公开(公告)号:JPH1060032A
公开(公告)日:1998-03-03
申请号:JP10415397
申请日:1997-04-22
Applicant: BASF AG
Inventor: FISCHER DAVID DR , FRANK HELMUT , LUX MARTIN DR , HINGMANN ROLAND DR , SCHWEIER GUENTHER DR
IPC: C08F4/64 , C08F2/34 , C08F2/44 , C08F4/602 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/646 , C08F4/6592 , C08F4/68 , C08F10/00 , C08F10/06 , C08F110/06 , C08F210/16 , C08J5/18 , D01F6/04 , D01F6/06 , D01F6/30
Abstract: PROBLEM TO BE SOLVED: To produce the subject polymer having a narrow mol.wt. distribution in a state capable of being performed in an industrial scale by carrying out the polymerization in the presence of a specific catalyst composition. SOLUTION: This method for producing an alkene-1 polymer comprises polymerizing an alkene-1 at a temperature of -50 to 300 deg.C in a pressure of 0.5-3000 bars in the presence of a catalyst composition comprising (A) an inorganic or organic carrier, (B) a metallocene complex, (C) a compound forming an metallocene ion and, if necessary, (D) a metal compound of the formula [M is an alkali(ne earth) metal, a metal belonging to the group III main elements in the periodic table; R is H, a 1-10C alkyl, a 6-15C aryl, an alkylaryl; R , R are each H, a halogen, a 1-10C alkyl, a 6-15C aryl, etc.; (r) is 1-3; (s) and (t) are each 0, 2, wherein (r)+(s)+(t) corresponds to the atomic valency of M ] and (E) an antistatic agent. The alkene-1 preferably comprises 50-100mol.% of propene, 0-50mol.% of ethylene and 0-20mol.% of a 4-12C alkene-1.
-
公开(公告)号:DE19615953A1
公开(公告)日:1997-10-23
申请号:DE19615953
申请日:1996-04-22
Applicant: BASF AG
Inventor: FISCHER DAVID DR , FRANK HELMUT , LUX MARTIN DR , HINGMANN ROLAND DR , SCHWEIER GUENTHER DR
IPC: C08F4/64 , C08F2/34 , C08F2/44 , C08F4/602 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/646 , C08F4/6592 , C08F4/68 , C08F10/00 , C08F10/06 , C08F110/06 , C08F210/16 , C08J5/18 , D01F6/04 , D01F6/06 , D01F6/30
Abstract: A method for the preparation of 2-12C alpha-olefin polymers at -50 to +300 degrees C and 0.5-3000 bar in the presence of a catalyst system - uses a catalyst that contains the following components :(A) an (in)organic carrier ; (B) a metallocene complex ; (C) a metallocenium ion-forming compound ; and (D) optionally a metal compound of formula (I). M )r(R )s(R )t (I) M = alkali(ne earth) or Group III metal ; R = H, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl or 6-20C aryl-(1-10C)-alkyl ; R , R = H, halogen, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl, 6-20C aryl-(1-10C)-alkyl or 1-10C alkoxy ; r = 1-3 ; and s, t = 0-2, with the provision that the sum of r-t is equal to the valency of M . An anti-static agent is also used with the catalyst.
-
公开(公告)号:ES2140931T3
公开(公告)日:2000-03-01
申请号:ES97106319
申请日:1997-04-17
Applicant: BASF AG
Inventor: FISCHER DAVID DR , FRANK HELMUT , LUX MARTIN DR , HINGMANN ROLAND DR , SCHWEIER GUNTHER DR
IPC: C08F4/64 , C08F2/34 , C08F2/44 , C08F4/602 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/646 , C08F4/6592 , C08F4/68 , C08F10/00 , C08F10/06 , C08F110/06 , C08F210/16 , C08J5/18 , D01F6/04 , D01F6/06 , D01F6/30
Abstract: A method for the preparation of 2-12C alpha-olefin polymers at -50 to +300 degrees C and 0.5-3000 bar in the presence of a catalyst system - uses a catalyst that contains the following components :(A) an (in)organic carrier ; (B) a metallocene complex ; (C) a metallocenium ion-forming compound ; and (D) optionally a metal compound of formula (I). M )r(R )s(R )t (I) M = alkali(ne earth) or Group III metal ; R = H, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl or 6-20C aryl-(1-10C)-alkyl ; R , R = H, halogen, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl, 6-20C aryl-(1-10C)-alkyl or 1-10C alkoxy ; r = 1-3 ; and s, t = 0-2, with the provision that the sum of r-t is equal to the valency of M . An anti-static agent is also used with the catalyst.
-
公开(公告)号:DE59700778D1
公开(公告)日:2000-01-05
申请号:DE59700778
申请日:1997-04-17
Applicant: BASF AG
Inventor: FISCHER DAVID , FRANK HELMUT , LUX MARTIN , HINGMANN ROLAND , SCHWEIER GUENTHER
IPC: C08F4/64 , C08F2/34 , C08F2/44 , C08F4/602 , C08F4/639 , C08F4/6392 , C08F4/642 , C08F4/646 , C08F4/6592 , C08F4/68 , C08F10/00 , C08F10/06 , C08F110/06 , C08F210/16 , C08J5/18 , D01F6/04 , D01F6/06 , D01F6/30
Abstract: A method for the preparation of 2-12C alpha-olefin polymers at -50 to +300 degrees C and 0.5-3000 bar in the presence of a catalyst system - uses a catalyst that contains the following components :(A) an (in)organic carrier ; (B) a metallocene complex ; (C) a metallocenium ion-forming compound ; and (D) optionally a metal compound of formula (I). M )r(R )s(R )t (I) M = alkali(ne earth) or Group III metal ; R = H, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl or 6-20C aryl-(1-10C)-alkyl ; R , R = H, halogen, 1-10C alkyl, 6-15C aryl, 1-10C alkyl-(6-20C)-aryl, 6-20C aryl-(1-10C)-alkyl or 1-10C alkoxy ; r = 1-3 ; and s, t = 0-2, with the provision that the sum of r-t is equal to the valency of M . An anti-static agent is also used with the catalyst.
-
-
-