公开(公告)号:KR1020150120788A
公开(公告)日:2015-10-28
申请号:KR1020140046905
申请日:2014-04-18
Applicant: 현대자동차주식회사
CPC classification number: F01L3/04
Abstract: 엔진용배기밸브가개시된다. 개시된엔진용배기밸브는엔진의연소실에서발생된배기가스를배출하기위한것으로서, 화염이접촉하는페이스부에폴리아마이드이미드수지및 폴리아마이드이미드수지에분산된에어로겔을포함하며 0.60W/m이하의열전도도를갖는단열코팅층이형성될수 있다.
Abstract translation: 公开了一种用于发动机的排气阀。 用于发动机的排气阀将排放在发动机的燃烧室中产生的废气。 用于发动机的排气阀可以具有绝缘涂层,其在与分散在聚酰胺酰亚胺树脂中的火焰和气凝胶接触的面部中包括聚酰胺酰亚胺树脂,并且具有等于或小于0.60W / m的导热性。
-
公开(公告)号:KR1020150080239A
公开(公告)日:2015-07-09
申请号:KR1020130168496
申请日:2013-12-31
Applicant: 현대자동차주식회사
IPC: C09D179/08 , C09D7/12 , C09D5/00
Abstract: 본발명은폴리아마이드이미드수지의용매분산체및 에어로겔의용매분산체를포함하는단열코팅조성물및 이로부터얻어지는단열코팅층에관한것이다.
Abstract translation: 本发明涉及包含聚酰胺 - 酰亚胺树脂的溶剂分散体和气凝胶的溶剂分散体的绝热涂料组合物以及由其获得的绝热涂层。
-
公开(公告)号:KR101534715B1
公开(公告)日:2015-07-08
申请号:KR1020130168491
申请日:2013-12-31
Applicant: 현대자동차주식회사
IPC: C09D7/12 , C09D5/00 , C09D201/00
CPC classification number: F02B77/11 , C08K5/5333 , C09D5/26 , C09D7/63 , C09D183/00 , C09D183/04 , Y10T428/249953 , C09D201/00 , C09D5/00
Abstract: 본발명은, 수계용매에분산된고분자수지, 에어로겔및 특정의작용기를포함하는중량평균분자량 200 내지 5,000의양친성화합물을포함하는단열코팅조성물및 이로부터얻어지는단열코팅층에관한것이다.
Abstract translation: 本发明涉及一种隔热涂料组合物,其包括分散在水性溶剂中的树脂,气凝胶和具有特定官能团和重均分子量为200-5000的两亲化合物,以及绝热涂层 层从同一层获得。
-
公开(公告)号:KR1020140077354A
公开(公告)日:2014-06-24
申请号:KR1020120146054
申请日:2012-12-14
Applicant: 현대자동차주식회사
CPC classification number: C23C14/0641 , C01B21/0602 , C01B21/0761 , H01J37/32082
Abstract: Introduced in the present invention are a TiAgN coating layer, a TiAgN coating method, and a TiAgN coating apparatus. The TiAgN coating layer is coated applied onto a base material having a surface roughness of 0.05-0.1 um by a plasma coating method, and is formed by periodically applying and stopping an Ag source under the state of maintaining nitrogen atmospheric gas and applying a Ti source. In the coating step, the Ti source and the Ag source are arranged to face each other across the base material. A jig for fixating the base material is coated while rotating in a velocity of 20-50 rpm. Moreover, in the coating step, the Ag source is applied and stopped in a period of 30-240 seconds.
Abstract translation: 在本发明中引入了TiAgN涂层,TiAgN涂覆法和TiAgN涂覆装置。 通过等离子体涂覆法将TiAgN涂层涂布在表面粗糙度为0.05〜0.1μm的基材上,并且在保持氮气气氛的状态下周期性地施加和停止Ag源而形成,并施加Ti源 。 在涂布步骤中,Ti源和Ag源布置成跨越基底材料彼此面对。 用于固定基材的夹具以20-50rpm的速度旋转涂覆。 此外,在涂布步骤中,Ag源在30-240秒的时间内施加和停止。
-
公开(公告)号:KR101382997B1
公开(公告)日:2014-04-08
申请号:KR1020120013022
申请日:2012-02-08
Applicant: 현대자동차주식회사
CPC classification number: C23C14/0641 , C23C14/024
Abstract: 본 발명은 코팅층 형성 공정상 공정 압력을 조절하여 표면 모폴로지 미세화 및 Ag 함량을 증가시켜 고온에서 표면 특성(저마찰 및 내마모 특성)을 향상시킬 수 있는 코팅층 표면 처리 방법을 제공하는데 그 목적이 있다.
상기한 목적을 달성하기 위해 본 발명에 따른 코팅층 표면 처리 방법은 피코팅재를 챔버 내에서 가열하는 히팅 단계; 상기 가열된 피코팅재의 표면에서 이물질을 제거하는 클리닝 단계; 상기 피코팅재의 표면에 버퍼층을 형성하는 단계; 상기 버퍼층 위에 코팅층을 형성하는 단계;를 포함하여 이루어지며, 상기 코팅층 형성 시 공정 압력을 조절하여 고온에서 표면 특성을 향상시킬 수 있도록 된 것을 특징으로 한다.-
公开(公告)号:KR1020130058323A
公开(公告)日:2013-06-04
申请号:KR1020110124270
申请日:2011-11-25
Applicant: 현대자동차주식회사
IPC: C23C14/34
CPC classification number: C23C14/0641 , C23C14/325 , C23C14/3492 , C23C14/58 , H01J37/32055 , H01J37/34 , H01J37/3497 , Y10T428/24372
Abstract: PURPOSE: A method for forming a low friction coating layer is provided to improve low frictional properties by forming Ag particles on an existing coating layer with controlling bias voltage and sputter power. CONSTITUTION: A method for forming a low frication coating layer comprises a coating step, a fraction increasing step, and a nanoparticle forming step. In the coating step, TiAgN coating layer is formed on the surface of a basic material using Ti arc sources and Ag sputtering sources. In the fraction increasing step, Ag fraction on the surface increases by boosting sputtering power and bias voltage for a certain period of time. In the nanoparticle forming step, Ag nanoparticles are formed on the surface by being maintained in a temperature rise section for a certain period of time. [Reference numerals] (AA) Gas (N); (BB) Arc ion source (Ti); (CC) Sputter ion source (Ag)
Abstract translation: 目的:提供一种形成低摩擦涂层的方法,以通过在具有控制偏压和溅射功率的现有涂层上形成Ag颗粒来改善低摩擦性能。 构成:形成低烧结涂层的方法包括涂布步骤,级分增加步骤和纳米颗粒形成步骤。 在涂覆步骤中,使用Ti电弧源和Ag溅射源在基材表面上形成TiAgN涂层。 在分数增加步骤中,表面上的Ag分数通过在一定时间段内提高溅射功率和偏压而增加。 在纳米颗粒形成步骤中,通过在温度上升部分保持一定时间而在表面上形成Ag纳米颗粒。 (附图标记)(AA)气体(N); (BB)电弧离子源(Ti); (CC)溅射离子源(Ag)
-
公开(公告)号:KR1020120059255A
公开(公告)日:2012-06-08
申请号:KR1020100120926
申请日:2010-11-30
Applicant: 현대자동차주식회사
CPC classification number: C23C14/3464 , C23C14/0036 , C23C14/0641 , C23C14/325
Abstract: PURPOSE: A multi-composition coating material and a coating method thereof are provided to obtain a high-temperature wear resistance and low friction property by doping silver in a coating material. CONSTITUTION: A coating method of a multi-composition coating material is as follows. A bias voltage is applied to an objected to be coated, and nitrogen gas(N2) is drawn in. Electricity of 50-200 A and 0.1-1.2 A is applied to an arc gun with a titanium target and a sputter gun with a silver target, respectively, for 10-60 minutes.
Abstract translation: 目的:提供多组分涂料及其涂布方法,以通过在涂料中掺杂银来获得高温耐磨性和低摩擦特性。 构成:多组分涂料的涂布方法如下。 将偏压施加到被涂覆的物体上,并且吸入氮气(N 2)。将50-200A和0.1-1.2A的电施加到具有钛靶的电弧枪和具有银的溅射枪 目标,分别为10-60分钟。
-
公开(公告)号:KR1020060017341A
公开(公告)日:2006-02-23
申请号:KR1020040065994
申请日:2004-08-20
Applicant: 현대자동차주식회사
Inventor: 여인웅
IPC: C09D5/46
Abstract: 본 발명은 저마찰특성이 우수한 용사코팅 실린더 블록용 세라믹 플라즈마 용사코팅제 조성물에 관한 것으로서, 더욱 상세하게는 산화물계 세라믹스를 주재로 하고 여기에 CaF
2 와 Mo를 함유시킴으로써 고온 및 저온에서 좋은 마찰 특성을 나타내며, 표면가공이 용이한 기공도와 높은 강도 및 내 마모특성을 가지는 용사코팅 실린더 블록용 세라믹 플라즈마 용사코팅제 조성물에 관한것이다.
저마찰특성, 플라즈마 용사코팅재, 세라믹-
公开(公告)号:KR101826558B1
公开(公告)日:2018-02-07
申请号:KR1020160013597
申请日:2016-02-03
Applicant: 현대자동차주식회사
CPC classification number: C09K5/10 , C01B32/15 , C01B32/198 , C01B32/28
Abstract: 본발명의일 실시예에의한산화그래핀-나노다이아몬드결합체는산화그래핀및 산화그래핀의표면에화학적으로결합한나노다이아몬드를포함한다.
-
-
-
-
-
-
-
-
-