after which the elastomeric shell B), which makes up from 40 to 5% by weight, based on A + B, is polymerised on. This shell is built up from a mixture of from 60 to 99% by weight of at least one acrylate having 1 to 8 carbon atoms in the alcohol radical and from 0.1 to 5% by weight of a polyfunctional crosslinking monomer. The graft shell C is present in a proportion of from 20 to 90% by weight, based on from 10 to 80% by weight of the sum of the elastomer components A + B, and is built up from a mixture of from 50 to 95% by weight of at least one unsaturated aromatic hydrocarbon having up to 12 carbon atoms, and from 5 to 50% by weight of at least one copolymerisable, monoethylenically unsaturated monomer. The moulding composition may additionally contain from 10 to 150 parts by weight, based on 100 parts by weight of A + B + C, of a hard phase D. The hard phase is formed from a monomer from the group consisting of vinylaromatic monomers and ethylenically unsaturated monomers. Conventional assistants in effective amounts may furthermore be present in the moulding composition. The moulding composition is used to produce mouldings.
-
-
-
-
-
-