Abstract:
PURPOSE: Conductive paste for an inner electrode and a multi-layer ceramic electronic component therewith are provided to form an inner electrode having excellent electrical properties using a conductive paste solvent. CONSTITUTION: Conductive paste for an inner electrode comprises conductive metal powder, organic binder, and a solvent. The organic binder comprises one or more of acryl-based resin, butyral-based resin, and cellulose-based resin. The solvent comprises eucalyptol and dihydroxy terephthalic acid.
Abstract:
A binder resin for a multi layer ceramic condenser internal electrode paste and a method for preparing the binder resin and an internal electrode paste are provided to reduce use of compound-type additives by using a binder. A method for preparing a binder resin and an internal electrode paste includes the steps of: heating Maleic acid anhydride and Hexanediol compound for 30min to 1hr at 100 to 300 degrees centigrade; manufacturing hydroxy-end polyester-type oligomer by heating and distilling for 30 minutes to 1 hour in nitride atmosphere; manufacturing isocyanate-end polyester-type oligomer by heating phenyl isocyanate and diphenyl-methane isocyanate compound with the hydroxy-end polyester-type oligomer at 60 to 100 degrees centigrade for 2 to 5 hours; and grafting ethyl-cellulose polyester-type oligomer by dissolving isocyanate-end polyester-type oligomer with ethyl-cellulose in solvent.
Abstract:
초고용량 적층 세라믹 콘덴서 제조시 내부전극 형성에 사용되는 표면조도, 건조막밀도 및 분산성이 우수한 내부전극용 금속 페이스트 제조방법에 관한 것이다. 금속 파우더와 금속 파우더 100중량부당, 터피네올 및/또는 석유계 용매 100-300중량부 및 분산제 0-1.5중량부를 예비혼합하고 저점도 분산하는 단계; 세라믹 공재(共材)와 세라믹 공재 100중량부당, 터피네올 및/또는 석유계 용매 100-300중량부 및 포스페이트 에스테르 분산제 0-1.5중량부를 예비혼합하고 저점도 분산하는 단계; 금속분산물과 세라믹 공재(共材) 분산물을 금속 파우더 100중량부당 세라믹 공재 10-30중량부가 되도록 혼합 및 분산하는 단계; 필터링하여 상기 용매를 제거하는 단계; 금속 파우더 100중량부당 에틸 셀룰로스 수지 4-8중량부 및 터피네올 용매 70-80중량부가 되도록 에틸 셀룰로스 수지 및 터피네올 용매를 첨가 및 혼합하는 단계; 점도조절 및 진공 탈포(脫泡)하는 단계; 및 카트리지 필터링하는 단계를 포함하는 내부전극용 금속 페이스트 제조방법이 제공된다. 본 발명의 방법으로 제조된 내부전극용 금속 페이스트는 분산성이 개선되며, 우수한 표면조도, 건조막 밀도 및 소성 수축율을 나타낸다. 금속 파우더, 세라믹 공재, 내부전극, 금속 페이스트, 고분산
Abstract:
본 발명은 내환원성 유전체 자기조성물과 이를 이용한 적층세라믹 커패시터에 관한 것이다. 본 발명의 적층세라믹 커패시터는 비유전율이 높으면서도 X5R특성(-55∼85 ℃, △C=±15% 이내)을 만족하고, 1200~1250℃ 의 저온소성으로 얻을 수 있다. 본 발명은, BaTiO 3 와, 이 BaTiO 3 100몰에 대해, MgCO 3 :0.2∼3.0몰, Y 2 O 3 , Ho 2 O 3 , Dy 2 O 3 , Yb 2 O 3 의 그룹에서 선택된 1종이상:0.05∼1.5몰, Cr 2 O 3 :0.1∼1.5몰, Ba x Ca (1-x) SiO 3 (단, 0 ≤x ≤1):0.2∼3.0몰, Mn 2 V 2 O 7 :0.01∼1.5몰을 포함하여 이루어지는 내환원성 저온소성 유전체 자기조성물과, 상기 유전체 자기조성물로 이루어진 유전체와 내부전극이 교대로 적층하여 이루어지는 적층세라믹 커패시터 및, MnO와 V 2 O 5 를 650~800℃ 에서 하소하여 Mn 2 V 2 O 7 분말을 얻는 단계, BaTiO 3 와 이 BaTiO 3 100몰에 대해 MgCO 3 :0.2∼3.0몰, Y 2 O 3 , Ho 2 O 3 , Dy 2 O 3 , Yb 2 O 3 의 그룹에서 선택된 1종이상:0.05∼1.5몰, Cr 2 O 3 :0.1∼1.5몰, Ba x Ca (1-x) SiO 3 (단, 0≤ x≤ 1):0.2∼3.0몰 및, 상기에서 얻은 Mn 2 V 2 O 7 을 0.01∼1.5몰로 혼합하여 유전재료를 얻는 단계, 상기 유전재료와 내부전극을 교대로 적층한 후 소성하는 단계를 포함하여 이루어지는 적층세라믹 커패시터의 제조방법에 관한 것을 그 기술요지로 한다.
Abstract:
PURPOSE: A magnetic composition of a low-temperature-fired dielectric and a laminated ceramic capacitor are provided to reduce the thickness of the dielectric by performing a low temperature firing process without lowering a dielectric constant. CONSTITUTION: A magnetic composition of a low-temperature-fired dielectric is formed with aBaTiO3-bMgCO3-cY2O3-dCr2O3-eV2O5-f(xZrO2-y(Kali)2O-zSiO2) under the condition such as x+y+z=1, 0.05
Abstract translation:目的:提供低温烧制电介质和层压陶瓷电容器的磁性组合物,通过在不降低介电常数的情况下进行低温烧制工艺来减小电介质的厚度。 构成:在诸如x + y + z = 1的条件下,用BaTiO3-bMgCO3-cY2O3-dCr2O3-eV2O5-f(xZrO2-y(Kali)2O-zSiO2)形成低温烧结电介质的磁性组合物 ,0.05 <= x <=0.18,0.01≤y≤0.08,0.74≤z≤0.93。 低温烧结电介质的磁性组成的摩尔比为a = 100,1.0 <= b <= 2.0,0.2 <= c <= 2.0,0.02 <= d <= 0.3,0.02 <= e < 0.3和0.5 <= f <2。 BaTiO3的平均晶粒尺寸小于0.4微米。 (xZrO2-y(K,Li)2O-zSiO2)的平均粒径小于0.5微米。
Abstract:
PURPOSE: A piezo transformer driving circuit is provided to improve driving efficiency of a piezo transformer by decreasing boost rate of voltage applied to an input terminal of the piezo transformer. CONSTITUTION: A piezo transformer driving circuit comprises: first and second switching devices (Q1,Q2), connected to an input power (Vin) in parallel as well as in serial, oprating on/off; an oscillating device (OSC) supplying opposite pulse signals to the first and the second switching device (Q1,Q2); and an inductor (L) connected between a common contact point of the first and the second switching means (Q1,Q2) and an input terminal of a piezo transformer (PT). The piezo transformer driving circuit is provided to improve efficiency by decreasing boost rate of the input voltage, and to make product miniaturized and product price decreased by changing currents of the inductor on both sides so as to reduce current capacity.