Abstract:
본 발명에 따른 발전장치가 구비된 모바일 케이스는 모바일 장치를 감싸는 커버부, 상기 커버부에 연장 형성되며 내부에 공간을 형성하는 하우징, 상기 하우징의 내부에 구비되고, 외부에서 인가되는 외력에 의해 전력을 발생시키는 발전장치, 상기 발전장치의 일측에 구비되어 상기 외력에 의한 진동을 증가시켜 전력 발생효율을 증가시키기 위한 제1진동보조장치, 및 상기 발전장치와 이격되도록 구비되어 제1진동보조장치의 운동을 유도하는 제2진동보조장치를 포함한다.
Abstract:
The present invention relates to a metal-ceramic layered composite material and a method for manufacturing the same and, more particularly, to a method for manufacturing a metal-ceramic layered composite material including a step for simultaneously surface-treating a metal and ceramic, which are bonding targets, in a vacuum chamber by using plasma; and a step for bonding the metal and the ceramic during the surface treatment process, in which the surface treatment and the bonding are performed at room temperature, and a metal-ceramic layered composite material manufactured by using the manufacturing method described above. According to the present invention, surfaces of the metal and the ceramic, which constitute the composite material, are cleaned and activated by using the plasma in a high-vacuum state, and thus foreign matters generated on the surfaces can be easily removed. Also, the possibility of foreign matter growth, in which the foreign matters are nuclei, is extremely low. Accordingly, the manufactured composite material can be uniform in material properties and improved in performance.
Abstract:
본 발명의 플라스틱 사출 금형용 알루미늄 합금의 표면처리 방법은, 강산 수용액을 사용하여 알루미늄 합금 표면의 이물질 및 산화층을 제거하는 전처리단계, 상기 전처리단계를 거친 알루미늄 합금을 50g/L~70g/L의 농도의 수산 전해액 속에 담그고, 20℃~30℃의 온도에서 30분~90분간 1.0A/d㎡~2.0A/d㎡의 전류 밀도를 가지는 직류 전류를 가하여 알루미늄 산화물의 피막을 형성하는 양극산화단계 및 상기 피막 처리된 알루미늄 합금을 실링 처리하는 실링단계를 포함한다.
Abstract:
본 발명은 도금 및 표면처리 분야에서 모재와 코팅층의 밀착력 평가시 기준으로 삼을 수 있는 도금층의 스트레스를 측정하는 방법에 관한 것으로서, 실리콘 스트립 기판에 도금층을 형성시킨 후, 곡률반경 측정장치를 이용하여 상기 도금층의 스트레스를 측정하는 도금층의 스트레스 측정방법을 제공한다. 본 발명에 의하면, 모재와 코팅층의 밀착력 평가시 기준으로 삼을 수 있는 도금층의 스트레스를 보다 간단하고, 정밀하며, 재현성있게 측정할 수 있다.
Abstract:
PURPOSE: A torsion testing jig device for a smart card is provided to obtain a reliable flexibility testing result of a smart card because frequencies being applied to a fatigue test have a constant cycle and a rapid speed. CONSTITUTION: A torsion testing jig device for a smart card comprises a first fixing plate(23), a second fixing plate(24), a rotary jig(20a), a fixing jig(20b), a tilting link(25), and a lifting rod(26). The first and second fixing plates are installed in upper both sides of a base plate(10). The rotary jig forms a groove(22a) where a smart card can be fitted. The groove is installed in the first fixing plate to be rotated. The fixing jig forms a groove(22b) where the smart card can be fitted. The fixing jig installs the groove to be faced to the groove formed in the rotary jig. The tilting link rotates the rotary jig. One end part of the lifting rod is joined to the tilting link to be rotated. The other end part of the lifting rod is connected to a lifting bar of a smart tester.
Abstract:
PURPOSE: A method for manufacturing a printed circuit board including a minute wiring pattern with a high etching factor is provided to remove the residual stress of a copper layer by applying tension. CONSTITUTION: A first copper layer is formed on the upper side of an insulation substrate(S210). The first copper layer is processed(S220). The processed first copper layer is dried(S230). A via hole is formed in an insulation substrate by using a drill process(S240). A second copper layer is formed on the surface of the first copper layer and the via hole by using an electroless copper plating process(S250). The residual stress of the second copper layer is removed by applying tension to the second copper layer(S260). The second copper layer is homogenized. A minute wiring pattern is formed by etching the first copper layer and the second copper layer(S270).
Abstract:
본 발명의 탄소나노튜브 복합 솔더볼 제조방법은 용융솔더가 통과되는 홀이 형성된 용기에 용융솔더를 넣는 준비단계, 상기 용융솔더가 상기 홀을 통과하여 중력 방향으로 하강하며, 상기 용융솔더는 하강 도중 방울 형태를 이루는 하강단계, 분사기를 이용하여 탄소나노튜브 분무액을 상기 하강단계의 용융솔더에 분사하는 분사단계 및 상기 분사단계 이후 탄소나노튜브가 혼합된 방울 형태의 용융솔더가 냉각오일에 투입되어 응고되는 응고단계를 포함한다. 그리고 본 발명의 솔더페이스트 제조방법은 상기 방법에 의하여 제조된 솔더볼을 플럭스와 섞어 솔더페이스트를 제조한다.