Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.
Abstract:
A process for the post-treatment of a zeolitic material having a BEA framework structure, the process comprising (i) providing a zeolitic material having a BEA framework structure, wherein the framework structure of the zeolitic material comprises X203 and Y02, wherein Y is a tetravalent element and X is a trivalent element and wherein the molar ratio X203 : Y02 is greater than 0.02 : 1; (ii) treating the zeolitic material provided in (i) with a liquid solvent system thereby obtaining a zeolitic material having a molar ratio X203 : Y02 of at most 0.02 : 1, and at least partially separating the zeolitic material from the liquid solvent system; (iii) treating the zeolitic material obtained from (ii) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75 ?C.
Abstract:
The present invention relates to a micropowder, wherein the particles of the micropowder have a Dv10 value of at least 2 micrometer and the micropowder comprises mesopores which have an average pore diameter in the range of from 2 to 50 nm and comprise, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc.
Abstract:
Un proceso para el postratamiento de un material zeolítico que tiene una estructura de armazón BEA, comprendiendo el proceso (i) proporcionar un material zeolítico que tenga una estructura de armazón BEA, en donde la estructura de armazón del material zeolítico comprende X2O3 y YO2, en donde Y es un elemento tetravalente y X es un elemento trivalente y en donde la relación molar X2O3:YO2 es mayor que 0.02:1, en donde Y se selecciona del grupo que consiste en Si, Sn, Ti, Zr, Ge, y combinaciones de dos o más de los mismos en donde X se selecciona del grupo que consiste en Al, B, In, Ga, Fe y combinaciones de dos o más de los mismos; (ii) tratar el material zeolítico provisto en (i) con un sistema de solvente líquido obteniendo así un material zeolítico que tiene una relación molar X2O3:YO2 de como máximo 0.02:1, y separando al menos parcialmente el material zeolítico del sistema de solvente líquido, en donde el sistema de solvente líquido se selecciona del grupo que consiste en agua, alcoholes monohídricos, alcoholes polihídricos y mezclas de dos o más de los mismos, en donde en (ii), el tratamiento se lleva a cabo a una temperatura en el intervalo de 50 a 125ºC; (iii) tratar el material zeolítico obtenido de (ii) con un sistema acuoso líquido con un pH en el rango de 5.5 a 8 y una temperatura de al menos 75°C, en donde el contenido de agua del sistema acuoso líquido es mayor que 50% en peso, en donde en (iii), el material zeolítico se trata con el sistema acuoso líquido durante un período en el intervalo de 0.5 a 24 h; en donde el pH del sistema acuoso usado en (iii) se determina usando un electrodo de vidrio sensible al pH.
Abstract:
La presente invención se refiere a un micropolvo en donde las partículas del micropolvo tienen un valor Dv10 de al menos 2 micrómetros y el micropolvo contiene mesoporos los cuales tienen un diámetro de poro promedio en el intervalo desde 2 hasta 50 nm y contiene, con base en el peso del micropolvo, al menos 95% en peso de un material microporoso zeolítico libre de aluminio del tipo de estructura MWW con un contenido de titanio y zinc.
Abstract:
Un micropolvo, cuyas partículas tienen un valor de Dv10 de al menos 2 micrómetros, comprendiendo dicho micropolvo mesoporos que tienen un diámetro medio de poro (4V/A) en el intervalo de 2 a 50 nm determinado por porosimetría de Hg según DIN 66133, y que comprende, con base en el peso del micropolvo, por lo menos 95% en peso de un material zeolítico microporoso libre de aluminio de tipo MWW de estructura que contiene titanio y zinc (ZnTiMWW), donde el valor de Dv10 representa el tamaño medio de partícula donde el 10% en volumen de las partículas del micropolvo tienen un tamaño más pequeño.
Abstract:
The present invention relates to a molding, comprising a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc (ZnTiMWW), said molding preferably comprising a micropowder comprising, based on the weight of the micropowder, at least 95 weight-% of a microporous aluminum-free zeolitic material of structure type MWW containing titanium and zinc (ZnTiMWW), the molding preferably further comprising at least one binder, preferably a silica binder.
Abstract:
Un proceso para el postratamiento de un material zeolítico que tiene una estructura marco BEA que comprende (i) proporcionar un material zeolítico que tiene una estructura marco BEA, en donde la estructura marco del material zeolítico comprende X2O3 e YO2, en donde Y es un elemento tetravalente y X es un elemento trivalente y en donde la relación molar X2O3: YO2 es mayor que 0,02: 1; (ii) tratar el material zeolítico proporcionado en (i) con un sistema solvente líquido obteniendo así un material zeolítico con una relación molar X2O3 : YO2 de a lo sumo 0,02 1 y al menos separar parcialmente el material zeolítico del sistema solvente líquido; (iii) tratar el material zeolítico obtenido de (ii) con un sistema acuoso líquido que tiene un pH en el rango de 5,5 a 8 y una temperatura de al menos 75 °C.
Abstract:
A process for the post-treatment of a zeolitic material having a BEA framework structure, the process comprising (i) providing a zeolitic material having a BEA framework structure, wherein the framework structure of the zeolitic material comprises X2O3 and YO2, wherein Y is a tetravalent element and X is a trivalent element and wherein the molar ratio X2O3:YO2 is greater than 0.02:1; (ii) treating the zeolitic material provided in (i) with a liquid solvent system thereby obtaining a zeolitic material having a molar ratio X2O3:YO2 of at most 0.02:1, and at least partially separating the zeolitic material from the liquid solvent system; (iii) treating the zeolitic material obtained from (ii) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75° C.
Abstract:
processo para o pós-tratamento de um material zeolítico, material zeolítico e uso do mesmo processo para o pós-processamento de um material zeolítico possuindo uma estrutura em framework beta, o processo compreendendo (i) provisão de um material zeolítico possuindo uma estrutura em framework beta, em que a estrutura em framework do material zeolítico compreende x2o3 e yo2, em que y é um elemento tetravalente e x é um elemento trivalente e em que a proporção molar x2o3 : yo2 é maior que 0,02 : 1; (ii) tratamento do material zeolítico provido em (i) com um sistema de solvente líquido, deste modo obtendo um material zeolítico possuindo uma proporção molar x2o3 : yo2 de no máximo 0,02 : 1, e pelo menos separação parcial do material zeolítico do sistema de solvente líquido; (iii) tratamento do material zeolítico obtido em (ii) com um sistema líquido aquoso possuindo um ph em torno de 5,5 a 8 e uma temperatura de pelo menos 75 °c.