公开(公告)号:JP2001020138A
公开(公告)日:2001-01-23
申请号:JP19386299
申请日:1999-07-08
Applicant: TORAY INDUSTRIES
Inventor: SHIMIZU YUZO , MATSUMURA YOSHITAKA , KONNO YOSHIHIRO
Abstract: PROBLEM TO BE SOLVED: To obtain a basic dye-dyeable copolyester fiber which has a high strength, a stretching property, and excellent dyeability with basic dyes and disperse dyes and is suitable for sport wears, by processing a specific polyester into the fiber having a prescribed Young's modulus and a prescribed elongation elastic recovery. SOLUTION: This basic dye-dyeable polyester fiber comprises a polyester which contains propylene terephthalate units as main components and a polyoxyalkylene glycol having a mol.wt. of >=192 preferably in an amount of 0.01 to 20 wt.% and has been copolymerized with a basic dye-dyeable site component such as a sulfoisophthalic acid alkali metal salt (preferably in an amount of 0.01 to 10 mol.% based on the total acid components), has a Young's modulus of
-
公开(公告)号:JP2000212836A
公开(公告)日:2000-08-02
申请号:JP1304099
申请日:1999-01-21
Applicant: TORAY INDUSTRIES
Inventor: KONNO YOSHIHIRO , AONO SHOJI
Abstract: PROBLEM TO BE SOLVED: To obtain an antistatic polyester fiber having a sufficient antistatic performance and capable of being developed to all colored uses including white color uses by forming a conjugate fiber which comprises a polyester component containing an antistatic agent and a matting agent and a polyester component substantially not containing an antistatic agent and containing a matting agent. SOLUTION: This antistatic polyester fiber comprises a conjugate fiber comprising one component and another component. The one component comprises a polyester containing >=1.0 wt.% of an antistatic agent and >=1.0 wt.% of a matting agent such as titanium dioxide. Another component comprises a polyester substantially not containing an antistatic agent and containing
-
公开(公告)号:JP2000192325A
公开(公告)日:2000-07-11
申请号:JP28228099
申请日:1999-10-04
Applicant: TORAY INDUSTRIES
Inventor: HIRAI SATOSHI , FUKUHARA MOTOTADA , KONNO YOSHIHIRO
Abstract: PROBLEM TO BE SOLVED: To obtain a highly modified cross-section yarn having excellent deep- colorable properties, water absorption, covering properties, lightweight and heat retaining properties and dry touch. SOLUTION: This highly modified cross-section yarn comprises a thermoplastic polymer, is an approximately δ type cross-section yarn consisting of a hollow base part having one hollow part and a branch part extended from the hollow base part. Two recessed parts composed of the hollow base part and the branch part exist. One recessed part forms a bay part which a line segment obtained by drawing a line from the center of the hollow base part to the tip of the branch part crosses. The yarn thickness T of the branch part is substantially constant. In the yarn, preferably the thermoplastic polymer is a polyethylene terephthalate. Preferably the ratio Dp/T of the depth(Dp) of the bay part to the thickness of the branch part T is >=0.5.
-
公开(公告)号:JP2000160430A
公开(公告)日:2000-06-13
申请号:JP33270698
申请日:1998-11-24
Applicant: TORAY INDUSTRIES
Inventor: TAKEHARA KATSUMI , SUGIMURA SHOICHI , KONNO YOSHIHIRO
Abstract: PROBLEM TO BE SOLVED: To provide heat-bonding fibers used for cushion materials having high temperature setting resistance and good amenity is uses often exposed to high temperature, such as vehicles, and to provide the cushion material. SOLUTION: The heat-bonding fibers are produced from only a polymer having a glass transition temperature and a melting point which simultaneously satisfy the inequalities, 75 deg.C =70% at 70 deg.C.
-
公开(公告)号:JPH11152646A
公开(公告)日:1999-06-08
申请号:JP31353597
申请日:1997-11-14
Applicant: TORAY INDUSTRIES
Inventor: FUJIMOTO MASUMI , MIYAMOTO JINROKU , KONNO YOSHIHIRO
IPC: D03D27/00
Abstract: PROBLEM TO BE SOLVED: To obtain a pile cloth excellent in soft feeling, resistance to hair falling-down, covering property, mottled feeling and print coloring property by using a pile yarn constituted of polyester fibers having a specific S-letter like cross section and different contents of delustering agent. SOLUTION: This pile cloth is manufactured by using a pile yarn of pile part-constituting fibers comprising 20-80 wt.% of polyester fibers having S-letter like cross section having an aspect ratio of in the cross section Within the range of 0.5-3.5 and 1.5-6 de single fiber size containing >=1.5 wt.% of delustering agent such as titanium oxide and 80-20 wt.% of fibers containing
-
公开(公告)号:JPH10204722A
公开(公告)日:1998-08-04
申请号:JP502697
申请日:1997-01-14
Applicant: TORAY INDUSTRIES
Inventor: AONO SHOJI , KONNO YOSHIHIRO , HIRAI SATOSHI
Abstract: PROBLEM TO BE SOLVED: To obtain the subject staple capable of providing a spun textile having not only high lightfastness but also bulking feeling, soft feeling and light feeling by heat treating a drawn fiber comprising a specific copolyester under a specified condition. SOLUTION: The objective staple fiber is obtained by extruding a copolyester including (A) isophthalic acid and (B) 2,2-bis 4-(2-hydroxyethoxy)phenyl}propane as copolymerizing components, simultaneously satisfying the formula I to III [P(a) is a molar fraction (%) of the component A in the whole acid components; P(b) is the molar fraction (%) of the component B in the whole glycol components] and having >=0.55 intrinsic viscosity, from a cap having nozzles comprising two or more slits, spinning and drawing the extruded fiber, and thereafter heat treating the drawn fiber by controlling the condition so that the initial water content of the drawn fiber at a heat treating zone may be >=5wt.%, a relaxation ratio may be (-2) to 5%, and a treating temperature may be 110-180 deg.C, to form the objective staple having 3% larger than that in 160 deg.C dry air after treating by the boiling water and
-
公开(公告)号:JPH09228238A
公开(公告)日:1997-09-02
申请号:JP3767796
申请日:1996-02-26
Applicant: TORAY INDUSTRIES
Inventor: KONNO YOSHIHIRO , NAGAHAMA AKIHIKO
IPC: D06M11/00 , D01D5/24 , D01F6/92 , D06M11/38 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32
Abstract: PROBLEM TO BE SOLVED: To obtain the subject short fiber capable of providing sufficient softness without greatly damaging fiber tenacity and physical properties of woven fabric, by blending a base polymer with a readily soluble polymer in spinning, fibrillating preferentially the tip part of the fiber when the fiber is subjected to weight-loss processing with a solvent. SOLUTION: This short fiber is obtained by a method for blending a base polymer such as a homopolyethylene terephthalate with a readily soluble polymer (e.g. a polyester copolymerized with 5mol% of 5-sodium sulfoisophthalate) by polymer blending in spinning and cutting the prepared fiber into =3 fiber number at the tip part of the short fiber when subjected to 10% weight loss processing with a solvent and >=1.3 ratio of the fibril number at the tip of the short fiber to that of a non-tip part of the short fiber.
-
公开(公告)号:JPH09228190A
公开(公告)日:1997-09-02
申请号:JP3841896
申请日:1996-02-26
Applicant: TORAY INDUSTRIES
Inventor: MIYAMOTO JINROKU , FUJIMOTO MASUKI , KONNO YOSHIHIRO
Abstract: PROBLEM TO BE SOLVED: To obtain a polyester pile fabric excellent in wearing amenities without sweaty unpleasantness and itchy irritation caused by static electricity by using polyester fibers having both of moisture-absorbing and antistatic properties as pile yarns and/or ground yarns. SOLUTION: A polyester copolymer prepared by copolymerizing a polyether- ester-amide block copolymer or dimethyl terephthalate/ethylene glycol/a polar group-bearing compound, for example, 5-sodiosulfo-isophthalic acid/trimethyl trimellitate is arranged in the fiber core and usual polyester is arranged in the sheath to prepare a sheath-core type conjugated fiber and the fiber is drawn to form a polyester fiber with moisture absorption and release parameter ΔMR of >=1%, frictionally charging voltage of .
-
公开(公告)号:JPH0835156A
公开(公告)日:1996-02-06
申请号:JP16374094
申请日:1994-07-15
Applicant: TORAY INDUSTRIES
Inventor: FUJIMOTO MASUKI , AOYANAGI ISAO , KONNO YOSHIHIRO
Abstract: PURPOSE:To obtain the lightweight and soft cushion material little in permanent set in fatigue setting and in compression residual strain, having good air permeability and moisture permeability, and comfortable in touch. CONSTITUTION:A modified PET as a thermoplastic polymer R1, PET as R2 and a modified PET having a melting point of 80-170 deg.C which is lower by at least 20 deg.C than the melting points of R1 and R2, as R3, are subjected to a bicomponent spinning treatment to obtain the latent crimping conjugate fiber having a fineness of 1-10 denier and a fiber length of 10-100mm, giving a crimp number N of 3-20 mountains / 25 mm and a crimping degree number ratio y expressed by an inequality of -0.07N+1.8
-
公开(公告)号:JPH0699856B2
公开(公告)日:1994-12-07
申请号:JP13797488
申请日:1988-06-03
Applicant: TORAY INDUSTRIES
Inventor: SASAMOTO FUTOSHI , OKADA TAKEHIKO , KONNO YOSHIHIRO
IPC: D04B1/16 , D03D15/00 , D03D27/00 , D04B1/02 , D04B1/04 , D04B21/04 , D06M13/02 , D06M13/165 , D06M101/00 , D06M101/16 , D06M101/30 , D06M101/32
-
-
-
-
-
-
-
-
-