公开(公告)号:DE102005031491A1
公开(公告)日:2007-01-11
申请号:DE102005031491
申请日:2005-07-04
Applicant: DEGUSSA
Inventor: DOWE ANDREAS , GOERING RAINER , BOEER MICHAEL , WURSCHE ROLAND , HIMMELMANN MARTIN , BAUMANN FRANZ-ERICH , KUHMANN KARL
IPC: C08L77/00 , B29C47/06 , B32B27/08 , B32B27/34 , C08L69/00 , C09D169/00 , C09D177/00
Abstract: The use of moulding materials (I) containing (a) 100 parts by weight (pts. wt.) polyamide and (b) 0.005-10 pts. wt. of a compound (II) with at least two carbonate units, for coextrusion with a moulding material (III) based on a high-melting polymer with a crystallite melting point (Tm) of at least 255 deg C and/or a glass transition point(Tg)of at least 180 deg C. Independent claims are included for (1) a method for the production of multilayer composites by making a polyamide moulding material, mixing this with 0.005-10 pts. wt. (II) per 100 pts. wt. polyamide, optionally storing and/or transporting the mixture and then coextruding it with (III) (2) multilayer composites obtained by this method .
-
公开(公告)号:BRPI0600419A
公开(公告)日:2006-10-03
申请号:BRPI0600419
申请日:2006-02-15
Applicant: DEGUSSA
Inventor: DOWE ANDREAS , RING RAINER G , HIMMELMANN MARTIN , BOLLMANN SONJA , BAUMANN FRANZ-ERICH , WURSCHE ROLAND
Abstract: Preparation of molded articles under condensation of a polyamide molded mass (A), where the polyamide portion contains at least 5 ppm of phosphorus in the form of acid compound, with a compound (I) having at least two carbonate units, comprises adding 0.001-10 wt.% of a salt of a weak acid to (A) before/during compounding, preparing a mixture of finished compounds and (I), transporting the mixture, which is optionally stored, and processing the mixture to molded articles, where the condensation is carried out first. An independent claim is included for a molded mass obtained by the process.
-
公开(公告)号:DE50207375D1
公开(公告)日:2006-08-10
申请号:DE50207375
申请日:2002-11-20
Applicant: DEGUSSA
Inventor: BAUMANN FRANZ-ERICH DR , HIMMELMANN MARTIN , BARTZ WILFRIED DR , FARGES OLIVIER
Abstract: A molding composition comprises (wt.%): (A) a polyetheramide (99.9-95) based on a linear 6-12C aliphatic diamine, a linear 6-12C aliphatic or aromatic dicarboxylic acid and a primary amine-terminated polyetherdiamine with at least3C per ether oxygen atom; and (B) a copolymer (0.1-5) containing acid anhydride or epoxide units (0.8-20). A molding composition comprises (wt.%): (A) a polyetheramide (99.9-95) based on a linear 6-12C aliphatic diamine, a linear 6-12C aliphatic or aromatic dicarboxylic acid and a primary amine-terminated polyetherdiamine with at least3C per ether oxygen atom; and (B) a copolymer (0.1-5) containing: (i) acrylate units of formula (I) (0-85); (ii) imide units of formula (II) (0-80); (iii) acrylic acid units of formula (III) (0-15); (iv) acid anhydride or epoxide units of formula (IVA) or (IVB) respectively (0.8-20); and (v) 0-95% hydrocarbon units of formula (V) (0-95). Alkyl = 1-6C alkyl; R1 - R7 = H, CnH2n+1 or phenyl; m = 0 or 1; and n = 1-6.
-
公开(公告)号:DE50101434D1
公开(公告)日:2004-03-11
申请号:DE50101434
申请日:2001-10-26
Applicant: DEGUSSA
Inventor: HAEGER DR , SCHMITZ DR , RICHTER DR , BARTZ DR , BAUMANN DR , HIMMELMANN MARTIN , OENBRINK DR
Abstract: A molding composition of at least 50% by weight of a polyamine-polyamide copolymer obtained from 0.05 to 2.5% by weight of a polyamine having at least 4 nitrogen atoms and having a viscosity of at least 5 000 Pa.s at 250° C. and at a shear rate of 0.1 l/s, and having a viscosity ratio of at least 7 at 250° C., when the melt viscosities at shear rates of 0.1 l/s and 100 l/s are compared with one another, has high melt stiffness and is easy to cut, and performs well in blow molding.
-
公开(公告)号:AT258962T
公开(公告)日:2004-02-15
申请号:AT01125584
申请日:2001-10-26
Applicant: DEGUSSA
Inventor: HAEGER HARALD , SCHMITZ GUIDO , RICHTER RALF , BARTZ WILFRIED , BAUMANN FRANZ-ERICH , HIMMELMANN MARTIN , OENBRINK GEORG
Abstract: A molding composition of at least 50% by weight of a polyamine-polyamide copolymer obtained from 0.05 to 2.5% by weight of a polyamine having at least 4 nitrogen atoms and having a viscosity of at least 5 000 Pa.s at 250° C. and at a shear rate of 0.1 l/s, and having a viscosity ratio of at least 7 at 250° C., when the melt viscosities at shear rates of 0.1 l/s and 100 l/s are compared with one another, has high melt stiffness and is easy to cut, and performs well in blow molding.
-
公开(公告)号:BR0300051A
公开(公告)日:2003-09-02
申请号:BR0300051
申请日:2003-01-15
Applicant: DEGUSSA
Inventor: HIMMELMANN MARTIN , BARTZ WILFRIED , BAUMANN FRANZ-ERICH , FRAGES OLIVIER
Abstract: A molding composition comprises (wt.%): (A) a polyetheramide (99.9-95) based on a linear 6-12C aliphatic diamine, a linear 6-12C aliphatic or aromatic dicarboxylic acid and a primary amine-terminated polyetherdiamine with at least3C per ether oxygen atom; and (B) a copolymer (0.1-5) containing acid anhydride or epoxide units (0.8-20). A molding composition comprises (wt.%): (A) a polyetheramide (99.9-95) based on a linear 6-12C aliphatic diamine, a linear 6-12C aliphatic or aromatic dicarboxylic acid and a primary amine-terminated polyetherdiamine with at least3C per ether oxygen atom; and (B) a copolymer (0.1-5) containing: (i) acrylate units of formula (I) (0-85); (ii) imide units of formula (II) (0-80); (iii) acrylic acid units of formula (III) (0-15); (iv) acid anhydride or epoxide units of formula (IVA) or (IVB) respectively (0.8-20); and (v) 0-95% hydrocarbon units of formula (V) (0-95). Alkyl = 1-6C alkyl; R1 - R7 = H, CnH2n+1 or phenyl; m = 0 or 1; and n = 1-6.
-
公开(公告)号:BRPI0602498A
公开(公告)日:2007-03-06
申请号:BRPI0602498
申请日:2006-07-03
Applicant: DEGUSSA
Inventor: DOWE ANDREAS , GOERING RAINER , BOOER MICHAEL , WURSCHE ROLAND , HIMMELMANN MARTIN , BAUMANN FRANZ-ERICH , KUHMANN KARL
Abstract: The use of moulding materials (I) containing (a) 100 parts by weight (pts. wt.) polyamide and (b) 0.005-10 pts. wt. of a compound (II) with at least two carbonate units, for coextrusion with a moulding material (III) based on a high-melting polymer with a crystallite melting point (Tm) of at least 255 deg C and/or a glass transition point(Tg)of at least 180 deg C. Independent claims are included for (1) a method for the production of multilayer composites by making a polyamide moulding material, mixing this with 0.005-10 pts. wt. (II) per 100 pts. wt. polyamide, optionally storing and/or transporting the mixture and then coextruding it with (III) (2) multilayer composites obtained by this method .
-
公开(公告)号:NO20043051L
公开(公告)日:2005-01-19
申请号:NO20043051
申请日:2004-07-16
Applicant: DEGUSSA
Inventor: BARTZ WILFRIED , HIMMELMANN MARTIN , BAUMANN FRANZ-ERICH , FARGES OLIVIER
IPC: B29C45/00 , C08L77/06 , B29C47/00 , B29C49/04 , C08L23/08 , C08L33/14 , C08L53/00 , C08L77/12 , C08L79/00 , C08L77/00
Abstract: A composition (C1) comprises (pbw) a polyetheramide (a1) (80 - 97, preferably 85 - 95) containing linear 6-14C aliphatic diamine, linear 6-14C aliphatic or aromatic dicarboxylic acid, and polyetherdiamines having at least 3C per ether oxygen and having primary amino groups at the chain ends; and a rubber (b1) (3 - 20, preferably 5 - 15) containing at least one functional group. An independent claim is included for a molding produced from (C1).
-
公开(公告)号:CZ20030167A3
公开(公告)日:2003-09-17
申请号:CZ20030167
申请日:2003-01-17
Applicant: DEGUSSA
Inventor: HIMMELMANN MARTIN , BARTZ WILFRIED DR , BAUMANN FRANZ-ERICH DR , FARGES OLIVIER
CPC classification number: C08L77/00 , C08G69/40 , C08L23/08 , C08L33/06 , C08L33/064 , C08L33/068 , C08L33/24 , C08L77/06 , Y10T428/13 , Y10T428/1352 , Y10T428/139 , Y10T428/1397 , C08L2666/06 , C08L33/00 , C08L23/00
-
公开(公告)号:NO20030255L
公开(公告)日:2003-07-21
申请号:NO20030255
申请日:2003-01-17
Applicant: DEGUSSA
Inventor: HIMMELMANN MARTIN , BARTZ WILFRIED , BAUMANN FRANZ-ERICH , FARGES OLIVIER
Abstract: A molding composition comprises (wt.%): (A) a polyetheramide (99.9-95) based on a linear 6-12C aliphatic diamine, a linear 6-12C aliphatic or aromatic dicarboxylic acid and a primary amine-terminated polyetherdiamine with at least3C per ether oxygen atom; and (B) a copolymer (0.1-5) containing acid anhydride or epoxide units (0.8-20). A molding composition comprises (wt.%): (A) a polyetheramide (99.9-95) based on a linear 6-12C aliphatic diamine, a linear 6-12C aliphatic or aromatic dicarboxylic acid and a primary amine-terminated polyetherdiamine with at least3C per ether oxygen atom; and (B) a copolymer (0.1-5) containing: (i) acrylate units of formula (I) (0-85); (ii) imide units of formula (II) (0-80); (iii) acrylic acid units of formula (III) (0-15); (iv) acid anhydride or epoxide units of formula (IVA) or (IVB) respectively (0.8-20); and (v) 0-95% hydrocarbon units of formula (V) (0-95). Alkyl = 1-6C alkyl; R1 - R7 = H, CnH2n+1 or phenyl; m = 0 or 1; and n = 1-6.
-
-
-
-
-
-
-
-
-