公开(公告)号:KR1020130060544A
公开(公告)日:2013-06-10
申请号:KR1020110126658
申请日:2011-11-30
Applicant: 현대자동차주식회사 , 현대하이스코 주식회사
CPC classification number: C23C14/025 , C23C14/0021 , C23C14/0641 , C23C14/14 , C23C14/32 , C23C14/325 , C23C14/345 , C23C14/505 , C23C14/54 , C23C14/586 , C23C28/322 , C23C28/34 , C23C28/42 , C23F15/00
Abstract: PURPOSE: A nanomultilayer coating layer forming method and a forming device are provided to improve corrosion resistance and conductivity by controlling a crystal growth direction through the control of bias voltage in a coating process and to use metal including excellent conductivity for a minute tissue and a multilayer on a CrN coating layer. CONSTITUTION: A Mo coating layer is formed on base metal by using a Mo target and Ar gas of a steering device(S100). A nitride film is formed by using the Ar gas and N-2 gas of an arc ionic plating device(S200). A nano complex coating layer of the Cr-Mo-N is formed on the base metal by simultaneously using a Mo target and the Ar gas of the steering device and the Ar gas, and N-2 gas, a Cr source of the arc ionic plating device(S300). The base metal revolves around a rotary shaft, and a multilayer on which the nano complex coating layer of Cr-Mo-N and the Mo coating layer are repeated is coated(S400). [Reference numerals] (AA) Start; (BB) End; (S100) First coating step; (S200) Nitriding step; (S300) Second coating step; (S400) Multi coating step
Abstract translation: 目的:提供纳米多层涂覆层形成方法和成形装置,以通过在涂布工艺中控制偏压来控制晶体生长方向,并且使用包括优异导电性的金属用于微小组织和多层膜来提高耐腐蚀性和导电性 在CrN涂层上。 构成:通过使用转向装置的Mo靶和Ar气体在母材上形成Mo涂层(S100)。 通过使用电弧离子镀装置的Ar气体和N-2气体来形成氮化膜(S200)。 通过同时使用Mo靶和转向装置的Ar气体和Ar气体,以及N-2气体,电弧离子的Cr源,在基体金属上形成Cr-Mo-N的纳米复合涂层 电镀装置(S300)。 基体金属围绕旋转轴旋转,并且涂覆其上重复Cr-Mo-N和Mo涂层的纳米复合物涂层的多层(S400)。 (附图标记)(AA)开始; (BB)结束; (S100)第一涂布步骤; (S200)氮化步骤 (S300)第二涂布步骤; (S400)多涂层步骤
-
公开(公告)号:KR1020130057110A
公开(公告)日:2013-05-31
申请号:KR1020110122875
申请日:2011-11-23
Applicant: 현대자동차주식회사
Abstract: PURPOSE: An A1-CNT composite and a manufacturing method thereof are provided to secure elasticity equivalent to cast iron by enhancing elastic modulus to 120GPa. CONSTITUTION: An A1-CNT composite has CNT which is vertically stood up by a magnetic field effect and is embedded in an aluminum alloy. The surface of CNT is coated with metallic oxide. The surface of metallic oxide is coated with Fe-Co-Ni based metallic oxide and has enhanced elastic modulus. CNT is coated with metallic oxide and then is coated in FeSO4, CoSO4, NiSO4, H3Bo3 solutions in an electroless plating method. [Reference numerals] (AA) Metal oxide; (BB) Fe-Co-Ni based metal compound
Abstract translation: 目的:提供一种A1-CNT复合材料及其制造方法,以通过将弹性模量提高到120GPa来确保与铸铁相当的弹性。 构成:A1-CNT复合材料具有通过磁场效应垂直站立并嵌入铝合金的CNT。 CNT的表面涂有金属氧化物。 金属氧化物的表面涂覆有Fe-Co-Ni基金属氧化物,并具有增强的弹性模量。 CNT被金属氧化物涂覆,然后以化学镀方法涂覆在FeSO 4,CoSO 4,NiSO 4,H 3 BO 3溶液中。 (标号)(AA)金属氧化物; (BB)Fe-Co-Ni基金属化合物
-
公开(公告)号:KR101210118B1
公开(公告)日:2012-12-07
申请号:KR1020100120947
申请日:2010-11-30
Applicant: 현대자동차주식회사 , 현대하이스코 주식회사
Abstract: 본발명은다층박막의표면을가지는금형에관한것으로서, 기재와; 상기기재의상부면에코팅된 Mo 중간층과; 상기 Mo 중간층의상부면에코팅된 CrN-Mo 탑층을포함하는것을특징으로한다.이에의하여, 기재와 CrN-Mo 탑층사이에 Mo 중간층을형성함으로써, 종래 CrN 경질피막코팅막에비해구조안정성및 밀착력이향상될뿐만아니라내마모성이향상될수 있다.
-
公开(公告)号:KR1020000067500A
公开(公告)日:2000-11-25
申请号:KR1019990015364
申请日:1999-04-29
Applicant: 현대자동차주식회사 , 삼양화학산업 주식회사
Inventor: 강혁
IPC: C23C22/13
CPC classification number: C23C22/365 , C23C22/13
Abstract: PURPOSE: A surface treatment agent for basic painting capable of simultaneously treating aluminum alloy and steel plate is provided to continually surface treat aluminum steel. CONSTITUTION: A surface treatment agent for basic painting capable of simultaneously treating aluminum alloy and steel plate is composed by adding an auxiliary agent including fluorine compound to solution which is made by diluting undiluted solution of phosphate coating at 4 to 6 %. The undiluted solution of phosphate coating is composed of 25 to 40 weight % phosphoric acid, 5 to 15 weight % nitric acid, 0.1 to 1 weight % nitric iron, 1 to 5 weight % zinc, 0.5 to 1.5 weight % nickel, and 0.3 to 1 weight % manganese.
Abstract translation: 目的:提供一种能够同时处理铝合金和钢板的基础涂料表面处理剂,用于不断表面处理铝钢。 构成:用于同时处理铝合金和钢板的基础油漆表面处理剂是通过向溶液中加入含氟化合物的辅助剂组成的,该溶液是通过将未稀释的磷酸盐涂层溶液稀释至4至6%而制得的。 未稀释的磷酸盐涂层溶液由25至40重量%的磷酸,5至15重量%的硝酸,0.1至1重量%的硝酸铁,1至5重量%的锌,0.5至1.5重量%的镍和0.3至 1重量%锰。
-
公开(公告)号:KR2019980052063U
公开(公告)日:1998-10-07
申请号:KR2019960065242
申请日:1996-12-31
Applicant: 현대자동차주식회사
Inventor: 강혁
IPC: B60J3/00
CPC classification number: B60J3/0234 , B60J3/0256 , B60Y2200/10
Abstract: 본고안은선비저구동장치에관한것으로서, 선비저의이동을안내하는가이드레일과, 상기스프링에탄지된상태로가이드레일의내측으로결합되며, 사용자가누를수 있도록된 버튼과, 상기버튼을감싸고있으며, 버튼이눌려짐에따라연동되어가이드레일로부터이탈되는록킹부와, 상기록킹부의외주면에결합되어가이드레일에접촉된상태로선비저가고정되도록하는고무판으로구성된것을특징으로하어사용자가선비저를원하는위치로이동시킬수 있도록한 선비저구동장치에관한것이다.
Abstract translation: 纸张涉及的驱动装置的学者的内部,连接到所述导轨的内侧的弹性支撑的状态下与导轨用于引导学者运动我的,在弹簧,并围绕按钮包裹,该按钮使得用户可以按下, 与在根据从导轨释放的负荷按压互通的锁定部分,位置联接到锁定部分的外周面的用户haeo特征在于由橡胶板,使得固定在与导轨接触的学者成本所需的学者我 学者于所述驱动单元的要被移动到。
-
公开(公告)号:KR1019980040736A
公开(公告)日:1998-08-17
申请号:KR1019960059962
申请日:1996-11-29
Applicant: 현대자동차주식회사
Inventor: 강혁
IPC: G01P3/00
Abstract: 본 발명은 자동차용 스피드 센서의 로터에 관한 것으로, 스피드 센서용 로터의 몸체를 나이론과 같은 플라스틱 재질로 성형하는 동시에, 이 몸체의 외주면을 자성을 띄는 재질이 감싸는 형태가 되도록 일체로 성형함으로써, 스피드 센서의 로터 전체 무게를 경량화 시킬 수 있게 되어, 구동축의 받는 전체 토우크를 줄여서, 각 구성품들의 피로수명을 높일 수 있는 자동차용 스피드 센서의 로터를 제공하는데 있다.
-
-
公开(公告)号:KR101926881B1
公开(公告)日:2018-12-07
申请号:KR1020130166817
申请日:2013-12-30
Abstract: 스퍼터링기구와 아크이온플레이팅기구가 구비된 물리기상증착기를 이용한 코팅층 형성방법으로서, 모재에 스퍼터링기구의 Mo 타겟과 Ar 가스를 이용하여 Mo코팅층을 형성하는 제1코팅단계; 아크이온플레이팅기구의 Ar 가스 및 N
2 가스를 이용하여 질화물 박막 형성 분위기를 형성하는 질화단계; 모재에 스퍼터링기구의 Mo 타겟과 Ar 가스 및 아크이온플레이팅기구의 Ar 가스, N
2 가스 및 Cr 소스를 동시에 이용하여 Cr-Mo-N의 나노복합코팅층을 형성하는 제2코팅단계; 및 모재를 회전축을 중심으로 공전시킴으로써 Cr-Mo-N의 나노복합코팅층과 Mo코팅층이 반복되는 멀티레이어로 코팅하는 멀티코팅단계;를 포함하는 나노멀티레이어 코팅층 그 형성방법 및 형성장치가 소개된다.-
公开(公告)号:KR1020150069192A
公开(公告)日:2015-06-23
申请号:KR1020130155318
申请日:2013-12-13
Applicant: 현대자동차주식회사
CPC classification number: C23C14/0641 , C23C14/024 , C23C14/3464 , C23C14/548 , C23C14/5806
Abstract: Ti소스, Mo소스, Ag소스및 질소, 아르곤분위기가스를이용하여플라즈마코팅하는 TiAgMoN 코팅층형성방법으로서, 코팅챔버를진공처리하는진공단계; 및챔버내에아르곤가스와질소가스를투입하고 Ti소스, Mo소스및 Ag소스에각각전원을인가하여모재의표면에 TiAgMoN 코팅층을형성하되, 코팅층에서 Mo의비율이 10~13 at%가되도록 Mo소스의파워를제어하는코팅단계;를포함하는 TiAgMoN 코팅층형성방법이소개된다.
Abstract translation: 提供了使用Ti源,Mo源,Ag源,氮环境气体和氩气环境气体形成TiAgMoN涂层等离子体涂层的方法。 本发明包括:用于真空处理涂布室的真空步骤; 以及将氩气和氮气放入室中并向每个Ti源,Mo源和Ag源施加电力以在基材表面上形成TiAgMoN涂层并将Mo源的功率控制到 使涂层中Mo的比率为10〜13原子%。
-
公开(公告)号:KR101491217B1
公开(公告)日:2015-02-06
申请号:KR1020120145789
申请日:2012-12-13
Applicant: 현대자동차주식회사
CPC classification number: B32B15/01 , C23C4/10 , C23C14/0021 , C23C14/0641 , Y10T428/12806
Abstract: 질소가스, Ti소스 및 Ag소스를 이용한 플라즈마 코팅방식에 의해 코팅되며, 코팅층내 Ag의 함량이 15 at% 이상인 것을 특징으로 하는 TiAgN 코팅층, 코팅방법 및 코팅장비가 소개된다.
-
-
-
-
-
-
-
-
-