131.
    发明专利
    未知

    公开(公告)号:FI972059A0

    公开(公告)日:1997-05-14

    申请号:FI972059

    申请日:1997-05-14

    Applicant: BASF AG

    Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd

    134.
    发明专利
    未知

    公开(公告)号:DE4440837A1

    公开(公告)日:1996-05-23

    申请号:DE4440837

    申请日:1994-11-15

    Applicant: BASF AG

    Abstract: Biodegradable polyether esters P1 obtainable by the reaction of a mixture consisting essentially of: (a1) a mixture essentially of 20 to 95 mol% adipic acid or ester-forming derivatives thereof or mixtures thereof, 5 to 80 mol% terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0 to 5 mol% of a sulphonate group-containing compounds in which the sum of the individual mol percentages is 100; and (a2) a mixture of dihydroxy compounds consisting essentially of (a21) 15 to 99 mol% of a dihydroxy compound selected from the group consisting of C2-C6 alkane diols and C5-C10 cycloalkane diols; (a22) 85 to 0.2 mol% of an ether function-containing dihydroxy compound as in formula I HO-[(CH2)n-O]m-H in which n is 2, 3 or 4 and m is a whole number from 2 to 250, or mixtures thereof, in which the molar ratio of (a1) to (a2) is in the range from 0.4:1 to 1.5:1 with the proviso that the polyether esters P1 have a molar weight (Mn) in the range from 5,000 to 80,000 g/mol, a viscosity index in the range from 30 to 450 g/ml (measured in o-dichlorobenzole/phenol (weight ratio 50/50) at a concentration of 0.5 wt.% polyether esters P1 at a temperature of 25 DEG C) and a melting point in the range from 50 to 200 DEG C, and with the further proviso that from 0.01 to 5 mol%, in relation to the molar quantity of the components (a1) used, of a compound D with at least three groups capable of ester formation are used to produce the polyether esters P1, and other biodegradable polymers and thermoplastic moulding compounds, process for their production and biodegradable mouldings, adhesives, foams and blends with starch obtainable from the polymers or moulding compounds of the invention.

    BIODEGRADABLE POLYMERS, THE PREPARATION THEREOF, AND THE USETHEREOF FOR PRODUCING BIODEGRADABLE MOLDINGS

    公开(公告)号:CA2205072A1

    公开(公告)日:1996-05-23

    申请号:CA2205072

    申请日:1995-06-27

    Applicant: BASF AG

    Abstract: Biodegradable polyether esters P1 obtainable by the reaction of a mixture consisting essentially of: (a1) a mixture essentially of 20 to 95 mol% adipic acid or ester-forming derivatives thereof or mixtures thereof, 5 to 80 mol% terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0 to 5 mol% of a sulphonate group-containing compounds in which the sum of the individual mol percentages is 100; and (a2) a mixture of dihydroxy compounds consisting essentially of (a21) 15 to 99 mol% of a dihydroxy compound selected from the group consisting of C2-C6 alkane diols and C5-C10 cycloalkane diols; (a22) 85 to 0.2 mol% of an ether function-containing dihydroxy compound as in formula I HO-¢(CH2)n-O!m-H in which n is 2, 3 or 4 and m is a whole number from 2 to 250, or mixtures thereof, in which the molar ratio of (a1) to (a2) is in the range from 0.4:1 to 1.5:1 with the proviso that the polyether esters P1 have a molar weight (Mn) in the range from 5,000 to 80,000 g/mol, a viscosity index in the range from 30 to 450 g/ml (measured in o-dichlorobenzole/phenol (weight ratio 50/50) at a concentration of 0.5 wt.% polyether esters P1 at a temperature of 25 ~C) and a melting point in the range from 50 to 200 ~C, and with the further proviso that from 0.01 to 5 mol%, in relation to the molar quantity of the components (a1) used, of a compound D with at least three groups capable of ester formation are used to produce the polyether esters P1, and other biodegradable polymers and thermoplastic moulding compounds, process for their production and biodegradable mouldings, adhesives, foams and blends with starch obtainable from the polymers or moulding compounds of the invention.