41.
    发明专利
    未知

    公开(公告)号:PT927212E

    公开(公告)日:2000-12-29

    申请号:PT97943850

    申请日:1997-09-19

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP97/04908 Sec. 371 Date Mar. 17, 1999 Sec. 102(e) Date Mar. 17, 1999 PCT Filed Sep. 19, 1997 PCT Pub. No. WO98/12242 PCT Pub. Date Mar. 20, 1998Biodegradable polyesters based on A) 95-99.99 mol % of at least one polyester A containing as monomeric building blocks of an acid component comprising a11) 20-95 mol % of at least one aliphatic or cycloaliphatic dicarboxylic acid or its ester-forming derivative and a12) 5-80 mol % of at least one aromatic dicarboxylic acid or its ester-forming derivative and at least one dihydroxy compound or at least one amino alcohol or their mixtures, and B) 0.01-5 mol % of a mixture comprising mono-, bi-, tri-, tetra- and higher-nuclear isocyanurates or corresponding compounds containing two, three or four functional groups capable of reacting with the end groups of polyester A, or mixtures of the isocyanurates and the corresponding compounds, as well as molding compositions comprising said polyesters, their manufacture and their use in the manufacture of moldings, filsm, fibers and coatings.

    42.
    发明专利
    未知

    公开(公告)号:ES2147918T3

    公开(公告)日:2000-10-01

    申请号:ES96903976

    申请日:1996-02-03

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP96/00457 Sec. 371 Date Aug. 14, 1997 Sec. 102(e) Date Aug. 14, 1997 PCT Filed Mar. 5, 1996 PCT Pub. No. WO96/25446 PCT Pub. Date Aug. 22, 1996Biodegradable polyesters having a molecular weight (Mn) of from 5000 to 50,000 g/mol (measured by gel permeation chromatography), a viscosity number of from 30 to 350 g/ml (measured in 50:50 by weight of o-dichlorobenzene/phenol at a concentration of 0.5% by weight of polyester at 25 DEG C.), and a melting point of from 50 to 170 DEG C., and having both hydroxyl and carboxyl end groups, the molar ratio of carboxyl end groups to hydroxyl end groups being greater than one, which is obtained by reacting a mixture consisting essentially of a1) a mixture consisting essentially of from 45 to 80 mol % of adipic acid or ester-forming derivatives thereof, or mixtures thereof, from 20 to 55 mol % of terephthalic acid or ester-forming derivatives thereof, or mixtures thereof, and from 0 to 5 mol % of a sulfonate compound, where the sum of the individual mole percentages is 100 mol %, and a2) a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, in the presence of from 0.01 to 5 mol %, per mol of component a1), of a compound D having at least three groups capable of ester formation, the molar ratio of a1) to a2) being from 0.4:1 to 1.5:1, polymers and biodegradable thermoplastic molding compositions, processes for their preparation and their use for producing biodegradable moldings, adhesives, foams and blends with starch obtained from the polymers or molding compositions.

    43.
    发明专利
    未知

    公开(公告)号:DE19800020A1

    公开(公告)日:1999-07-08

    申请号:DE19800020

    申请日:1998-01-05

    Applicant: BASF AG

    Abstract: Continuous gas phase polymerization for producing ethylene homopolymers and -copolymers, comprises polymerizing ethylene or monoolefin from but-1-en, pent-1-en, 2-methylpentene, hex-1-en, hept-1-en and oct-1-en in the a polymerization reactor; and endowing a catalyst poison with boiling point higher than a circle gas pipeline, and molecular weight greater than 100 g/mol at a position after the reactor, but before the cooler and compressor. Continuous gas phase polymerization for producing ethylene homopolymers and -copolymers, comprises polymerizing ethylene and/or monoolefin from but-1-en, pent-1-en, 2-methylpentene, hex-1-en, hept-1-en or oct-1-en, in the polymerization zone of a gas phase polymerization reactor at 30-125[deg]C and 1-100 bar in the gaseous phase in a finely divided polymer bed, in the presence of a metallocene catalyst in carrier form polymer, where a reactor gas is lead into the circle gas pipeline for the removal of the polymerization heat; and endowing a catalyst poison with boiling point higher than circle gas pipeline and molecular weight greater than 100 g/mol at a position after the reactor but before the cooler and compressor, for preventing polymer linings, such that the productivity of the catalyst is not essentially affected in the reactor.

    44.
    发明专利
    未知

    公开(公告)号:DK0809666T3

    公开(公告)日:1999-06-28

    申请号:DK96902980

    申请日:1996-02-03

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP96/00458 Sec. 371 Date Aug. 14, 1997 Sec. 102(e) Date Aug. 14, 1997 PCT Filed Feb. 3, 1996 PCT Pub. No. WO96/25448 PCT Pub. Date Aug. 22, 1996Biodegradable polymers comprising a polyether ester P1 obtained by reacting a first mixture of 20-95 mol% of adipic acid or ester-forming derivatives thereof or mixtures thereof, 5-80 mol% of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and 0-5 mol% of a compound containing sulfonate groups, and a second mixture of 15-99.8 mol% of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols, 85-0.2 mol% of a dihydroxy compound IHO-[(CH2)n-O]m-H(n=2, 3 or 4, m=2-250) with 0-5 mol%, based on the first mixture, of a compound D having at least three groups capable of ester formation, and a bisoxazoline C1, their preparation and their use in the manufacture of biodegradable molding materials.

    45.
    发明专利
    未知

    公开(公告)号:DE19723003A1

    公开(公告)日:1998-12-03

    申请号:DE19723003

    申请日:1997-06-02

    Applicant: BASF AG

    Abstract: The invention relates to polymer mixtures containing at least 85 wt pct ethylene/ alpha -olefin copolymers (A) produced by metallocene catalysis and 1 to 15 wt pct essentially linear ethylene/ alpha -olefin copolymers (B) produced with a different catalyst, in relation to the total mass of the polymer mixture.

    46.
    发明专利
    未知

    公开(公告)号:DE59600363D1

    公开(公告)日:1998-08-27

    申请号:DE59600363

    申请日:1996-01-08

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP96/00067 Sec. 371 Date Jul. 3, 1997 Sec. 102(e) Date Jul. 3, 1997 PCT Filed Jan. 8, 1996 PCT Pub. No. WO96/21692 PCT Pub. Date Jul. 18, 1996Biodegradable polyesteramides as defined in the specification obtained by reacting a mixture consisting essentially of (a1) from 95 to 99.9% by weight of a polyesteramide, (a2) from 0.1 to 5% by weight of a divinyl ether, and (a3) from 0 to 5 mol % of compound D as defined in the specification, and other biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings, and adhesives, biodegradable moldings obtained from the polymers and molding compositions according to the invention.

    BIOLOGICALLY DEGRADABLE POLYMERS, PROCESS OF THEIR PREPARATION AND THEIR USE FOR PREPARING BIOLOGICALLY DEGRADABLE SHAPED BODIES

    公开(公告)号:CZ143797A3

    公开(公告)日:1997-11-12

    申请号:CZ143797

    申请日:1995-06-27

    Applicant: BASF AG

    Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd

    BIOLOGICALLY DEGRADABLE POLYMERS, PROCESSES OF THEIR PREPARATION AS WELL AS THEIR USE FOR PRODUCING BIOLOGICALLY DEGRADABLE SHAPED ARTICLES

    公开(公告)号:CZ146597A3

    公开(公告)日:1997-10-15

    申请号:CZ146597

    申请日:1995-06-27

    Applicant: BASF AG

    Abstract: Biodegradable polyether esters P1 obtainable by reacting a mixture essentially comprising(a1) a mixture essentially comprising20-95 mol % of adipic acid or ester-forming derivatives thereof or mixtures thereof,5-80 mol % of terephthalic acid or ester-forming derivatives thereof or mixtures thereof, and0-5 mol % of a compound containing sulfonate groups,where the total of the individual mole percentages is 100 mol %, and(a2) a mixture of dihydroxy compounds essentially comprising(a21) from 15 to 99.8 mol % of a dihydroxy compound selected from the group consisting of C2-C6-alkanediols and C5-C10-cycloalkanediols,(a22) from 85 to 0.2 mol % of a dihydroxy compound containing ether functionalities of the formula Iwhere n is 2, 3 or 4 and m is an integer from 2 to 250, or mixtures thereof,where the molar ratio of (a1) to (a2) is chosen in the range from 0.4:1 to 1.5:1, with the proviso that the polyether ester P1 has a molecular weight (Mn) in the range from 5000 to 80,000 g/mol, a viscosity number in the range from 30 to 450 g/ml (measured in o-dichlorobenzene/phenol (50/50 ratio by weight) at a concentration of 0.5% by weight of polyether ester P1 at 25° C.) and a melting point in the range from 50 to 200° C., and with the further proviso that from 0.01 to 5 mol %, based on the molar quantity of component (a1) employed, of a compound D with at least three groups capable of ester formation are employed to prepare the polyether ester P1,and further biodegradable polymers and thermoplastic molding compositions, processes for the preparation thereof, the use thereof for producing biodegradable moldings and adhesives, biodegradable moldings, films and blends with starch obtainable from the polymers and molding compositions according to the invention.

    50.
    发明专利
    未知

    公开(公告)号:BR9509685A

    公开(公告)日:1997-09-16

    申请号:BR9509685

    申请日:1995-06-27

    Applicant: BASF AG

    Abstract: The following are claimed: (A) biodegradable polyester P1, preparable by reaction of a mixt. comprising: (a1) a mixt. comprising: (a11) 35-95 mol.% of adipic acid and/or one or more ester-forming derivs. of this, (a12) 5-65 mol.% of terephthalic acid and/or one or more ester-forming derivs. of this, and (a13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (a11)-(a13) being 100 mol.%; and (a2) a dihydroxy cpd. selected from 2-6C alkane-diols and 5-10C cycloalkane-diols. The molar ratio of (a1) to (a2) is 0.4-1.5:1. In addn., 0.01-5 mol.% (based on the molar amt. of component (a1)) of a cpd. D, which comprises at least three gps. capable of forming ester gps., are also used for prodn. of polyester P1. Polyester P1 has (a) a mol.wt. (Mn) of 5000-50000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (B) biodegradable polyester P2, preparable by reaction of a mixt. comprising: (b1) mixt. comprising: (b11) 20-95 mol.% of adipic acid and/or one or more ester-forming deriv. of this, (b12) 5-80 mol.% of terephthalic acid and/or one or more ester- forming deriv. of this, and (b13) 0-5 mol.% of a cpd. contg. sulphonate gps., the total of mol.% in (b11)-(b13) being 100 mol.%; (b2) a dihydroxy cpd. as (a2) above; (b3) 0.01-100 wt.% (based on the amt. of component (b1) of a hydroxycarboxylic acid B1 which is of formula (Ia) or (Ib); and (b4) 0-5 mol.% (based on the amt. of component (b1)) of a cpd. D. The molar ratio of (b1) to (b2) is 0.4-1.25:1. Polyester P2 has (a) a mol.wt. (Mn) of 5000-80000 g/mol; (b) a viscosity no. of 30 - 450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a P2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. p = a whole no. from 1-1500; r = a whole no. from 1-4; G = phenylene, (CH2)k, C(R)H and C(R)HCH2; k = 1-5; R = Me or Et. (C) biodegradable polyester Q1 which have: (a) a mol.wt. (Mn) of 5000-100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. Q1 are obtained by reaction of a mixt. comprising; (c1) polyester P1 and/or a polyester PWD; (c2) 0.01-50 wt.% (based on (c1)) of a hydroxycarboxylic acid B1; and (c3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. Polyester PWD is obtainable by reaction of components (a1) and (a2) in a molar ratio of (a1) to (a2) of 0.4-1.5:1. Polyester PWD have: (a) a mol.wt. (Mn) of 5000 - 50000 g/mol; (b) a viscosity no. of 30 - 350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a PWD concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. (D) biodegradable polyesters Q2 which have: (a) a mol.wt. (Mn) of 6000 - 60000 g/mol; (b) a viscosity no. of 30-350 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a Q2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-170 degrees C. Q2 are obtained by reaction of a mixt. comprising: (d1) 95-99.9 wt.% of polyester P1 and/or PWD; and (d2) 0.1-50 wt.% of a diisocyanate C1; and (d3) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of P1 and/or PWD) of a cpd. D. (E) biodegradable polymers T1 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol; (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T1 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T1 are obtd. by reaction of polyester Q1 with (e1) 0.1-5 wt.% (based on the amt. of Q1) of diisocyanate C1 and (e2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q1 via the polyester P1 and/or PWD) of a cpd. D. (F) biodegradable polymers T2 which have: (a) a mol.wt. (Mn) of 10000 - 100000 g/mol/. (b) a viscosity no. of 30-450 g/ml (measured in o-dichlorobenzene/phenol (wt. ratio 50/50) at 25 degrees C and a T2 concn. of 0.5 wt.%); and (c) a m.pt. of 50-235 degrees C. T2 are obtained by reaction of polyester Q2 with (f1) 0.01-50 wt.% (based on the amt. of Q2) of hydroxycarboxylic acid B1 and (f2) 0-5 mol.% (based on the amt. of component (a1) used in prodn. of Q2 via the polyester P1 and/or PWD) of a cpd