A COMBINATION OF MATERIALS FOR MERCURY-DISPENSING DEVICES AND DEVICES CONTAINING SAID COMBINATION OF MATERIALS
    3.
    发明申请
    A COMBINATION OF MATERIALS FOR MERCURY-DISPENSING DEVICES AND DEVICES CONTAINING SAID COMBINATION OF MATERIALS 有权
    用于汞分配装置的材料的组合和包含材料的组合的装置

    公开(公告)号:US20150294830A1

    公开(公告)日:2015-10-15

    申请号:US14438466

    申请日:2014-09-15

    Abstract: An improved mercury-dispensing combination of materials is made up of a compound A including mercury and a second metal selected among titanium, zirconium and mixtures thereof and an alloy or an intermetallic compound B including copper and tin, said mercury-dispensing combination of materials further containing an amount of oxygen comprised between 0.03% and 0.48% with respect to the overall weight of the composition A+B. It is also possible to add a getter material C that includes metals such as titanium, zirconium, tantalum, niobium, vanadium and mixtures thereof or their alloys with other metals such as nickel, iron, aluminum.

    Abstract translation: 改进的汞分配组合材料由包括汞和选自钛,锆及其混合物的第二金属的化合物A和包括铜和锡的合金或金属间化合物B组成,所述汞分配组合进一步 含有相对于组合物A + B的总重量在0.03%至0.48%之间的氧气的量。 还可以添加包括金属如钛,锆,钽,铌,钒及其混合物或其合金与其他金属如镍,铁,铝的金属的吸气剂材料C.

    Composite getters
    6.
    发明授权
    Composite getters 有权
    复合吸气剂

    公开(公告)号:US08864886B2

    公开(公告)日:2014-10-21

    申请号:US14347812

    申请日:2012-10-25

    CPC classification number: B01D53/04 H01J7/183

    Abstract: A composite getter system is described. The system has NEG materials coated with a polyimide or polyamide based compound.

    Abstract translation: 描述了复合吸气剂系统。 该系统具有涂覆有聚酰亚胺或聚酰胺基化合物的NEG材料。

    Method of forming layers of getter material on glass parts
    7.
    发明授权
    Method of forming layers of getter material on glass parts 失效
    在玻璃部件上形成吸气剂材料层的方法

    公开(公告)号:US08119209B2

    公开(公告)日:2012-02-21

    申请号:US12281178

    申请日:2007-03-02

    Abstract: A method of forming a layer (12) of getter particles (11) on a glass part (10) includes contacting the getter particles with the glass part and irradiating the particles through the glass by a laser, thus heating the particles at a temperature greater than the softening temperature of the glass but lower than the melting temperature of the particles.

    Abstract translation: 在玻璃部件(10)上形成吸气剂颗粒(11)的层(12)的方法包括使吸气剂颗粒与玻璃部分接触,并通过激光将玻璃上的颗粒照射,从而在更大的温度下加热颗粒 比玻璃的软化温度低但低于颗粒的熔融温度。

    GETTER MATERIAL AND EVAPORABLE GETTER DEVICE USING THE SAME, AND ELECTRON TUBE
    8.
    发明申请
    GETTER MATERIAL AND EVAPORABLE GETTER DEVICE USING THE SAME, AND ELECTRON TUBE 有权
    使用它的材料和可蒸发的设备,以及电子管

    公开(公告)号:US20100275727A1

    公开(公告)日:2010-11-04

    申请号:US12839230

    申请日:2010-07-19

    Abstract: The present invention provides a getter material configured by a pressed powder mixture comprising Ba—Al alloy powder and Ni powder, wherein when the pressed powder mixture is heated in a vacuum atmosphere or an inert gas atmosphere, a temperature at which an exothermic reaction starts is ranging from 750° C. to 900° C. According to this getter material, since the temperature at which the pressed powder mixture starts the exothermic reaction is set within a range from 750° C. to 900° C., there can be provided a getter material and an evaporation type getter device capable of suitably controlling an evaporation amount of getter components under a stable condition, and is excellent in responsiveness because a time ranging from a starting time of heating the getter material to a starting time of evaporation of the getter components can be shortened. In addition, the metal container to be filled with the getter material is free from deformation and melting, and a heat-evaporation process time of the getter material can be shortened, so that there can be provided the evaporation type getter device excellent in responsiveness because a time required for the electron tube to attain to a predetermined vacuum degree can be also shortened.

    Abstract translation: 本发明提供一种由包含Ba-Al合金粉末和Ni粉末的压制粉末混合物构成的吸气剂材料,其中当在真空气氛或惰性气体气氛中加压压粉混合物时,发生放热反应的温度为 根据该吸气剂材料,由于压粉混合物开始放热反应的温度设定在750℃至900℃的范围内,因此可以提供 吸气剂材料和蒸发型吸气装置,其能够在稳定的条件下适当地控制吸气剂组分的蒸发量,并且响应性优异,因为从吸气剂材料的加热开始时间到蒸发的起始时间 吸气剂组分可以缩短。 此外,要填充吸气剂材料的金属容器没有变形和熔化,并且可以缩短吸气剂材料的热蒸发处理时间,从而可以提供响应性优异的蒸发型吸气装置,因为 电子管达到预定真空度所需的时间也可以缩短。

    Field emission plane light source and method for making the same
    9.
    发明授权
    Field emission plane light source and method for making the same 有权
    场发射平面光源及其制作方法

    公开(公告)号:US07745983B2

    公开(公告)日:2010-06-29

    申请号:US11603639

    申请日:2006-11-21

    Abstract: A field emission plane light source generally incorporates an anode and a cathode. The anode includes an anode substrate, an anode conductive layer formed on a surface of the anode substrate, and a fluorescent layer formed on the anode conductive layer. The cathode includes a cathode substrate facing and separated from the anode substrate, a cathode conductive layer formed on a surface of the cathode substrate, and an electron emission layer formed on the cathode conductive layer and facing the fluorescent layer of the anode. The cathode and anode substrates have a seal formed therebetween. The electron emission layer includes a glass matrix and a plurality of carbon nanotubes, metallic conductive particles and getter powders dispersed therein. A method for making such field emission plane light source is also provided.

    Abstract translation: 场发射平面光源通常包含阳极和阴极。 阳极包括阳极衬底,形成在阳极衬底的表面上的阳极导电层和形成在阳极导电层上的荧光层。 阴极包括面对阳极基板的阴极基板,形成在阴极基板的表面上的阴极导电层和形成在阴极导电层上并与阳极的荧光层相对的电子发射层。 阴极和阳极基板之间形成有密封件。 电子发射层包括玻璃基体和分散在其中的多个碳纳米管,金属导电颗粒和吸气剂粉末。 还提供了制造这种场致发射平面光源的方法。