PHOTO-MAGNETIC RECORDING MEDIUM
    2.
    发明专利

    公开(公告)号:JPS60119649A

    公开(公告)日:1985-06-27

    申请号:JP22815783

    申请日:1983-12-02

    Applicant: SONY CORP

    Abstract: PURPOSE:To improve the S/N by forming a soft magnetic thin film made of an amorphous material mainly made of Co onto a magnetic recording layer formed on the base. CONSTITUTION:A magnetic recording layer, i.e., a vertical magnetizing film 12 is formed on a base 11 and the soft magnetic thin film 13 made of the amorphous material mainly made of Co formed by the vapor deposition or sputter is formed. A material having a large Kerr rotating angle thetaK is preferred for the film 13 and a low magnetostriction amorphous alloy including lots of cobalt atoms is preferred. The recording of information is recorded to hatched parts and the magnetization 16 is inverted. A magnetized pattern 17 is produced to the film 13 by the magnetic distribution of the magnetic recording layer 12, the magnetized pattern 17 is produced to the film 13 and the information of the layer 12 is transferred to the film 13. The information is read by forming the laser light to linear polarized light 5, irradiating the light to the film 13, utilizing the magnetic Kerr effect where the polarized plane is rotated by the reflection on the film 13 and detecting its reflecting light 5'.

    AMORPHOUS MAGNETIC ALLOY
    3.
    发明专利

    公开(公告)号:JPS60116742A

    公开(公告)日:1985-06-24

    申请号:JP22586583

    申请日:1983-11-30

    Applicant: SONY CORP

    Abstract: PURPOSE:To obtain a specially suitable amorphous magnetic alloy as a core material of a magnetic head used as a magnetic recording and reproducing for a magnetic recording medium having high coercive force such as a metallic tape, by dispersing and mixing a fine granule of metal carbide selected among TaC, WC, NbC, MoC, VC and Cr3C2. CONSTITUTION:An amorphous magnetic alloy is composed by dispersing and mixing fine granules of a metal carbide selected among TaC, WC, NbC, MoC, VC and Cr3C2 into a base alloy in the ratio of 0.1-10vol%. An average grain size of the fine granule of said metal carbide is in a range of, for example, 0.1- 10.0mu preferably 0.5-1.0mu. In order to prevent the metal carbide from dissolving in the base alloy, the metal element of fine granules of said carbides is desirably dissolved as a component of the base alloy into said base alloy. Namely, when a composition of the base alloy for dispersing, for example, the fine TaC granule is supposed to be an Fe-Co-Ta-B series and said TaC granule is mixed into the base alloy, the TaC granule is hardly dissolved in the base alloy and its magnetic characteristic is deviated not so much from an expected value.

    AMORPHOUS ALLOY MAGNETIC HEAD AND ITS PRODUCTION

    公开(公告)号:JPS567219A

    公开(公告)日:1981-01-24

    申请号:JP8095479

    申请日:1979-06-27

    Applicant: SONY CORP

    Abstract: PURPOSE:To obtain a high-permeability and high-magnetic flux density magnetic head, by polishing the surface of an amorphous alloy having a comparatively small positive magnetic distortion constant and by etching it. CONSTITUTION:An amorphous alloy having a comparatively small positive magnetic distortion constant such as the Co-system amorphous alloy is adjusted. Next, the surface of the obtained amorphous alloy is subjected to processings such as unidirectional polishing dependent upon the tape coated with an abrasive paper, minute- diameter alumina, and so on, thereby making an axis difficult to magnetize and an axis easy to magnetize in the polishing direction and the orthogonal direction respectively. Next, the processed surface is eliminated by etching by approximately 1.5mum or more to eliminate the processing distortion layer on the surface.

    MANUFACTURE OF HIGHHPERMEABILITY AMORPHOUS ALLOY CORE

    公开(公告)号:JPS5580303A

    公开(公告)日:1980-06-17

    申请号:JP15524178

    申请日:1978-12-13

    Applicant: SONY CORP

    Abstract: PURPOSE:To obtain a soft magnetic core suitable for magnetic heads, by preparing a thin core material by the use of an amorphous alloy of FeCo.SiB wherein the composition is specified and the magnetic Curie temperature is lower than crystallizing temperature, forming the material into a core shape, holding the core at a specified temperature, and then rapidly cooling it. CONSTITUTION:A thin core material is prepared by using an amorphous alloy which is expressed by (Fe1-xCox)100-z(Si1-yBy)z, where x=0.90-0.98, y=0.30- 0.80, and z=22-30, and a Curie temperature Tc is lower than a crystallizing temperature Tcry. Then, the material is machined into a core shape. After the core is held at a temperature T which is 0.95XTc( deg.K)

    AMORPHOUS MAGNETIC ALLOY
    6.
    发明专利

    公开(公告)号:JPS5443118A

    公开(公告)日:1979-04-05

    申请号:JP10974677

    申请日:1977-09-12

    Applicant: SONY CORP

    Abstract: PURPOSE:To provide an amorphous magnetic alloy suitable for use as a magnetic head material obtd. by adding a limited amt. of Ru and one or more kinds of amorphism forming elements selected from P, C, Si, B and Ge to iron. CONSTITUTION:The amorphous magnetic alloy consists of Ru; 2-20at%, one or more kinds of amorhism forming elements selected from P, C, Si, B and Ge; 10- 30%, and the balance almost iron. The addn. of Ru decreases the magnetostriction constant and this compsn improves the working resistance and toughness, thereby reducing a fluctuation in effective permeability before and after resin molding. This alloy can be rolled to stably manufacture tough straight foil.

    HEAT PROCESSING METHOD FOR AMORPHOUS MAGNETIC MATERIAL

    公开(公告)号:JPS58107607A

    公开(公告)日:1983-06-27

    申请号:JP20634781

    申请日:1981-12-21

    Applicant: SONY CORP

    Abstract: PURPOSE:To attain high maganetic permeability through the condition which is the same as that when there is no inductive magnetic anisotropy by executing heat processing under the magnetic field so that the inductive magnetic anisotropy Ki which crosses orthogonally and equal to that at the time of manufacturing. CONSTITUTION:A sample is produced using magnetic distortion-free amorphous Fe5Co75Si4B16 (atomic ratio). In view of eliminating distortion generated during manufacturing process and non-homogeneous anisotropy, the field is applied in the direction (x) for the heat processing under the field. Thereby the inductive magnetic anisotropy in the direction (x) can be obtained. This sample is placed under the heat processing in the orthogonal field by applying the field to the direction (y) orthogonally crossing the direction (x). Thereby, the inductive field anisotropies Kx and Ky in the directions (x) and (y) become equal. Now, it seems that the inductive magnetic anisotropy does not physically exist within amorphous magnetic material and high magnetic permeability can be attained.

    HEAT TREATMENT OF THIN STRIP OF AMORPHOUS MAGNETIC ALLOY FOR MAGNETOSTRICTIVE DELAY WIRE

    公开(公告)号:JPS57140824A

    公开(公告)日:1982-08-31

    申请号:JP2505381

    申请日:1981-02-23

    Applicant: SONY CORP

    Abstract: PURPOSE:To produce a magnetostrictive delay wire having uniform characteristics by heat-treating a thin strip consisting of an amorphous magnetic alloy at temps. lower than the crystallization temp. of the amorphous magnetic alloy while holding the same in the state in which tension is acted upon the same. CONSTITUTION:An amorphous alloy ribbon 1 is taken up from a supply reel 2 via a kiln 4 on a take-up reel 3. At this time, tension to the extent of permitting holding of the ribbon 1 substantially linearly is acted upon said ribbon, wherein the tension of about is sufficient. The treating temp. in the kiln 4 is required to be maintained at the temp. lower than the crystallization temp. because the amorphous alloy 1 does not crystallize. The heat treating time is determined by the correlation with treating temps. The cooling may be natural air cooling, but in general it is accomplished at about 25 deg.C/sec. The magnetostrictive constant of the magnetostrictive material is preferably negative.

    MANUFACTURE OF HIGH PERMEABILITY AMORPHOUS ALLOY

    公开(公告)号:JPS55161057A

    公开(公告)日:1980-12-15

    申请号:JP6955879

    申请日:1979-06-04

    Applicant: SONY CORP

    Abstract: PURPOSE:To increase the permeability of a Co-Fe type amorphous alloy over a wide frequency band zone by rapidly cooling the alloy whose magnetic Curie temp. is lower than the crystallization temp. from a specified temp. followed by reheating treatment in a nonmagnetic field. CONSTITUTION:A soft magnetic core for a magnetic head such as a video head requiring superior permeability at very high frequency is made of Co-Fe type amorphous alloy contg. Co>=60 atomic% and Fe 15-25 atomic%. Ni may be substituted for part of the Co, and Si or B>=22 atomic% is added as an element for making the alloy amorphous. The magnetic Curie temp. To of this alloy is made lower than the crystallization temp. Tcry. This alloy is heated to T deg.K satisfying 0.95XTc( deg.K)