Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.
Abstract:
Un proceso continuo para la preparacion de oxido de propileno, que comprende (a) hacer reaccionar propeno, opcionalmente mezclado con propano, con peroxido de hidrogeno en un aparato de reaccion en presencia de acetonitrilo como disolvente, obteniendo una corriente S0 que sale del aparato de reaccion, S0 que contiene oxido de propileno, acetonitrilo, agua, al menos un componente adicional B, opcionalmente propeno y opcionalmente propano, en el que el punto de ebullicion normal de al menos un componente B es mas alto que el punto de ebullicion normal del acetonitrilo y en el que el logaritmo decadico del coeficiente de particion octanol-agua (log KOW) de al menos un componente B es mayor que cero; (b) separar el oxido de propileno de S0, opcionalmente despues de haber separado el propeno y opcionalmente el propano, obteniendo una corriente S1 que contiene acetonitrilo, agua y al menos otro componente B; (c) dividir S1 en dos corrientes S2 y S3, en el que el peso total de S3 con respecto al peso total de S1 esta en el intervalo de 0,01 a 25%; (d) someter a S3 a un fraccionamiento vapor-liquido en una primera unidad de fraccionamiento, obteniendo una corriente de fraccion de vapor S4a que se agota, en relacion con S3, en al menos uno de al menos un componente B y obtener una corriente liquida de fondos S4b, y someter al menos parte de la corriente de fraccion de vapor S4a a un fraccionamiento vapor-liquido en una segunda unidad de fraccionamiento, obteniendo una corriente de fraccion de vapor S4c y una corriente liquida de fondos S4 que se agota, en relacion con S4a, en al menos uno de al menos un componente B; (e) reciclar al menos una parte de S4, opcionalmente despues del tratamiento, a (a), y reciclar al menos una parte de S2, opcionalmente despues del tratamiento, a (a).
Abstract:
A continuous process for preparing propylene oxide proceeds by (a) reacting propene with hydrogen peroxide in a reaction apparatus in the presence acetonitrile as solvent, obtaining a stream S0 containing propylene oxide, acetonitrile, water, at least one further component B; (b) separating propylene oxide from S0, obtaining stream S1 containing acetonitrile, water and B; (c) dividing S1 into streams S2 and S3; (d) subjects S3 to vapor-liquid fractionation in a first fractionation unit, obtaining vapor fraction stream S4a being depleted, relative to S3, of at least one of B and obtaining liquid bottoms stream S4b, and subjecting at least part of vapor fraction stream S4a to vapor-liquid fractionation in a second fractionation unit, obtaining vapor fraction stream S4c and liquid bottoms stream S4 being depleted, relative to S4a, of at least one of B; (e) recycling at least a portion of S4 to (a).
Abstract:
Regeneration of a Titanium Containing Zeolite The present invention relates to a process for the regeneration of a catalyst comprising a #" titanium-containing zeolite, said catalyst having been used in a process for the preparation of an olefin oxide and having phosphate deposited thereon, said process for the regeneration comprising the steps: (a) separating the reaction mixture from the catalyst, (b) washing the catalyst obtained from (a) with liquid aqueous system; (c) optionally drying the catalyst obtained from (b) in a gas stream comprising an inert gas at a temperature of less than °C; (d) $%" calcining the catalyst obtained from (c) in a gas stream comprising oxygen at a temperature of at least 300 °C. " " &'(")*+,-./0"1+2*304"
Abstract:
Un micropolvo, cuyas partículas tienen un valor de Dv10 de al menos 2 micrómetros, comprendiendo dicho micropolvo mesoporos que tienen un diámetro medio de poro (4V/A) en el intervalo de 2 a 50 nm determinado por porosimetría de Hg según DIN 66133, y que comprende, con base en el peso del micropolvo, por lo menos 95% en peso de un material zeolítico microporoso libre de aluminio de tipo MWW de estructura que contiene titanio y zinc (ZnTiMWW), donde el valor de Dv10 representa el tamaño medio de partícula donde el 10% en volumen de las partículas del micropolvo tienen un tamaño más pequeño.
Abstract:
The present invention relates to a molding, comprising a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc (ZnTiMWW), said molding preferably comprising a micropowder comprising, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc (ZnTiMWW), the molding preferably further comprising at least one binder, preferably a silica binder.
Abstract:
The present invention relates to a process for the regeneration of a catalyst comprising a titanium-containing zeolite, said catalyst having been used in a process for the preparation of an olefin oxide and having phosphate deposited thereon, said process for the regeneration comprising the steps: (a) separating the reaction mixture from the catalyst, (b) washing the catalyst obtained from (a) with liquid aqueous system; (c) optionally drying the catalyst obtained from (b) in a gas stream comprising an inert gas at a temperature of less than 300° C.; (d) calcining the catalyst obtained from (c) in a gas stream comprising oxygen at a temperature of at least 300° C.
Abstract:
Un proceso para producir óxido de propileno que comprende (I) hacer reaccionar propeno con peróxido de hidrógeno en la presencia de un catalizador para dar una mezcla (GI) quecomprende óxido de propileno, propeno sin reaccionar y oxígeno; (II) separar óxido de propileno de la mezcla (GI) para dar una mezcla (GII) que comprende propeno y oxígeno; (III) agregar hidrógeno a la mezcla (GII) y reducir el oxígeno contenido en la mezcla (GII) al menos parcialmente porreacción con hidrógeno en presencia de un catalizador que comprende cobre en forma elemental y/o oxidada sobre unsoporte, en donde el cobre está presente sobre el soporte en una cantidad de 30 a 80% en peso, con base en elcatalizador completo calculado como CuO.