과산화수소를 이용한 산화물 박막 형성 방법 및 산화물 박막 트랜지스터 제조 방법
    61.
    发明授权
    과산화수소를 이용한 산화물 박막 형성 방법 및 산화물 박막 트랜지스터 제조 방법 有权
    用于形成氧化膜的方法和用于制造使用过氧化氢的氧化物薄膜晶体管的方法

    公开(公告)号:KR101433857B1

    公开(公告)日:2014-08-26

    申请号:KR1020130079125

    申请日:2013-07-05

    Inventor: 김현재 권정무

    Abstract: The present invention relates to a method of forming an oxide thin film and a method of manufacturing an oxide thin film using hydrogen peroxide. The method of forming an oxide thin film according to an embodiment comprises a step of mixing hydrogen peroxide in a precursor solution that a precursor material is dissolved in a solvent; a step of spreading the precursor solution with the hydrogen peroxide mixed on a substrate within a predetermined time after mixing the hydrogen peroxide; a step of thermally processing the substrate at a first temperature; and a step of thermally processing the substrate at a second temperature.

    Abstract translation: 本发明涉及形成氧化物薄膜的方法和使用过氧化氢制造氧化物薄膜的方法。 根据一个实施方案的形成氧化物薄膜的方法包括将前体材料溶解在溶剂中的前体溶液中混合过氧化氢的步骤; 在混合过氧化氢之后的预定时间内,将过氧化氢混合在基材上的步骤; 在第一温度下热处理所述基板的步骤; 以及在第二温度下热处理所述基板的步骤。

    용액 공정 기반의 정공 전도층 제조방법 및 이를 이용한 유기태양전지의 제조방법
    65.
    发明授权
    용액 공정 기반의 정공 전도층 제조방법 및 이를 이용한 유기태양전지의 제조방법 有权
    溶液处理半导体缓冲层的制造方法和使用它的太阳能电池

    公开(公告)号:KR101316237B1

    公开(公告)日:2013-10-08

    申请号:KR1020110129537

    申请日:2011-12-06

    CPC classification number: Y02E10/549 Y02P70/521

    Abstract: 본 발명은 고효율, 고안정성의 유기 태양전지 제조를 위하여 CuAlO
    2 박막을 정공 전도층으로 사용한 유기태양전지 제조 방법에 관한 것이다. 현재 유기 태양전지의 활성층 물질로 regioregular poly(3-hexylthiophene) (P3HT) 와 phenyl-C
    61 -butyric acid methyl ester (PCBM) 의 혼합물을 활성층으로 하고 PEDOT:PSS를 정공 전도층으로 사용하여 유기 태양전지를 제작하고 있다. 하지만 유기물 소자의 한계라고 할 수 있는 낮은 이동도로 인한 낮은 에너지 변환 효율과 외부환경 요인에 이한 전지의 수명 저하에 대해 많은 개선이 필요한 실정이다. 본 발명에서는 위에서 언급한 유기 물질인 PEDOT:PSS를 대체하여 사용한 CuAlO
    2 박막을 정공 전도층으로 사용하여 기존의 공정을 그대로 사용하면서 전자 에너지 장벽 (electron energy barrier)을 통해서 전자 손실 전류를 줄임으로써 광 에너지 변환 효율을 기존 유기태양전지 만큼 증가시키고, 또한, 유기 박막의 단점으로 지적되고 있는 산소, 수분 등에 의한 시간에 따른 소자의 특성 저하를 억제할 수 있기 때문에 고수명 전자소자로써의 역할로도 기대된다.

    용액 공정 기반 산화물 박막 트랜지스터 바이오 센서 및 그 제조방법
    66.
    发明公开
    용액 공정 기반 산화물 박막 트랜지스터 바이오 센서 및 그 제조방법 无效
    使用溶液处理氧化物薄膜晶体管的生物传感器及其制造方法

    公开(公告)号:KR1020130102148A

    公开(公告)日:2013-09-17

    申请号:KR1020120023122

    申请日:2012-03-07

    CPC classification number: C12Q1/6825 G01N27/4145

    Abstract: PURPOSE: An oxide thin film transistor biosensor is provided to show reliability and reproducibility, superior resistance to environmental stress and heat, and superior electrical characteristics. CONSTITUTION: A field effect transistor comprises: a substrate (200); a gate electrode (210) which is formed on the substrate; a gate insulation film (220) which is formed on the gate electrode; an oxide semiconductor layer (230) which is formed on the gate insulation film; and a source (240) and a drain electrode (250) which are formed on the oxide semiconductor layer to expose the oxide semiconductor layer. A field effect transistor biosensor detects components of a biomaterial (260) through current-voltage characteristics by bonding the biomaterial to a part of the oxide semiconductor layer which is exposed between the source and the drain electrode.

    Abstract translation: 目的:提供氧化物薄膜晶体管生物传感器,以显示可靠性和再现性,优异的耐环境应力和热性,以及优异的电气特性。 构成:场效应晶体管包括:衬底(200); 形成在所述基板上的栅电极(210) 栅极绝缘膜(220),其形成在栅电极上; 形成在所述栅极绝缘膜上的氧化物半导体层(230) 以及形成在所述氧化物半导体层上以暴露所述氧化物半导体层的源极(240)和漏极(250)。 场效应晶体管生物传感器通过将生物材料结合到暴露在源极和漏极之间的氧化物半导体层的一部分,通过电流 - 电压特性来检测生物材料(260)的成分。

    액상공정을 이용한 박막 트랜지스터 및 그 제조방법
    67.
    发明公开
    액상공정을 이용한 박막 트랜지스터 및 그 제조방법 有权
    使用液相工艺的薄膜晶体管及其制造方法

    公开(公告)号:KR1020130093922A

    公开(公告)日:2013-08-23

    申请号:KR1020120015171

    申请日:2012-02-15

    CPC classification number: H01L29/7869 H01L21/02623 H01L29/66742

    Abstract: PURPOSE: A thin film transistor using a liquid phase process and a manufacturing method thereof are provided to improve the characteristics and reliability of a device by increasing the density of a thin film through a multilayer channel structure in comparison to a single channel structure. CONSTITUTION: A source (500) and a drain (600) are in contact with both ends of a channel layer (400). A gate (200) corresponds to the channel layer. A gate insulating layer (300) is formed between the channel layer and the gate. The channel layer includes a plurality of oxide semiconductor layers (400a,400b,400c) manufactured by a liquid phase process. At least one oxide semiconductor layer included in the channel layer includes a ZnO-based oxide semiconductor.

    Abstract translation: 目的:提供一种使用液相工艺的薄膜晶体管及其制造方法,以通过与单通道结构相比通过多层通道结构增加薄膜的密度来提高器件的特性和可靠性。 构成:源(500)和漏极(600)与沟​​道层(400)的两端接触。 门(200)对应于沟道层。 在沟道层和栅极之间形成栅极绝缘层(300)。 沟道层包括通过液相法制造的多个氧化物半导体层(400a,400b,400c)。 包括在沟道层中的至少一个氧化物半导体层包括ZnO基氧化物半导体。

    용액 공정 기반의 산화물 반도체를 이용한 역방향 구조의 유기태양전지 및 그 제조방법
    69.
    发明授权
    용액 공정 기반의 산화물 반도체를 이용한 역방향 구조의 유기태양전지 및 그 제조방법 有权
    倒置有机太阳能电池和制造方法使用溶液加工氧化物半导体

    公开(公告)号:KR101266674B1

    公开(公告)日:2013-05-28

    申请号:KR1020110090626

    申请日:2011-09-07

    CPC classification number: Y02E10/549 Y02P70/521

    Abstract: 본발명은유기태양전지의효율과수명향상을위한것이다. 유기물전자소자의한계라고할 수있는낮은캐리어이동도로인한낮은에너지변환효율의개선과더불어정공수송층으로사용하고있는 PEDOT:PSS의산도로인한투명전극의부식이수명을단축하는문제를모두해결하기위해, 본발명에서는 PEDOT:PSS를사용하지않고, 용액공정을기반으로한 SnO박막을전자수송층으로사용하여전자전도도를높여유기태양전지의효율을높이고, SnO박막의내식성으로인해소자수명을연장시켰다. 용액공정기반의제조방법은여전히유기태양전지의제조단가를낮추어전력당생산비면에서도유리하다.

    유기용매를 첨가한 전도성 유기박막의 제조방법 및 이를 이용한 유기태양전지
    70.
    发明公开
    유기용매를 첨가한 전도성 유기박막의 제조방법 및 이를 이용한 유기태양전지 有权
    改性PEDOT:PSS与有机溶剂和有机太阳能电池使用它

    公开(公告)号:KR1020130027213A

    公开(公告)日:2013-03-15

    申请号:KR1020110090664

    申请日:2011-09-07

    CPC classification number: Y02E10/549 Y02P70/521 H01L51/42

    Abstract: PURPOSE: A method for manufacturing a conductive organic thin film with an organic solvent and an organic solar cell using the same are provided to improve the conductivity of a hole transport layer by forming a hole transport layer thin film with the mixture of acetic acid solvent and PEDOT:PSS of a low hole mobility. CONSTITUTION: A hole transport layer is laminated between an anode and an active layer. The hole transport layer is formed by coating the anode with the mixture of an organic solvent and PEDOT:PSS. The organic solvent is one of glycerol, dimethylformamide, ethylene glycol, dimethyl sulfoxide, and sorbital. A volume ratio of the PEDOT:PSS to the organic solvent is 1 to 10:1. The mixture of the PEDOT:PSS and the organic solvent is stirred at 100 to 1000 rpm for 30 minutes to four hours. [Reference numerals] (AA) Manufacture process

    Abstract translation: 目的:提供一种使用有机溶剂和有机太阳能电池制造导电有机薄膜的方法,其通过用乙酸溶剂和乙酸溶剂的混合物形成空穴传输层薄膜来改善空穴传输层的导电性 PEDOT:PSS的低空移动性。 构成:在阳极和有源层之间层叠空穴传输层。 通过用有机溶剂和PEDOT:PSS的混合物涂覆阳极来形成空穴传输层。 有机溶剂是甘油,二甲基甲酰胺,乙二醇,二甲基亚砜和山梨醇之一。 PEDOT:PSS与有机溶剂的体积比为1至10:1。 将PEDOT:PSS和有机溶剂的混合物在100至1000rpm下搅拌30分钟至4小时。 (标号)(AA)制造工艺