1.
    发明专利
    未知

    公开(公告)号:BR9608801A

    公开(公告)日:1999-02-17

    申请号:BR9608801

    申请日:1996-05-17

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP96/02116 Sec. 371 Date Nov. 24, 1997 Sec. 102(e) Date Nov. 24, 1997 PCT Filed May 17, 1996 PCT Pub. No. WO96/37541 PCT Pub. Date Nov. 28, 1996Expanded polyolefin particles are produced by impregnation of polyolefin granules with a volatile blowing agent in suspension under pressure and subsequent decompression. The blowing agent used is ammonia.

    3.
    发明专利
    未知

    公开(公告)号:NO970804L

    公开(公告)日:1997-04-21

    申请号:NO970804

    申请日:1997-02-21

    Applicant: BASF AG

    Abstract: PCT No. PCT/EP95/03190 Sec. 371 Date Feb. 24, 1997 Sec. 102(e) Date Feb. 24, 1997 PCT Filed Aug. 11, 1995 PCT Pub. No. WO96/06129 PCT Pub. Date Feb. 29, 1996The invention relates to a process for the production of expanded polyolefin beads by impregnating polyolefin particles with volatile blowing agents in a fluidized bed.

    Foamed polyolefin mouldings free of cavities - suitable for insulation, upholstery or packaging

    公开(公告)号:DE2331306A1

    公开(公告)日:1975-01-23

    申请号:DE2331306

    申请日:1973-06-20

    Applicant: BASF AG

    Abstract: Foamed articles are made by compressing a mixt. of finely divided polyolefin with 0.3-4.0 g, per l, polyolefin, of a solvent-free curable blinder to 40-80% of the original bulk vol. of the mixt., whilst treating it with a gas of greater permeability coefft. than air. The polyolefin specif. has a crystallinity of >20 wt% at 25 degrees C and MFI 0.1-200 g/10 mins (190 degrees C/2.16 Kg, ASTM-D 1238-65T) and pref. is high pressure polyethylene of 0.918-0.935 g/cm3. The granules have an ave. dia. of 1-35 mm, pref. 3-20 mm and have a bulk density of 5-200 g/l, pref. 10-60 g/l. The binder is esp. a polyester or an epoxy resin, pref. in an amt. 0.6-2 g/l. The gas, (permeability coefft. measured to ASTM D 1434-63), is pret. ammonia or CO2, though (halogenated) hydrocarbons (b.pt. is not >15 degrees C) or CO may also be used. Compression is pref. to 50-70 vol%.

    Foamed polyolefins mouldings free of cavities - suitable for insulation, upholstery or packaging

    公开(公告)号:DE2331303A1

    公开(公告)日:1975-01-23

    申请号:DE2331303

    申请日:1973-06-20

    Applicant: BASF AG

    Abstract: Foamed polyolefin articles are made by heating and compressing foamed cross-linked polyolefin granules in moulds which are not gas-tight while treating them with a gas whose permeability coefficient is greater than that of air. The polyolefin has a crystallinity of >20 wt% at 25 degrees C and MFI of 0.1-200 g/10 mins (190 degrees C/2.16 Kg) and is pref. high pressure polyethylene of 0.918-0.935 g/cm3. The granules have an ave. dia. of 1-35 mm, pref. 3-20 mm and a bulk density of 5-200 g/l, pref. 10-60 g/l. The gas, (permeability coeff. measured to D/N 53380 or ASTM D 1434-63), is pref. ammonia or CO2. The granules, heated to 40-80 degrees C in the presence of the gas are transferred to the mould and sintered at 5-150 degrees C, pref. 10-100 degrees C above their crystalline m.pt., i.e. at 90-250 degrees C, pref. 110-180 degrees C. After heating, the granules are compressed to 40-80% pref. 50-70% of their original vol.

Patent Agency Ranking