公开(公告)号:DE3605573A1
公开(公告)日:1987-08-27
申请号:DE3605573
申请日:1986-02-21
Applicant: BASF AG
Inventor: LAUSBERG DIETRICH DR , REIMANN HORST DR
Abstract: Thermoplastic molding materials based on (A) nylons and (B) polycarbonates, and containing 0.1-30% by weight of (C) a polymer containing hydroxyl groups, -OH. The molding materials have good surface characteristics and high impact strength, especially at low temperatures.
-
公开(公告)号:DE19752037A1
公开(公告)日:1999-05-27
申请号:DE19752037
申请日:1997-11-24
Applicant: BASF AG
Inventor: GUETTES BERND , HINZ WERNER DR , LAUSBERG DIETRICH DR , ROTERMUND UDO DR
Abstract: Polyurethanes (PUR) are obtained by reacting (a) polyfunctional isocyanates (optionally in presence of blowing agents and normal additives etc.) with (b) special isocyanate-reactive compounds comprising polyether-alcohols with a single functionality of n \! 0.1, where n = 3-9. An Independent claim is also included for the production of rigid PUR foam by the process described above with blowing agents (c) as an obligatory component.
-
公开(公告)号:AT109181T
公开(公告)日:1994-08-15
申请号:AT90103744
申请日:1990-02-26
Applicant: BASF AG
Inventor: LAUSBERG DIETRICH DR , BRAUN HANS-GEORG DR , STREU JOACHIM DR , FAEHNDRICH KNUD
-
公开(公告)号:DE58907589D1
公开(公告)日:1994-06-09
申请号:DE58907589
申请日:1989-02-09
Applicant: BASF AG
-
公开(公告)号:DE4022741A1
公开(公告)日:1992-01-23
申请号:DE4022741
申请日:1990-07-18
Applicant: BASF AG
Inventor: ZEITLER GERHARD DR , LEHR GERHARD , LAUSBERG DIETRICH DR
Abstract: Multilayer polyurethane film (I) is claimed, in which at least 2 of the layers consist of thermoplastic PU (TPU) with different Shore hardness. Pref. (I) is double-layer film with layers of different Shore hardness. At least one layer (1) is TPU with Shore A hardness (SAH) = 60-98 and at least one layer (2) is TPU with Shore D hardness (SDH) = 50-74, pref. based on polyether-polyol and polyester-polyol, respectively, and pref. forming the upper or patterned layer (1) and the lower layer (2). (I) is 0.2-2.5 mm thick, and the separate layers are 01.-2.4 mm thick, opt. the film material can be a thermoplastic moulding material contg. at last 50 wt.% TPU and up to 50 wt.% ABS copolymer, As copolymer, styrene copolymer modified with acrylate rubber, polyester, polycarbonate, polyamide, or a mixt. of at least 2 of these plastics; (I) is produced by coextrusion. USE/ADVANTAGE - (I) is useful for the prodn. of covering layers by thermoforming (claimed). Cost-effective process for the prodn. of (I). The film has good thermal and light stability, and can be backed with PU foam without undesirable interactions, or thermoformed over a wide temp. range, e.g. to produce "mould skins" for automobile dashboards, glove boxes, etc.
-
公开(公告)号:DE4016297A1
公开(公告)日:1991-11-28
申请号:DE4016297
申请日:1990-05-21
Applicant: BASF AG
Inventor: TREMMEL GREGOR , DEIMLING AXEL DR , UHR HERMANN , AECKERLE ECKHARD , NIKLES ALBERT , LAUSBERG DIETRICH DR
IPC: C02F1/26
-
公开(公告)号:DE4005818A1
公开(公告)日:1991-08-29
申请号:DE4005818
申请日:1990-02-23
Applicant: BASF AG
Inventor: LAUSBERG DIETRICH DR , MUEHLBACH KLAUS DR , BLUMENSTEIN UWE DR , FAEHNDRICH KNUD
Abstract: The invention relates to thermoplastic moulding compositions of improved green strength and low-temperature impact strength based on a TPU copolymer mixture and containing, based on 100 parts by weight, A) from 20 to 90 parts by weight of at least one thermoplastic polyurethane, B) from 1 to 40 parts by weight of at least one rubber-elastic graft copolymer built up from B1) a graft base comprising a rubber-elastic polymer having a glass transition temperature of below -20 DEG C based on butadiene or C1-C10-acrylates, and optionally a crosslinking agent, and B2) a graft shell prepared by one-step or multistep copolymerisation of styrene, alpha -methylstyrene, acrylonitrile, methacrylonitrile and methyl methacrylate or mixtures of at least two of said monomers, C) from 5 to 75 parts by weight of at least one copolymer of C1) from 55 to 90% by weight of alpha -methylstyrene and C2) from 10 to 45% by weight of acrylonitrile or methacrylonitrile or mixtures thereof, D) from 0.1 to 5 parts by weight of at least one copolymer of D1) from 60 to 99% by weight of styrene and D2) from 1 to 40% by weight of at least one olefinically unsaturated monomer containing at least one carboxyl, anhydride, tert-butyl ester, hydroxyl or amino group, and E) from 0 to 60 parts by weight of at least one reinforcing filler. The moulding compositions can be prepared by melting together the starting components and are preferably used for the production of injection mouldings.
-
公开(公告)号:DE3932360A1
公开(公告)日:1991-04-11
申请号:DE3932360
申请日:1989-09-28
Applicant: BASF AG
Inventor: LAUSBERG DIETRICH DR , STEINBERGER ROLF DR
-
公开(公告)号:DE3766912D1
公开(公告)日:1991-02-07
申请号:DE3766912
申请日:1987-08-08
Applicant: BASF AG
Inventor: LAUSBERG DIETRICH DR , MCKEE GRAHAM EDMUND DR , TAUBITZ CHRISTOF DR , WASSMUTH GEORG DR , KNOLL MANFRED
Abstract: Thermoplastic molding materials contain, as essential components, (A) from 10 to 89.99% by weight of a polyester, (B) from 10 to 89.99% by weight of a polycarbonate and (C1) from 0.01 to 1% by weight of a low molecular weight organic compound of not more than 70 carbon atoms which contains (-SO3)mQ groups where Q is hydrogen, NH4 or an alkali or alkaline earth metal and m is an integer equal to the valency of Q, and/or (C2) from 0.01 to 30% by weight of a polymer containing sulfo groups and having a weight average molecular weight of not less than 1000, and, as a further component, (D) from 0 to 30% by weight of a rubber impact modifier.
-
公开(公告)号:DE3834085A1
公开(公告)日:1990-04-12
申请号:DE3834085
申请日:1988-10-07
Applicant: BASF AG
Inventor: TAUBITZ CHRISTOF DR , LAUSBERG DIETRICH DR , BRANDT HERMANN DR
Abstract: Thermoplastic moulding compositions based on A) polyesters and B) polyphenylene ethers, characterised by a content of C) from 0.1 to 40% by weight, based on the sum of A, B and C, of a copolymer comprising c1) from 40 to 99.9 mol % of a vinylaromatic monomer, c2) from 0.1 to 60 mol % of a compound of the formula (I) wherein R is -OH, alkoxy, aryloxy, aralkoxy or alkylaryloxy having up to 25 carbon atoms or, together with R is -NR -, R is -H or, if R is -H, is alkyl, aryl, aralkyl or alkaryl having up to 25 carbon atoms or chlorine, R is -H or, if R is -H, is alkyl, aryl, aralkyl or alkaryl having up to 25 carbon atoms or chlorine, R is alkoxy, aryloxy, aralkoxy or alkylaryloxy having up to 25 carbon atoms or, together with R , is -NR -, and R is hydrogen or an alkyl, cycloalkyl, aralkyl or aryl group having up to 12 carbon atoms which itself may be substituted by C1-C4-alkyl or -alkoxy groups, and c3) from 0 to 20 mol % of further copolymerisable monomers, and the preparation and use thereof.k
-
-
-
-
-
-
-
-
-