公开(公告)号:DE59702242D1
公开(公告)日:2000-09-28
申请号:DE59702242
申请日:1997-05-28
Applicant: BASF AG
Inventor: WEBER MARTIN , WEISS ROBERT , HECKMANN WALTER , HINGMANN ROLAND , HAEHNLE HANS-JOACHIM
Abstract: Flame-retardant thermoplastic molding materials containingA) at least one polyphenylene ether,B) at least one vinylaromatic polymer, andC) at least one flameproofing agent furthermore compriseD) as an antidrip agent, a high molecular weight polymer based on acrylamide having a viscosity of more than about 1.5 mpas, measured in 0.1% strength aqueous solution at 25° C.,and are used for the production of fibers, films and moldings.
-
公开(公告)号:ES2142596T3
公开(公告)日:2000-04-16
申请号:ES96923950
申请日:1996-06-27
Applicant: BASF AG
Inventor: WEBER MARTIN , HOFMANN JURGEN , WEISS ROBERT , HECKMANN WALTER , HINGMANN ROLAND , WUNSCH JOSEF
IPC: C08F2/14 , C08F12/00 , C08L53/02 , C08F12/06 , C08L25/00 , C08L25/06 , C08L71/12 , C08L101/00 , D01F6/46 , D01F6/66 , D01F6/94
Abstract: PCT No. PCT/EP96/02803 Sec. 371 Date Jan. 5, 1998 Sec. 102(e) Date Jan. 5, 1998 PCT Filed Jun. 27, 1996 PCT Pub. No. WO97/02299 PCT Pub. Date Jan. 23, 1997Halogen-free antidrip agents for thermoplastic molding materials contain polymers based on vinylaromatic monomers and having molecular weights (Mw) of at least 800 000 g/mol and a narrow molecular weight distribution.
-
公开(公告)号:DE59604054D1
公开(公告)日:2000-02-03
申请号:DE59604054
申请日:1996-06-27
Applicant: BASF AG
Inventor: WEBER MARTIN , HOFMANN JUERGEN , WEISS ROBERT , HECKMANN WALTER , HINGMANN ROLAND , WUENSCH JOSEF , MCKEE GRAHAM
IPC: C08F2/14 , C08F12/00 , C08L53/02 , C08F12/06 , C08L25/00 , C08L25/06 , C08L71/12 , C08L101/00 , D01F6/46 , D01F6/66 , D01F6/94
Abstract: PCT No. PCT/EP96/02803 Sec. 371 Date Jan. 5, 1998 Sec. 102(e) Date Jan. 5, 1998 PCT Filed Jun. 27, 1996 PCT Pub. No. WO97/02299 PCT Pub. Date Jan. 23, 1997Halogen-free antidrip agents for thermoplastic molding materials contain polymers based on vinylaromatic monomers and having molecular weights (Mw) of at least 800 000 g/mol and a narrow molecular weight distribution.
-
公开(公告)号:AU1032497A
公开(公告)日:1997-06-19
申请号:AU1032497
申请日:1996-11-28
Applicant: BASF AG
-
公开(公告)号:DE4421929A1
公开(公告)日:1996-01-04
申请号:DE4421929
申请日:1994-06-23
Applicant: BASF AG
Inventor: MARCZINKE BERND LOTHAR DR , SCHWAGER HARALD DR , HINGMANN ROLAND , HOFMANN JUERGEN , SEELERT STEFAN DR
Abstract: Partly crosslinked plastic materials (A) with a melt flow index 230/2.16 of 0.1-100 g/10 minutes are obtd from: (a1) a polymer contg: (a1.1) 25-97 wt% of a copolymer of propylene with 0.1-15 wt% 2-10C alkene-1, and (a1.2) 3-75 wt% of a copolymer of propylene with 15-80 wt% 2-10C alkene-1; or (a2) a polymer contg: (a2.1) 25-97 wt% propylene homopolymer, and (a2.2) 3-75 wt% copolymer (a1.2) as above; or (a3) a propylene homopolymer with a melt flow index 230/2 of 0.1-100 g/10 minutes; or (a4) a statistical propylene copolymer contg less than 15 wt% 2-10C alkene-1 comonomer; and (b) a cpd of formula: (H2C=CR-COO)nX (I) R = H or 1-4C alkyl; X = 1-30C alkyl or 7-30C aralkyl, opt contg in-chain O and/or N atom(s); and n = 2 or 3; and these materials (A) are obtd by reacting (a1), (a2), (a3) or (a4) with cpd (b) at 180-280 deg C and 1-100 bar for a mean residence time of 0.2-10 minutes. Also claimed are: (i) a process for the prodn of (A) by reacting the above polymers with (b) at 190-260 deg C and 1-60 bar for a mean residence time of 0.2-5 minutes, pref immediately after prodn of the polymer in a mixer connected to the polymerisation reactor; and (ii) films, fibres and mouldings made from (A).
-
16.
公开(公告)号:ZA934259B
公开(公告)日:1994-12-19
申请号:ZA934259
申请日:1993-06-16
Applicant: BASF AG
Inventor: MARCZINKE BERND LOTHAR , SCHWAGER HARALD , BROSIUS SIBYLLE , WERNER RAINER ALEXANDER , SCHERER GUENTER , KERTH JUERGEN , HUNGENBERG KLAUS-DIETER , HINGMANN ROLAND , HUBER KARL
IPC: C08K5/3415 , C08L23/10 , C08F , C08L
-
17.
公开(公告)号:ZA9304259B
公开(公告)日:1994-12-19
申请号:ZA9304259
申请日:1993-06-16
Applicant: BASF AG
Inventor: MARCZINKE BERND LOTHAR , SCHWAGER HARALD , BROSIUS SIBYLLE , WERNER RAINER ALEXANDER , SCHERER GUENTER , KERTH JUERGEN , HUNGENBERG KLAUS-DIETER , HINGMANN ROLAND , HUBER KARL
IPC: C08K5/3415 , C08L23/10 , C08F , C08L
CPC classification number: C08K5/3415 , C08L23/142 , C08L23/16 , C08L2205/02 , C08L2312/00 , C08L23/10 , C08L2666/06
-
公开(公告)号:ES2150779T3
公开(公告)日:2000-12-01
申请号:ES97927077
申请日:1997-05-28
Applicant: BASF AG
Inventor: WEBER MARTIN , WEISS ROBERT , HECKMANN WALTER , HINGMANN ROLAND , HAHNLE HANS-JOACHIM
Abstract: Flame-retardant thermoplastic molding materials containingA) at least one polyphenylene ether,B) at least one vinylaromatic polymer, andC) at least one flameproofing agent furthermore compriseD) as an antidrip agent, a high molecular weight polymer based on acrylamide having a viscosity of more than about 1.5 mpas, measured in 0.1% strength aqueous solution at 25° C.,and are used for the production of fibers, films and moldings.
-
公开(公告)号:DE59700842D1
公开(公告)日:2000-01-20
申请号:DE59700842
申请日:1997-09-09
Applicant: BASF AG
Inventor: HUEFFER STEPHAN , MOLL ULRICH , MCKENZIE IAN DAVID , LANGHAUSER FRANZ , KOELLE PETER , HINGMANN ROLAND , SCHWEIER GUENTHER , HEMMERICH RAINER , KERTH JUERGEN
-
公开(公告)号:DE59700778D1
公开(公告)日:2000-01-05
申请号:DE59700778
申请日:1997-04-17
Applicant: BASF AG
Inventor: FISCHER DAVID , FRANK HELMUT , LUX MARTIN , HINGMANN ROLAND , SCHWEIER GUENTHER
IPC: C08F4/64 , C08F2/34 , C08F2/44 , C08F4/602 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/646 , C08F4/6592 , C08F4/68 , C08F10/00 , C08F10/06 , C08F110/06 , C08F210/16 , C08J5/18 , D01F6/04 , D01F6/06 , D01F6/30
Abstract: A method for the preparation of 2-12C alpha-olefin polymers at -50 to +300 degrees C and 0.5-3000 bar in the presence of a catalyst system - uses a catalyst that contains the following components :(A) an (in)organic carrier ; (B) a metallocene complex ; (C) a metallocenium ion-forming compound ; and (D) optionally a metal compound of formula (I). M )r(R )s(R )t (I) M = alkali(ne earth) or Group III metal ; R = H, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl or 6-20C aryl-(1-10C)-alkyl ; R , R = H, halogen, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl, 6-20C aryl-(1-10C)-alkyl or 1-10C alkoxy ; r = 1-3 ; and s, t = 0-2, with the provision that the sum of r-t is equal to the valency of M . An anti-static agent is also used with the catalyst.
-
-
-
-
-
-
-
-
-