ROPE COMPRISING CARBON FIBER-REINFORCED COMPOSITE MATERIAL AND PRODUCTION THEREOF

    公开(公告)号:JPH0533278A

    公开(公告)日:1993-02-09

    申请号:JP17946091

    申请日:1991-07-19

    Abstract: PURPOSE:To produce the subject rope useful for building materials, construction materials and having light weight, excellent shape retainability and good workability by twisting plural carbon fiber-reinforced composite materials impregnated with a thermoplastic resin so as to specify the content of the fibers. CONSTITUTION:Plural carbon fiber-reinforced composite materials each having a diameter of 1-5mm and produced by impregnating a carbon fiber bundle with a thermoplastic resin (preferably nylon) so as to give a fiber content of 40-70wt.% are twisted and subsequently subjected to a thermal treatment [at a temperature of the melting point -(5 to 20 deg.C)] to provide the objective rope.

    ACRYLIC FIBER FOR GRAPHITE FIBERS
    37.
    发明专利

    公开(公告)号:JPH02264011A

    公开(公告)日:1990-10-26

    申请号:JP8518389

    申请日:1989-04-03

    Abstract: PURPOSE:To obtain the title fibers giving graphite fibers of super-high elastic modulus by using a polymer containing acrylonitrile, a composition for accelerating pre-oxidation and boron containing vinyl compound at specified ratio. CONSTITUTION:The subject fibers are composed of (A) more than 85wt.%, preferably more than 90wt.% of acrylonitrile, (B) 0.1 to 4wt.%, preferably 0.3 to 1wt.% of a component for accelerating predeoxidation, for example, a vinyl monomer such as (meth)acrylic acid or itaconic acid, and (C) 0.05 to 3wt.%, preferably 0.3 to 1wt.% (based on boron) of a boron containing vinyl compound such as vinyl di-n-butoxyborane, isopropenyl di-n-butoxyborane).

    PRODUCTION OF CARBON FIBER
    38.
    发明专利

    公开(公告)号:JPH02242921A

    公开(公告)日:1990-09-27

    申请号:JP6454289

    申请日:1989-03-15

    Abstract: PURPOSE:To efficiently obtain a high quality and high performance carbon fiber in a short time by heat treatment of a precursor for carbon fiber production composed of a specific acryl-based copolymer in a fluid bed for disperse means. CONSTITUTION:A precursor for carbon fiber production composed of a copolymer of >=85% acrylonitrile and 1 to 10%, preferably 3 to 8% alkyl ester [preferably propyl ester of (meth)acrylic acid, etc.] of polymerizable unsaturated carboxylic acid is subjected to heat treatment in a fluid bed (preferably being means for subjecting solid heat mediated granules to heat treatment in a fluidized state with a gas and wherein fluidized state of the solid heat mediated granules with an oxidizing gas and heated state at >=240 deg.C coexist in the fluid bed) to provide the objective fiber.

    PRODUCTION OF IMPROVED GRAPHITE FIBER

    公开(公告)号:JPH0247309A

    公开(公告)日:1990-02-16

    申请号:JP19424188

    申请日:1988-08-03

    Abstract: PURPOSE:To prevent the formation of the crystals of metal carbide and nitride, etc., and elongate the life of an oven tube in a graphitization oven by charging an inert gas and carbon tetrachloride in the graphitization oven and graphitizing a carbon fiber at a high temperature in the oven. CONSTITUTION:An inert gas (e.g., nitrogen gas) and carbon tetrachloride are charged in a graphitization oven and a carbon fiber is subjected to a graphitization treatment at the highest heat treatment temperature of >=2000 deg.C to provide the objective fiber. The amount of the charged carbon tetrachloride is preferably 0.13-14.0g per kg of the carbon fiber. The concentration of the carbon tetrachloride in the mixed gases is preferably