181.
    发明专利
    未知

    公开(公告)号:DE10158652A1

    公开(公告)日:2003-06-12

    申请号:DE10158652

    申请日:2001-11-30

    Applicant: BASF AG

    Abstract: An aqueous polymer dispersion with a polymerisate in disperse distribution in a radically polymerized form is synthesized from at least one vinyl aromatic monomer A; a doubly conjugated ethylenically unsaturated monomer B; and a monomer C selected from alpha, beta-monoethylenically unsaturated mono- and dicarboxylic acids or their amide or ester derivatives. An aqueous polymer dispersion with a polymerisate in disperse distribution in a radically polymerized form synthesized from (wt.%): at east one vinyl aromatic monomer (monomer A)(20-65); at least one doubly conjugated ethylenically unsaturated double bonded monomer (monomer B)(30-75); and at least one other monomer (monomer C)(0.5-10) selected from alpha,beta-monoethylenically unsaturated mono- and dicarboxylic acids or their amide or ester derivatives, and their content GA of alkali metal ion, relative to the weight of dispersed polymerisate is ≥ 0.5 wt.% , where the pH of the aqueous dispersion medium is set at a value lower than 6 is new. An Independent claim is included for preparation of the aqueous polymer dispersion by radical emulsion polymerization of the starting monomers A, B, and C in the required ratios for production of the polymer, with setting of the pH of the aqueous dispersion medium at below 6 by addition of a specific amount of aqueous alkali metal hydroxide solution.

    187.
    发明专利
    未知

    公开(公告)号:ES2137778T3

    公开(公告)日:1999-12-16

    申请号:ES97905047

    申请日:1997-02-19

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP97/00768 Sec. 371 Date Aug. 21, 1998 Sec. 102(e) Date Aug. 21, 1998 PCT Filed Feb. 19, 1997 PCT Pub. No. WO97/31059 PCT Pub. Date Aug. 28, 1997A method for forming shaped products by mixing a formaldehyde-free aqueous binder comprising A) a free-radically polymerized polymer containing from 5 to 100% by weight of units derived from an ethylenically unsaturated acid anhydride or from an ethylenically unsaturated dicarboxylic acid whose carboxyl group can form an anhydride group, and B) an alkanolamine having at least two hydroxyl groups, with fibers or chips to form a shaped article, wherein said binder has a property of drying at 50 DEG C. in 72 hours to a film from 0.3 to 1 mm in thickness and, following a subsequent 15 minute cure at 130 DEG C. in air, has a gel content of above 50% by weight, wherein the binder includes less than 0.1% by weight, based on A)+B), of a phosphorus-containing reaction accelerant with fibers or chips.

    188.
    发明专利
    未知

    公开(公告)号:NO306610B1

    公开(公告)日:1999-11-29

    申请号:NO915072

    申请日:1991-12-20

    Applicant: BASF AG

    Abstract: A concrete tile (I) is claimed, which is coated with a copolymer (A) with Tg -25 to +30 deg.C, derived from (a) 0.1-10 wt.% monomer of formula R1CH=CR2-CO-X-R3-Z-CHR4R5 (III), (b) 85-99.9 wt.% at least 2 monomers of the type (1-24C alkyl) (meth)acrylates, vinyl esters of 1-20C carboxylic acids, up to 20C vinylaromatics, 3-6C unsatd. nitriles, vinyl halides and/or 2-8C non-aromatic hydrocarbons with olefinic double bond(s), and (c) 0-10 wt.% other Sn-free comonomers; R1, R2 = H or 1-4C alkyl; R3 = 1-20C bridging gp.; R4 = -COR6, -COOR6 or CN; R5 = H, -COR9, -COOR9 or CN; X = O or NR7; Z = single bond, CH2, O, NR8 or -OCO-; (with R6-R9 = H, or 1-12C alkyl, aryl, alkaryl or aralkyl). Also claimed is a process for the prodn. of (I), by application of an aq. prepn. contg. (A) to at least one surface of the green concrete, and drying the prepn. by hardening the concrete. More specifically, monomer (a) is acetylacetoxyethyl (meth)acrylate, acetylacetoxybutyl (meth)acrylate, cyanoacetoxyethyl (meth)acrylate, 1,1-dibenzoyl-2-(meth)acrylamidoethane, 1-benzoyl-1-acetyl-2- (meth)acrylamidoethane, or ethyl alpha-benzoyl-beta-(meth) acrylamidopropionate, and (b) are vinylaromatics or (1-8C alkyl) (meth)acrylates; (I) is coated with a prepn. contg. copolymer (A) and up to 450 wt.% mineral additives (B) and/or colour pigments (C) (w.r.t. amt. of A); another layer of the aq. prepn. is applied to the hardened tile and dried; the amt. of prepn. used is such that the total amt. of dry coating is 50-500 g/m2.

    189.
    发明专利
    未知

    公开(公告)号:AT184898T

    公开(公告)日:1999-10-15

    申请号:AT97905047

    申请日:1997-02-19

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP97/00768 Sec. 371 Date Aug. 21, 1998 Sec. 102(e) Date Aug. 21, 1998 PCT Filed Feb. 19, 1997 PCT Pub. No. WO97/31059 PCT Pub. Date Aug. 28, 1997A method for forming shaped products by mixing a formaldehyde-free aqueous binder comprising A) a free-radically polymerized polymer containing from 5 to 100% by weight of units derived from an ethylenically unsaturated acid anhydride or from an ethylenically unsaturated dicarboxylic acid whose carboxyl group can form an anhydride group, and B) an alkanolamine having at least two hydroxyl groups, with fibers or chips to form a shaped article, wherein said binder has a property of drying at 50 DEG C. in 72 hours to a film from 0.3 to 1 mm in thickness and, following a subsequent 15 minute cure at 130 DEG C. in air, has a gel content of above 50% by weight, wherein the binder includes less than 0.1% by weight, based on A)+B), of a phosphorus-containing reaction accelerant with fibers or chips.

Patent Agency Ranking