Abstract:
A method for manufacturing an optical article including the steps of providing a substrate tube; forming one or more cladding layers inside the substrate tube, the one or more cladding layers including an innermost cladding layer; forming a concentric fluorine reservoir adjacent to the innermost cladding layer; and forming a core adjacent to the fluorine reservoir and concentric with the one or more outer cladding layers. The fluorine concentration in the fluorine reservoir is higher than the fluorine concentration in either the core or the innermost cladding layer.
Abstract:
A silica glass has a structure determination temperature of 1200 K or lower and an OH group concentration of at least 1,000 ppm. The silica glass is used for photolithography together with light in a wavelength region of 400 nm or shorter.
Abstract:
A silica glass has a structure determination temperature of 1200 K or lower and a hydrogen molecule concentration of 1.times.10.sup.17 molecules/cm.sup.3 or more. The silica glass is used together with light in a wavelength region of 400 nm or shorter.
Abstract translation:石英玻璃的结构测定温度为1200K以下,氢分子浓度为1×10 17分子/ cm 3以上。 石英玻璃与波长400nm以下的光一起使用。
Abstract:
A method of making a multicore optical fiber preform, the method including consolidating a preform assembly to form the multicore optical fiber preform, the preform assembly including a plurality of core canes such that each core cane is disposed within an axial hole of a sleeve, each core cane including a core section of alkali doped silica glass such that the silica glass has a maximum alkali concentration between about 0.10 wt. % and about 10 wt. %, the core section of each core cane being encased by the sleeve along a height of the core cane and by covers disposed at first and second axial ends of the core section, and the covers including silica glass having a chlorine concentration of about 0.05 wt. % or less.
Abstract:
A co-doped optical fiber is provided having an attenuation of less than about 0.17 dB/km at a wavelength of 1550 nm. The fiber includes a core in the fiber having a graded refractive index profile with an alpha of greater than 5. The fiber also includes a cladding in the fiber that surrounds the core addition, the core includes silica that is co-doped with two or more halogens.
Abstract:
One aspect relates to a light guide comprising a jacket and one or more cores, wherein the jacket surrounds the cores. Each core has a refractive index profile perpendicular to the maximum extension of the core, wherein at least one refractive index nK of each refractive index profile is greater than the refractive index nM1 of the jacket. The jacket is made of silicon dioxide and has an OH content of less than 10 ppm, a chlorine content of less than 60 ppm, and an aluminium content of less than 200 ppb. One aspect also relates to a silicon dioxide granulate I, characterized by a chlorine content of less than 200 ppm and an aluminium content of less than 200 ppb, in each case based on the total weight of the silicon dioxide granulate I.
Abstract:
An optical fiber preform includes a silica-glass core portion, and a cladding portion surrounding the core portion, the cladding portion being composed of a fluorine-containing silica glass having a lower refractive index than the core portion, the core portion including a first region that does not include the central axis thereof, the first region containing a first dopant selected from sodium, potassium, and compounds thereof, and a second region that includes the central axis, the second region containing a second dopant that reduces the viscosity of the silica glass, the second dopant having a diffusion coefficient of 1×10−12 cm2/s or more and less than the first dopant at 2,000° C. to 2,300° C., in which the entire core portion has an average first dopant concentration of 10 atomic ppm or more and 2,000 atomic ppm or less and an average second dopant concentration of 10 atomic ppm or more.
Abstract:
A high silica glass composition comprising about 92 to about 99.9999 wt. % SiO2 and from about 0.0001 to about 8 wt. % of at least one dopant selected from Al2O3, CeO2, TiO2, La2O3, Y2O3, Nd2O3, other rare earth oxides, and mixtures of two or more thereof. The glass composition has a working point temperature ranging from 600 to 2,000° C. These compositions exhibit stability similar to pure fused quartz, but have a moderate working temperature to enable cost effective fabrication of pharmaceutical packages. The glass is particularly useful as a packaging material for pharmaceutical applications, such as, for example pre-filled syringes, ampoules and vials.
Abstract:
An optical fiber with large effective area, low bending loss and low attenuation. The optical fiber includes a core, an inner cladding region, and an outer cladding region. The core region includes a spatially uniform updopant to minimize low Rayleigh scattering and a relative refractive index and radius configured to provide large effective area. The inner cladding region features a large trench volume to minimize bending loss. The core may be doped with Cl and the inner cladding region may be doped with F.
Abstract:
An optical component made of synthetic quartz glass includes a glass structure substantially free of oxygen defect sites and having a hydrogen content of 0.1×1016 to 1.0×1018 molecules/cm3, an SiH group content of less than 2×1017 molecules/cm3, a hydroxyl group content of 0.1 to 100 wt. ppm, and an Active temperature of less than 1070° C. The optical component undergoes a laser-induced change in the refractive index in response to irradiation by a radiation with a wavelength of 193 nm using 5×109 pulses with a pulse width of 125 ns and a respective energy density of 500 μJ/cm2 at a pulse repetition frequency of 2000 Hz. The change totals a first measured value M193 nm when measured using the applied wavelength of 193 nm and a second measured value M633 nm when measured using a measured wavelength of 633 nm. The ratio M193 nm/M633 nm is less than 1.7.