Abstract:
The present invention provides a cermet coating that can take advantage of the hardness of a powder for a hard reinforcement phase more effectively, and spraying particles for forming the cermet coating. The cermet coating is formed on a base surface and has a hard reinforcement phase and a binder phase. The cermet coating has a Vickers hardness of from 50% to less than 100% of the hardness of the powder for a hard reinforcement phase, and has a surface roughness (center-line average roughness Ra) of less than 3.0. The cermet coating is formed by heating spraying particles prepared as aggregates of a powder for a hard reinforcement phase and a powder for a binder phase, and applying the spraying particles to a base at a supersonic velocity to integrate the powder for a hard reinforcement phase with the powder for a binder phase.